High temperature oxidation of Ti-48%Al-2%W intermetallics

被引:7
|
作者
Shim, WS [1 ]
Lee, DB [1 ]
机构
[1] Sungkyunkwan Univ, Ctr Adv Plasma Surface Technol, Suwon 440746, South Korea
关键词
TiAl; intermetallics; tungsten; oxidation;
D O I
10.1007/BF03027153
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Powder metallurgically produced Ti-48%Al-2%W alloys were oxidized between 800 and 1050degreesC in air. The W-addition was quite effective in providing isothermal and cyclic oxidation resistance. The alloys oxidized parabolically up to 1050degreesC during isothermal oxidation, with small weight gains. The scales were adherent up to 900degreesC during cyclic oxidation. Oxide scales consisted primarily of an outer TiO2 layer, an intermediate Al2O3 layer, and an inner (TiO2+Al2O3) mixed layer. Tungsten was present below the intermediate Al2O3 layer, and also at the scale-matrix interface as W-enriched compounds. Below the oxide scale, a Ti3Al zone containing some W and O existed.
引用
收藏
页码:473 / 477
页数:5
相关论文
共 50 条
  • [11] Anomalous wetting of Ti-48 at.% Al-2 at.% Cr-2 at.% Nb substrates by liquid copper
    Gale, WF
    Shen, Y
    Fergus, JW
    Wen, X
    JOURNAL OF MATERIALS RESEARCH, 1999, 14 (10) : 3889 - 3894
  • [12] A QUANTITATIVE INVESTIGATION OF PHASE-FORMATION DURING ANNEALING OF COLD-EXTRUDED ELEMENTAL POWDER MIXTURES TI-48 AT-PERCENT AL AND TI-48 AT-PERCENT AL-2 AT-PERCENT CR
    BOHNENKAMP, U
    WANG, GX
    JEWETT, TJ
    DAHMS, M
    INTERMETALLICS, 1994, 2 (04) : 275 - 283
  • [13] High temperature oxidation behaviour of Ti3Al-Nb intermetallics
    Jha, SK
    Khanna, AS
    Harendranath, CS
    HIGH TEMPERATURE CORROSION AND PROTECTION OF MATERIALS 4, PTS 1 AND 2, 1997, 251-2 : 203 - 210
  • [14] Modelling wide gap TLP bonding of Ti-48 at.-%Al-2 at.-%Cr-2 at.-%Nb alloys
    Zhou, T
    Gale, WF
    MATERIALS SCIENCE AND TECHNOLOGY, 2003, 19 (08) : 1084 - 1090
  • [15] Structure and High-Temperature Oxidation of Ti-Al-Nb and Ti-Al-Ta Intermetallics
    Vojtech, Dalibor
    Popela, Tomas
    MATERIALS STRUCTURE & MICROMECHANICS OF FRACTURE, 2011, 465 : 227 - 230
  • [16] Research on Ti-48%Al-2%Cr-2%Nb automobile exhaust valve cast by centrifugal casting process in permanent mold
    Sheng, W.B.
    Li, D.
    Yang, R.
    Guo, J.J.
    Liu, Y.Y.
    Su, Y.Q.
    Jia, J.
    Zhuzao/Foundry, 2001, 50 (03):
  • [17] Effects of surface conditions on room temperature ductility in Ti-48 at%Al alloy
    Motohashi, Y
    Murata, Y
    Kaminaga, T
    Sakuma, T
    Tsujimoto, T
    Nakamura, M
    JOURNAL OF THE JAPAN INSTITUTE OF METALS, 2000, 64 (11) : 1012 - 1019
  • [18] High-temperature oxidation of intermetallics based on Ti-Al-Si system
    Knaislová A.
    Šimůnková V.
    Novák P.
    Knaislová, Anna (knaisloa@vscht.cz), 2018, Jan-Evangelista-Purkyne-University (18): : 255 - 258
  • [19] Decomposition processes of α phase in a Ti-48 at% Al alloy
    Nakai, K
    Momosaki, T
    Ohmori, Y
    MATERIALS TRANSACTIONS JIM, 2000, 41 (03): : 406 - 413
  • [20] Formation of deformation textures in the Ti-48 at% Al alloy
    Rubina, EB
    RUSSIAN METALLURGY, 1996, (04): : 69 - 77