The behavior and mechanism of void self-shrinkage in diffusion bonded 1Cr11Ni2W2MoV steel joint: Effect of temperature and void morphology

被引:8
|
作者
Zhang, C. [1 ,2 ]
Li, M. Q. [1 ]
Li, H. [1 ]
机构
[1] Northwestern Polytech Univ, State Key Lab Solidificat Proc, Xian 710072, Peoples R China
[2] CNRS, INSA Lyon, LaMCoS, Dept Mech Engn, 20 Ave Sci, F-69621 Villeurbanne, France
基金
中国国家自然科学基金;
关键词
Diffusion bonding; Void self-shrinkage; Heat treatment; Steel; Void morphology; FRICTION WELDED-JOINT; HEAT-EXCHANGER; ALUMINUM-ALLOY; MICROSTRUCTURE; STRENGTH; INTERLAYER;
D O I
10.1016/j.jmapro.2018.07.017
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The aim of this study was to investigate the void self-shrinkage behavior and mechanism in the diffusion bonded 1Cr11Ni2W2MoV martensitic stainless steel joint. Two void morphologies, i.e., ellipse and long penny-shaped voids, were firstly manufactured by two kinds of prepared surfaces using diffusion bonding, and then heat treated at different temperatures. Results showed that for the ellipse voids the void self-shrinkage behavior hardly occurred at the lower heat treatment temperatures of 700 degrees C and 800 degrees C, while it occurred to transform the ellipse voids into smaller round voids at the higher temperatures of 900 degrees C and 1000 degrees C. For the penny-shaped voids, there was no obvious void self-shrinkage at the temperatures of 800 degrees C and 900 degrees C, while the void self-shrinkage was greatly improved at the temperature of 1000 degrees C. Joint shear strength could be significantly improved by the void self-shrinkage behavior. The void self-shrinkage mechanism was also analyzed, indicating that the void self-shrinkage behavior only occurred when the sum of internal driving force and external driving force was greater than the resistance for void self-shrinkage. The void self-shrinkage was mainly operated by diffusion of atoms, in which surface diffusion altered the void morphology, and grain boundary diffusion and volume diffusion reduced the void volume. Relative to ellipse voids, the void self-shrinkage of penny-shaped voids occurred at higher temperature due to the lack of surface diffusion.
引用
收藏
页码:71 / 78
页数:8
相关论文
共 50 条
  • [31] Diffusion bonding between nickel-base superalloy K24 and heat-resisting steel 1Cr11Ni2W2MoV
    ZHANG Jie
    ZHANG Jiuhai
    HAN Wenbo and LI Zhuoran(Measuring and Analysis Center
    China Welding, 1996, (02) : 89 - 95
  • [32] Diffusion bonding between nickel-base superalloy K24 and heat-resisting steel 1Cr11Ni2W2MoV
    ZHANG Jie
    ZHANG Jiuhai
    HEN Wenbo
    LI Zhuoran (Measuring and Analysis Center
    China Welding, 1997, (02) : 89 - 95
  • [33] Microstructural characteristics and erosion resistance of laser cladding Stellite 6 alloy on an 1Cr11Ni2W2MoV steel surface
    Chen, Meng
    An, Yinmin
    Wang, Quanbo
    Xu, Youwei
    Shi, Yu
    ENGINEERING FAILURE ANALYSIS, 2025, 168
  • [34] Process Parameters Optimization of Plasma Nitriding Depth of 1Cr11Ni2W2MoV Stainless Steel: Experimental and Simulation Studies
    Shiwei Guan
    Guifa Li
    Qiang Shi
    Linjie Zuo
    Yixin Xiao
    Haizhong Zheng
    Ping Peng
    JOM, 2024, 76 : 1937 - 1950
  • [35] 回火温度对1Cr11Ni2W2MoV钢冲击性能的影响
    孙奇
    张立新
    韦廷立
    张颖
    于湃
    刘天钊
    张闯
    理化检验(物理分册), 2017, 53 (03) : 165 - 168
  • [36] 1Cr11Ni2W2MoV钢制压气机叶片彩虹斑点故障分析
    唐恩军
    晁国涛
    王轶
    航空维修与工程, 2018, (10) : 79 - 82
  • [37] 1Cr11Ni2W2MoV不锈钢气体渗氮工艺研究
    王铮
    王大宏
    张金卓
    孙小琪
    王占鸿
    晁耀杰
    费岩晗
    金属加工(热加工), 2024, (06) : 23 - 28
  • [38] STUDY ON VOID HEALING BEHAVIOR DURING FORGING PROCESS FOR 25Cr2Ni4MoV STEEL
    Li Shijian
    Sun Mingyue
    Liu Hongwei
    Li Dianzhong
    ACTA METALLURGICA SINICA, 2011, 47 (07) : 946 - 953
  • [39] Process Parameters Optimization of Plasma Nitriding Depth of 1Cr11Ni2W2MoV Stainless Steel: Experimental and Simulation Studies
    Guan, Shiwei
    Li, Guifa
    Shi, Qiang
    Zuo, Linjie
    Xiao, Yixin
    Zheng, Haizhong
    Peng, Ping
    JOM, 2024, 76 (04) : 1937 - 1950
  • [40] 1Cr11Ni2W2MoV闪光对焊接头的组织与性能
    王金雪
    袁鸿
    张国栋
    余槐
    焊接, 2015, (04) : 58 - 60+76