Thermo-oxidative degradation and radio-processing of ethylene vinyl acetate elastomers

被引:25
|
作者
Giurginca, M
Popa, L
Zaharescu, T
机构
[1] Adv Res Inst Elect Engn, Bucharest 74204, Romania
[2] Anticorosiv SA, Bucharest 74584, Romania
[3] Univ Polytech, Bucharest 78126, Romania
关键词
ethylene vinyl acetate; degradation; FT-IR spectroscopy; DSC;
D O I
10.1016/S0141-3910(03)00200-3
中图分类号
O63 [高分子化学(高聚物)];
学科分类号
070305 ; 080501 ; 081704 ;
摘要
Thermal and radiation degradation of three ethylene vinyl acetate elastomers containing 28 and 33% VA were studied by IR spectroscopy and thermal analysis. Kinetic parameters: induction time, oxidation rate, reaction order and activation energy of oxidation were calculated on the basis of the modification in the carbonyl band absorbance during thermal degradation. Temperatures that characterize various processes occurring during degradation are pointed out. The progress in radiochemical degradation was assessed by changes in the 1735 cm(-1) band relative to a standard (1475 cm(-1)). A mechanism of degradation is proposed. (C) 2003 Elsevier Ltd. All rights reserved.
引用
收藏
页码:463 / 466
页数:4
相关论文
共 50 条
  • [41] ON MECHANISM OF THERMO-OXIDATIVE DEGRADATION OF CELLULOSE ETHERS
    KOZMINA, OP
    JOURNAL OF POLYMER SCIENCE PART C-POLYMER SYMPOSIUM, 1968, (16PC): : 4225 - &
  • [42] Effect of stereoregularity on the thermo-oxidative degradation of polypropylenes
    Kato, M
    Osawa, Z
    POLYMER DEGRADATION AND STABILITY, 1999, 65 (03) : 457 - 461
  • [43] Thermo-oxidative degradation and stabilization of rubber materials
    Mattson, Bengt
    Stenberg, Bengt
    Progress in rubber and plastics technology, 1993, 9 (01): : 1 - 53
  • [44] Influence of colorants on thermo-oxidative degradation of polycarbonate
    Saron, C.
    Felisberti, M., I
    MATERIA-RIO DE JANEIRO, 2009, 14 (03): : 1028 - 1038
  • [45] THERMO-OXIDATIVE DEGRADATION OF FATS - METHYLOLEATE AS AN EXAMPLE
    LECKER, G
    INDUSTRIE ALIMENTARI, 1983, 22 (06): : 498 - 498
  • [46] Thermo-Oxidative Degradation Behavior of Recycled Polypropylene
    Nasir, Asad
    Yasin, Tariq
    Islam, Atif
    JOURNAL OF APPLIED POLYMER SCIENCE, 2011, 119 (06) : 3315 - 3320
  • [47] MICRO-MECHANICAL MODEL FOR THERMO-OXIDATIVE AGING OF ELASTOMERS
    Mohammadi, Hamid
    Dargazany, Roozbeh
    PROCEEDINGS OF THE ASME INTERNATIONAL MECHANICAL ENGINEERING CONGRESS AND EXPOSITION, 2018, VOL 9, 2019,
  • [48] THERMAL AGING OF CURED ETHYLENE-VINYL ACETATE AND ETHYLENE-VINYL ACETATE-VINYL ALCOHOL ELASTOMERS
    SMITH, RM
    BAKER, GK
    SMITH, CH
    ABSTRACTS OF PAPERS OF THE AMERICAN CHEMICAL SOCIETY, 1976, 172 (SEP3): : 57 - 57
  • [49] Thermo-oxidative ageing of poly(vinyl chloride) based thermoplastic elastomers - Effect of ''New'' Epoxidized Natural Rubber
    Ishiaku, US
    Shaharum, A
    Mohd, ZA
    KAUTSCHUK GUMMI KUNSTSTOFFE, 1997, 50 (04): : 292 - 298
  • [50] Determination of the thermo-oxidative degradation activation energy for some elastomers, by the non-isothermal oxiluminescence method
    Jipa, S
    Setnescu, T
    Setnescu, R
    Dumitru, M
    Mihalcea, I
    MATERIALE PLASTICE, 1995, 32 (3-4) : 231 - 237