Strengthening of Vickers indented 3Y-TZP by hydrothermal ageing

被引:15
|
作者
Marro, F. G. [1 ,2 ]
Anglada, M. [1 ,2 ]
机构
[1] Univ Politecn Cataluna, Ctr Res Nanoengn, CRnE, E-08028 Barcelona, Spain
[2] Univ Politecn Cataluna, Dept Mat Sci & Met Engn, E-08028 Barcelona, Spain
关键词
ZrO(2); Fracture; Mechanical properties; Strength; Toughness and toughening; LOW-TEMPERATURE DEGRADATION; FRACTURE-TOUGHNESS; INDENTATION TECHNIQUES; FEMORAL-HEAD; ZIRCONIA; CRACK;
D O I
10.1016/j.jeurceramsoc.2011.08.019
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
The effect of hydrothermal ageing on indentation cracks has been determined in 3Y-TZP by measuring the flexure strength of indented specimens before and after ageing. A substantial increase in strength was observed after ageing, in contrast to the well known decrease in strength in smooth specimens with only natural flaws. The increase in strength with ageing also occurs if the indentation residual stresses are previously removed by annealing. Observations around the crack tip show the formation of a highly microcracked zone during vapour exposure. Fractographic and micro-Raman analysis observations show that the profile of the cracks is marked on the fracture surface by this zone which is intergranular with a crumbled appearance and in which transformation has taken place. The increase in strength is discussed in terms of crack tip blunting induced by the multiaxial stresses that develop in front of the crack under bending. (C) 2011 Elsevier Ltd. All rights reserved.
引用
收藏
页码:317 / 324
页数:8
相关论文
共 50 条
  • [31] Synthesis, sintering and microstructure of 3Y-TZP/CuO
    Ran, S
    Winnubst, L
    Wiratha, W
    Blank, DHA
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2006, 26 (4-5) : 391 - 396
  • [32] Preparation and Properties of 3Y-TZP Ceramic Tools
    Chen, Zhiwei
    Feng, Liu
    Niu, Jinye
    TESTING AND EVALUATION OF INORGANIC MATERIALS I, 2011, 177 : 373 - 377
  • [33] Tensile behaviour of 3Y-TZP/Ni composites
    López-Esteban, S
    Bartolomé, JF
    Moya, JS
    Sagisaka, A
    Matsumoto, K
    Tanimoto, T
    FRACTOGRAPHY OF ADVANCED CERAMICS, 2002, 223 : 79 - 82
  • [34] Thermal conductivity of superplastically deformed 3Y-TZP
    Wan, C
    Motohashi, Y
    Shibata, T
    Baba, S
    Ishihara, M
    Hoshiya, T
    MATERIALS TRANSACTIONS, 2002, 43 (10) : 2473 - 2479
  • [35] Investigation of superplasticity in 3Y-TZP by stress relaxation
    Seidensticker, JR
    Wiederhorn, SM
    TOWARDS INNOVATION IN SUPERPLASTICITY II, 1999, 304-3 : 403 - 409
  • [36] Surface modification of 3Y-TZP with cerium oxide
    Marro, F. G.
    Valle, J.
    Mestra, A.
    Anglada, M.
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2011, 31 (03) : 331 - 338
  • [37] Double torsion testing a 3Y-TZP ceramic
    Chevalier, J
    Saadaoui, V
    Olagnon, C
    Fantozzi, G
    CERAMICS INTERNATIONAL, 1996, 22 (02) : 171 - 177
  • [38] A review on the hydrothermal ageing behaviour of Y-TZP ceramics
    Ramesh, S.
    Lee, K. Y. Sara
    Tan, C. Y.
    CERAMICS INTERNATIONAL, 2018, 44 (17) : 20620 - 20634
  • [39] 干法成型制备3Y-TZP陶瓷
    李树先
    西藏科技, 2010, (07) : 49 - 50
  • [40] Study on sintering properties of 3Y-TZP powders
    Meng, Zhao-Qiang
    Huang, De-Xin
    Feng, Tao
    Xu, Hai-Fang
    Jiang, Dan-Yu
    Rengong Jingti Xuebao/Journal of Synthetic Crystals, 2009, 38 (SUPPL. 1): : 375 - 378