Peritectic solidification mechanism and accompanying microhardness enhancement of rapidly quenched Ni-Zr alloys

被引:4
|
作者
Si, Y. F. [1 ]
Wang, H. P. [1 ]
Lu, P. [1 ]
Wei, B. [1 ]
机构
[1] Northwestern Polytech Univ, Dept Appl Phys, Xian 710072, Shaanxi, Peoples R China
来源
基金
中国国家自然科学基金;
关键词
MICROSTRUCTURE; GROWTH; TRANSITION; SELECTION; BEHAVIOR;
D O I
10.1007/s00339-019-2399-x
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Hypoperitectic, peritectic, and hyperperitectic Ni-Zr alloys were rapidly solidified by melt spinning technique. The effect of cooling rate on their phase selection and microhardness was investigated. When the cooling rate reaches 1.0x10(7) K/s, the growth of primary Ni7Zr2 and interdendritic eutectic ((Ni)+Ni5Zr) phases during the solidification of peritectic Ni-16.7 at.% Zr alloy melt is inhibited, and complete peritectic Ni5Zr phase forms. The formation ability of complete peritectic Ni5Zr phase of hypoperitectic Ni-16 at.% Zr alloy is considerably higher than that of peritectic Ni-16.7 at.% Zr alloy. With the increase of cooling rate, the competitive growth of the primary Ni7Zr2 phase and the peritectic Ni5Zr phase occurs in the hyperperitectic Ni-20 at.% Zr alloy. The microstructure of primary Ni7Zr2 phase evolves from coarse dendrite to island banding. Furthermore, the microhardness of Ni-Zr peritectic type alloys is enhanced with the rise of cooling rate. In the case of peritectic Ni-16.7 at.% Zr alloy, this increases from 3.98 to 7.01 GPa, realizing an enhancement of 76.8%.
引用
收藏
页数:12
相关论文
共 50 条
  • [21] Dependence of microhardness on solidification processing parameters and dendritic spacing in directionally solidified Sn-Ni peritectic alloys
    Peng, Peng p
    Li, Xinzhong
    Su, Yanqing
    Li, Jiangong
    Guo, Jingjie
    Fu, Hengzhi
    JOURNAL OF ALLOYS AND COMPOUNDS, 2015, 618 : 49 - 55
  • [22] Enthalpy of mixing of liquid Ni-Zr and Cu-Ni-Zr alloys
    Witusiewicz, VT
    Sommer, F
    METALLURGICAL AND MATERIALS TRANSACTIONS B-PROCESS METALLURGY AND MATERIALS PROCESSING SCIENCE, 2000, 31 (02): : 277 - 284
  • [24] Enthalpy of mixing of liquid Ni-Zr and Cu-Ni-Zr alloys
    Victor T. Witusiewicz
    Ferdinand Sommer
    Metallurgical and Materials Transactions B, 2000, 31 : 277 - 284
  • [25] Evidence for the transition from primary to peritectic phase growth during solidification of undercooled Ni-Zr alloy levitated by electromagnetic field
    Lu, P.
    Zhou, K.
    Wang, H. P.
    SCIENTIFIC REPORTS, 2016, 6
  • [26] Oxidation behavior of amorphous Ni-Zr and Ni-Zr-Sm alloys
    Yamasaki, M
    Habazaki, H
    Asami, K
    Hashimoto, K
    JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 2000, 147 (12) : 4502 - 4506
  • [27] Study of the thermal decomposition of melt-quenched Ni-rich metastable bcc and amorphous Ni-Zr alloys
    Cziraki, A
    Gerocs, I
    Fogarassy, B
    Van Tendeloo, G
    Sommer, F
    Bakonyi, I
    INTERNATIONAL JOURNAL OF NON-EQUILIBRIUM PROCESSING, 1998, 10 (3-4): : 265 - 282
  • [28] HYDROGEN IN AMORPHOUS NI-ZR AND NI-TI ALLOYS
    KIRCHHEIM, R
    KIENINGER, W
    HUANG, XY
    FILIPEK, SM
    RUSH, J
    UDOVIC, T
    JOURNAL OF THE LESS-COMMON METALS, 1991, 172 : 880 - 889
  • [29] Evidence for the transition from primary to peritectic phase growth during solidification of undercooled Ni-Zr alloy levitated by electromagnetic field
    P. Lü
    K. Zhou
    H. P. Wang
    Scientific Reports, 6
  • [30] Modelling of dendritic solidification in undercooled dilute Ni-Zr melts
    Galenko, P. K.
    Reutzel, S.
    Herlach, D. M.
    Danilov, D.
    Nestler, B.
    ACTA MATERIALIA, 2007, 55 (20) : 6834 - 6842