Thermo-oxidative degradation and radio-processing of ethylene vinyl acetate elastomers

被引:25
|
作者
Giurginca, M
Popa, L
Zaharescu, T
机构
[1] Adv Res Inst Elect Engn, Bucharest 74204, Romania
[2] Anticorosiv SA, Bucharest 74584, Romania
[3] Univ Polytech, Bucharest 78126, Romania
关键词
ethylene vinyl acetate; degradation; FT-IR spectroscopy; DSC;
D O I
10.1016/S0141-3910(03)00200-3
中图分类号
O63 [高分子化学(高聚物)];
学科分类号
070305 ; 080501 ; 081704 ;
摘要
Thermal and radiation degradation of three ethylene vinyl acetate elastomers containing 28 and 33% VA were studied by IR spectroscopy and thermal analysis. Kinetic parameters: induction time, oxidation rate, reaction order and activation energy of oxidation were calculated on the basis of the modification in the carbonyl band absorbance during thermal degradation. Temperatures that characterize various processes occurring during degradation are pointed out. The progress in radiochemical degradation was assessed by changes in the 1735 cm(-1) band relative to a standard (1475 cm(-1)). A mechanism of degradation is proposed. (C) 2003 Elsevier Ltd. All rights reserved.
引用
收藏
页码:463 / 466
页数:4
相关论文
共 50 条
  • [31] Thermo-oxidative degradation of some elastomers with a high content of 3,4 isoprene units
    Ivan, G
    Meghea, A
    Giurginca, M
    Iftimie, N
    POLYMER DEGRADATION AND STABILITY, 2003, 80 (03) : 397 - 402
  • [32] Studies on thermal and thermo-oxidative degradation of poly(ethylene terephthalate) and poly(butylene terephthalate)
    Botelho, G
    Queirós, A
    Liberal, S
    Gijsman, P
    POLYMER DEGRADATION AND STABILITY, 2001, 74 (01) : 39 - 48
  • [33] SPECTROSCOPIC STUDY OF THE THERMO-OXIDATIVE DEGRADATION OF POLYMETHACRYLONITRILE
    PLATONOVA, NV
    GRACHEV, VI
    KLIMENKO, IB
    GOLTSIN, BE
    SMIRNOV, LV
    VYSOKOMOLEKULYARNYE SOEDINENIYA SERIYA B, 1978, 20 (12): : 914 - 917
  • [34] POLYPROPYLENE THERMO-OXIDATIVE DEGRADATION AND STABILIZATION MECHANISM
    SHIMADA, J
    REVIEW OF THE ELECTRICAL COMMUNICATIONS LABORATORIES, 1969, 17 (10): : 1146 - &
  • [35] Photo- and thermo-oxidative degradation of photocrosslinked ethylene-propylene-diene terpolymer
    Wang, WZ
    Qu, BJ
    POLYMER DEGRADATION AND STABILITY, 2003, 81 (03) : 531 - 537
  • [36] Synthesis and thermo-oxidative degradation of acyclic polyimides
    Ochirov, Boris D.
    Gorenskaia, Elena N.
    Kholkhoev, Bato Ch
    Ayurova, Oksana Zh
    Burdukovskii, Vitalii F.
    POLYMER, 2020, 205 (205)
  • [37] THERMO-OXIDATIVE DEGRADATION OF POLYOLEFINS .2.
    IRING, R
    KELEN, T
    TUDOS, F
    MAGYAR KEMIAI FOLYOIRAT, 1975, 81 (07): : 298 - 304
  • [38] Kinetic features of the nonisothermal oxidative degradation of ethylene vinyl acetate copolymers
    Ruban, LV
    Sychugova, OV
    Kolesnikova, NN
    Zaikov, GE
    JOURNAL OF APPLIED POLYMER SCIENCE, 2004, 91 (03) : 1958 - 1961
  • [40] Local thermo-oxidative degradation in injection molding
    Schmiederer, Dirk
    Gardocki, Aleksander
    Kuehnert, Ines
    Schmachtenberg, Ernst
    POLYMER ENGINEERING AND SCIENCE, 2008, 48 (04): : 717 - 722