High temperature oxidation of Ti-48%Al-2%W intermetallics

被引:7
|
作者
Shim, WS [1 ]
Lee, DB [1 ]
机构
[1] Sungkyunkwan Univ, Ctr Adv Plasma Surface Technol, Suwon 440746, South Korea
关键词
TiAl; intermetallics; tungsten; oxidation;
D O I
10.1007/BF03027153
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Powder metallurgically produced Ti-48%Al-2%W alloys were oxidized between 800 and 1050degreesC in air. The W-addition was quite effective in providing isothermal and cyclic oxidation resistance. The alloys oxidized parabolically up to 1050degreesC during isothermal oxidation, with small weight gains. The scales were adherent up to 900degreesC during cyclic oxidation. Oxide scales consisted primarily of an outer TiO2 layer, an intermediate Al2O3 layer, and an inner (TiO2+Al2O3) mixed layer. Tungsten was present below the intermediate Al2O3 layer, and also at the scale-matrix interface as W-enriched compounds. Below the oxide scale, a Ti3Al zone containing some W and O existed.
引用
收藏
页码:473 / 477
页数:5
相关论文
共 50 条
  • [41] Flow softening behavior during high temperature deformation of Ti-48Al-2W intermetallic compound
    Hee Y. Kim
    Soon H. Hong
    Metals and Materials, 1998, 4 : 765 - 770
  • [42] Flow Softening Behavior during High Temperature Deformation of Ti-48Al-2W Intermetallic Compound
    Kim, Hee Y.
    Hong, Soon H.
    Metals and Materials International, 1998, 4 (04): : 765 - 770
  • [43] Effect of microstructure on the high-temperature deformation behavior of Ti-48Al-2W intermetallic compounds
    Kim, HY
    Hong, SH
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 1999, 271 (1-2): : 382 - 389
  • [44] Effect of microstructure on the high-temperature deformation behavior of Ti-48Al-2W intermetallic compounds
    Dept. of Mat. Sci. and Engineering, Korea Adv. Inst. Sci. and Technol., 373-1 Kusung-dong, Yusung-gu, Taejon 305-701, Korea, Republic of
    Mater. Sci. Eng. A, 1-2 (382-389):
  • [45] Flow softening behavior during high temperature deformation of Ti-48Al-2W intermetallic compound
    Kim, HY
    Hong, SH
    METALS AND MATERIALS-KOREA, 1998, 4 (04): : 765 - 770
  • [46] High temperature tribological behavior of a Ti-46Al-2Cr-2Nb intermetallics
    Cheng, Jun
    Yang, Jun
    Zhang, Xinghua
    Zhong, Hong
    Ma, Jiqiang
    Li, Fei
    Fu, Licai
    Bi, Qinling
    Li, Jinshan
    Liu, Weimin
    INTERMETALLICS, 2012, 31 : 120 - 126
  • [47] Influence of Si and W additions on high temperature oxidation of gamma,alpha(2) Ti-Al alloys
    Tomasi, A
    Noseda, C
    Nazmy, M
    Gialanella, S
    HIGH-TEMPERATURE ORDERED INTERMETALLIC ALLOYS VII, 1997, 460 : 225 - 230
  • [48] Oxidation behavior of Al3Ti intermetallics
    Reddy, RG
    Wen, X
    EPD CONGRESS 1997, 1997, : 47 - 54
  • [49] Oxidation of Ti3Al and Ti3Al-Nb intermetallics
    Reddy, RG
    Wen, XR
    Li, Y
    TITANIUM: EXTRACTION AND PROCESSING, 1996, : 153 - 161
  • [50] Influence of oxygen on phase transformations in a Ti-48 at. pct Al alloy
    Lefebvre, W
    Loiseau, A
    Menand, A
    METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2003, 34A (10): : 2067 - 2075