Influence of process parameters and defect analysis in hot deep drawing process of aluminum alloy AA6082

被引:6
|
作者
Ma Wen-yu [1 ,2 ]
Wang Bao-yu [3 ]
Rong Qi [2 ,4 ]
Yang Jian-wei [1 ,2 ]
Zhang Jun [1 ,2 ]
机构
[1] Shougang Grp Co Ltd, Res Inst Technol, Beijing 100043, Peoples R China
[2] Shougang Imperial Lab Lightweight Steel Based Sys, London SW7 2AZ, England
[3] Univ Sci & Technol Beijing, Sch Mech Engn, Beijing 100083, Peoples R China
[4] Imperial Coll London, London SW7 2AZ, England
关键词
aluminum alloy; hot stamping; formability; damage; crack mechanism; CONSTITUTIVE MODEL; SHEET; COEFFICIENT; OPTIMIZATION; DEFORMATION; FRICTION;
D O I
10.1007/s11771-022-4984-y
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
In this study, a novel punch toolset was developed to investigate the hot stamping of AA6082-T4 sheet. The effect of the process parameters, including forming temperature, punching velocity, friction coefficient, and blank holder force (BHF) on formability was quantified using Taguchi design, analysis of variance (ANOVA) and mathematical statistics. The finite element (FE) model has been established in software Pamstamp for simulation and analysis of their effects on the minimum thickness and thickness variation of the hot-stamped component. The major factors influencing the minimum thickness of the hot-stamped part has been found to be BHF and friction coefficient with influence significance of 35.3% and 34.88%, respectively. Additionally, punch velocity and BHF affect the thickness deviation significantly with influence significance of 40.43% and 35.42%, respectively. Furthermore, a serious thinning occurs on the punch corner region of the hot-stamped cup when the BHF is larger than 2.4 kN. The thickness deviation of the hot-formed cup has been found to be firstly decreased and then increased with the increase of punch velocity. Low friction coefficient between punch and blank led to crack at bottom centre of the cup. Moreover, different type, phenomenon and mechanism of defects occurring during hot stamping process, such as crack and wrinkling, were discussed. The crack mode was dimple-dominated ductile fracture, which was induced by micro-void nucleation, growth and coalescence.
引用
收藏
页码:883 / 897
页数:15
相关论文
共 50 条
  • [31] Optimization of friction stir welding parameters for micro alloying of AA6082 alloy
    Aman Kishore Sharma
    Deepam Goyal
    B. S. Pabla
    Kuldeep K. Saxena
    Chander Prakash
    Dharam Buddhi
    International Journal on Interactive Design and Manufacturing (IJIDeM), 2024, 18 : 1219 - 1229
  • [32] Effect of FSW process parameters on mechanical properties and microstructure of dissimilar welded joints of AA2024 and AA6082
    Kumar, Ravi
    Salah, A. Nait
    Kant, Neeraj
    Singh, Pushpender
    Hashmi, Abdul Wahab
    Malla, Chandrabhanu
    MATERIALS TODAY-PROCEEDINGS, 2022, 50 : 1435 - 1441
  • [33] Investigating the influence of biodegradable nanofluid process cooling on dynamic recrystallization and grain microstructure in friction stir welding of AA6082 alloy
    Verma, Shubham
    Wu, Chuansong
    Thakur, Lalit
    Muhammad, Najib Ahmad
    Li, Shengli
    JOURNAL OF MATERIALS PROCESSING TECHNOLOGY, 2025, 336
  • [34] The effect of the number of passes in friction stir processing of aluminum alloy (AA6082) and its failure analysis
    Senthilkumar, R.
    Prakash, M.
    Arun, N.
    Jeyakumar, A. Arul
    APPLIED SURFACE SCIENCE, 2019, 491 : 420 - 431
  • [35] Mechanical property improvement of a AA6082 alloy by the TV-CAP process as a novel SPD method
    Kaya, Hasan
    Ozbeyaz, Kerim
    Kentli, Aykut
    MATERIALS TESTING, 2023, 65 (02) : 244 - 257
  • [36] Optimization of friction stir welding parameters for micro alloying of AA6082 alloy
    Sharma, Aman Kishore
    Goyal, Deepam
    Pabla, B. S.
    Saxena, Kuldeep K.
    Prakash, Chander
    Buddhi, Dharam
    INTERNATIONAL JOURNAL OF INTERACTIVE DESIGN AND MANUFACTURING - IJIDEM, 2024, 18 (03): : 1219 - 1229
  • [37] Influence of Dispersion Hardening and Severe Plastic Deformation on Structure, Strength and Ductility Behavior of an AA6082 Aluminum Alloy
    Zhukov, I.
    Promakhov, V.
    Vorozhtsov, S.
    Kozulin, A.
    Khrustalyov, A.
    Vorozhtsov, A.
    JOM, 2018, 70 (11) : 2731 - 2738
  • [38] Influence of Dispersion Hardening and Severe Plastic Deformation on Structure, Strength and Ductility Behavior of an AA6082 Aluminum Alloy
    I. Zhukov
    V. Promakhov
    S. Vorozhtsov
    A. Kozulin
    A. Khrustalyov
    A. Vorozhtsov
    JOM, 2018, 70 : 2731 - 2738
  • [39] Effect of different grain sizes and textures on the corrosion behaviour of aluminum alloy AA6082
    Haendel, M.
    Nickel, D.
    Lampke, T.
    MATERIALWISSENSCHAFT UND WERKSTOFFTECHNIK, 2011, 42 (07) : 606 - 611
  • [40] Influence of Process Parameters on the Deep Cup-drawing Process by Simulation
    Zhang, Xiao Bing
    Jiang, Xiao Hui
    FRONTIERS OF ADVANCED MATERIALS AND ENGINEERING TECHNOLOGY, PTS 1-3, 2012, 430-432 : 1107 - 1110