Influence of process parameters and defect analysis in hot deep drawing process of aluminum alloy AA6082

被引:6
|
作者
Ma Wen-yu [1 ,2 ]
Wang Bao-yu [3 ]
Rong Qi [2 ,4 ]
Yang Jian-wei [1 ,2 ]
Zhang Jun [1 ,2 ]
机构
[1] Shougang Grp Co Ltd, Res Inst Technol, Beijing 100043, Peoples R China
[2] Shougang Imperial Lab Lightweight Steel Based Sys, London SW7 2AZ, England
[3] Univ Sci & Technol Beijing, Sch Mech Engn, Beijing 100083, Peoples R China
[4] Imperial Coll London, London SW7 2AZ, England
关键词
aluminum alloy; hot stamping; formability; damage; crack mechanism; CONSTITUTIVE MODEL; SHEET; COEFFICIENT; OPTIMIZATION; DEFORMATION; FRICTION;
D O I
10.1007/s11771-022-4984-y
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
In this study, a novel punch toolset was developed to investigate the hot stamping of AA6082-T4 sheet. The effect of the process parameters, including forming temperature, punching velocity, friction coefficient, and blank holder force (BHF) on formability was quantified using Taguchi design, analysis of variance (ANOVA) and mathematical statistics. The finite element (FE) model has been established in software Pamstamp for simulation and analysis of their effects on the minimum thickness and thickness variation of the hot-stamped component. The major factors influencing the minimum thickness of the hot-stamped part has been found to be BHF and friction coefficient with influence significance of 35.3% and 34.88%, respectively. Additionally, punch velocity and BHF affect the thickness deviation significantly with influence significance of 40.43% and 35.42%, respectively. Furthermore, a serious thinning occurs on the punch corner region of the hot-stamped cup when the BHF is larger than 2.4 kN. The thickness deviation of the hot-formed cup has been found to be firstly decreased and then increased with the increase of punch velocity. Low friction coefficient between punch and blank led to crack at bottom centre of the cup. Moreover, different type, phenomenon and mechanism of defects occurring during hot stamping process, such as crack and wrinkling, were discussed. The crack mode was dimple-dominated ductile fracture, which was induced by micro-void nucleation, growth and coalescence.
引用
收藏
页码:883 / 897
页数:15
相关论文
共 50 条
  • [21] Effect of the heat treatment on the hot deformation behaviour of AA6082 alloy
    Zhang, B
    Baker, TN
    JOURNAL OF MATERIALS PROCESSING TECHNOLOGY, 2004, 153 : 881 - 885
  • [22] STRUCTURE REFINEMENT BY SPD AND PROPERTIES RESPOND OF AA6082 ALUMINUM ALLOY
    Zrnik, Jozef
    Scheriau, Stephan
    Pippan, Reinhard
    Slama, Peter
    METAL 2015: 24TH INTERNATIONAL CONFERENCE ON METALLURGY AND MATERIALS, 2015, : 1233 - 1239
  • [23] Influence of the temperature on AA6061 aluminum alloy in a hot extrusion process
    Marin, M. M.
    Camacho, A. M.
    Perez, J. A.
    MANUFACTURING ENGINEERING SOCIETY INTERNATIONAL CONFERENCE 2017 (MESIC 2017), 2017, 13 : 327 - 334
  • [24] Electrochemical Analysis of AA6082 Aluminium Alloy in Chloride Media
    Xhanari, Klodian
    Finsgar, Matjaz
    INTERNATIONAL JOURNAL OF ELECTROCHEMICAL SCIENCE, 2017, 12 (07): : 5845 - 5853
  • [25] Influence of hot-working and ageing on notched-strength and ductility of aluminium alloy AA6082
    Metallurgical R & D Cent, Sunndalsora, Norway
    Mater Sci Forum, pt 2 (1221-1226):
  • [26] Assessment on the impact of FSP process parameters on microstructural, mechanical and wear behaviour of FSPed AA6082
    Prabhu, Sivanesh M.
    Elayaperumal, A.
    Arulvel, S.
    Khan, M. Wasim
    SURFACE TOPOGRAPHY-METROLOGY AND PROPERTIES, 2021, 9 (01):
  • [27] Dry Sliding Tribological Properties of a Hard Anodized AA6082 Aluminum Alloy
    Santecchia, Eleonora
    Cabibbo, Marcello
    Hamouda, Abdel Magid Salem
    Musharavati, Farayi
    Popelka, Anton
    Spigarelli, Stefano
    METALS, 2020, 10 (02)
  • [28] Assessment of Super-Hydrophobic Textured Coatings on AA6082 Aluminum Alloy
    Calabrese, Luigi
    Khaskhoussi, Amani
    Patane, Salvatore
    Proverbio, Edoardo
    COATINGS, 2019, 9 (06):
  • [29] Influence of Metal Transfer Modes on Pore Formation during the Welding Process of AA6082/A360 Dissimilar Aluminum Alloys
    Hanlin Xiang
    Congchang Xu
    Teng Zhan
    Lin Wu
    Haijun Wang
    Luoxing Li
    Journal of Materials Engineering and Performance, 2023, 32 : 8750 - 8766
  • [30] Influence of Metal Transfer Modes on Pore Formation during the Welding Process of AA6082/A360 Dissimilar Aluminum Alloys
    Xiang, Hanlin
    Xu, Congchang
    Zhan, Teng
    Wu, Lin
    Wang, Haijun
    Li, Luoxing
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2023, 32 (19) : 8750 - 8766