The behavior and mechanism of void self-shrinkage in diffusion bonded 1Cr11Ni2W2MoV steel joint: Effect of temperature and void morphology

被引:8
|
作者
Zhang, C. [1 ,2 ]
Li, M. Q. [1 ]
Li, H. [1 ]
机构
[1] Northwestern Polytech Univ, State Key Lab Solidificat Proc, Xian 710072, Peoples R China
[2] CNRS, INSA Lyon, LaMCoS, Dept Mech Engn, 20 Ave Sci, F-69621 Villeurbanne, France
基金
中国国家自然科学基金;
关键词
Diffusion bonding; Void self-shrinkage; Heat treatment; Steel; Void morphology; FRICTION WELDED-JOINT; HEAT-EXCHANGER; ALUMINUM-ALLOY; MICROSTRUCTURE; STRENGTH; INTERLAYER;
D O I
10.1016/j.jmapro.2018.07.017
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The aim of this study was to investigate the void self-shrinkage behavior and mechanism in the diffusion bonded 1Cr11Ni2W2MoV martensitic stainless steel joint. Two void morphologies, i.e., ellipse and long penny-shaped voids, were firstly manufactured by two kinds of prepared surfaces using diffusion bonding, and then heat treated at different temperatures. Results showed that for the ellipse voids the void self-shrinkage behavior hardly occurred at the lower heat treatment temperatures of 700 degrees C and 800 degrees C, while it occurred to transform the ellipse voids into smaller round voids at the higher temperatures of 900 degrees C and 1000 degrees C. For the penny-shaped voids, there was no obvious void self-shrinkage at the temperatures of 800 degrees C and 900 degrees C, while the void self-shrinkage was greatly improved at the temperature of 1000 degrees C. Joint shear strength could be significantly improved by the void self-shrinkage behavior. The void self-shrinkage mechanism was also analyzed, indicating that the void self-shrinkage behavior only occurred when the sum of internal driving force and external driving force was greater than the resistance for void self-shrinkage. The void self-shrinkage was mainly operated by diffusion of atoms, in which surface diffusion altered the void morphology, and grain boundary diffusion and volume diffusion reduced the void volume. Relative to ellipse voids, the void self-shrinkage of penny-shaped voids occurred at higher temperature due to the lack of surface diffusion.
引用
收藏
页码:71 / 78
页数:8
相关论文
共 50 条
  • [21] 激光冲击处理1Cr11Ni2W2MoV不锈钢
    曹子文
    邹世坤
    刘方军
    樊国福
    刘元春
    中国激光, 2008, (02) : 316 - 320
  • [22] 1Cr11Ni2W2MoV模锻件耐蚀性改进工艺
    孙小岚
    杨堃
    电镀与涂饰, 2021, 40 (06) : 405 - 409
  • [23] 1Cr11Ni2W2MoV不锈钢气体渗碳工艺
    杨亚宁
    张波
    卢华
    热加工工艺, 2011, 40 (10) : 197 - 198
  • [24] 1Cr11Ni2W2MoV压缩机叶片表面缺陷分析
    吴勇军
    特钢技术, 2007, (01) : 15 - 17+46
  • [25] 酸性环境下1Cr11Ni2W2MoV钢腐蚀防护研究
    张林嘉
    王江
    张安琴
    高军
    尹翔
    肖钦夤
    全面腐蚀控制, 2024, 38 (10) : 200 - 204
  • [26] 1Cr11Ni2W2MoV钢的碳氮共渗研究
    吴运新
    朱张校
    丁连珍
    朱允明
    金属热处理, 1993, (08) : 7 - 9+18
  • [27] 1Cr11Ni2W2MoV不锈钢细长轴加工工艺
    陈卫林
    常星星
    李红进
    高茂洋
    金属加工(冷加工), 2024, (06) : 20 - 23
  • [28] 1Cr11Ni2W2MoV钢高压涡轮轴裂纹形成原因
    李欣
    詹平
    全琼蕊
    理化检验-物理分册, 2023, 59 (02) : 54 - 57+62
  • [29] 1Cr11Ni2W2MoV钢真空正压气淬热处理
    莫卫红
    航空制造技术, 2000, (03) : 53 - 55
  • [30] Diffusion bonding between nickel-base superalloy K24 and heat-resisting steel 1Cr11Ni2W2MoV
    Zhang, Jie
    Zhang, Jiuhai
    Han, Wenbo
    Li, Zhuoran
    China Welding, 1996, 5 (02):