摘要
Mechanical strength of low-k material greatly decreases; material composition change will also give dry etching a lot of problems which have never met before. This paper explores the approaches to solve new problems when plasma etching low-k material, such as avoiding low-k damage and other defects, keeping anisotropic and needed selectivity; finding out the process parameters with the biggest influence, such as gas species, pressure, RF frequency, power, etc. Applies the process trend to plasma etching low-k material (BD) of 40nm dual damascene trench etch and achieves the critical target.
引用
收藏
页码:395 / 398
页数:4
相关论文
共 50 条
  • [41] TDDB characteristics of low-k dielectrics after plasma damage recovery process
    Imada, T.
    Nakata, Y.
    Ozaki, S.
    Kobayashi, Y.
    Yoshikawa, K.
    Nakamura, T.
    ADVANCED METALLIZATION CONFERENCE 2007 (AMC 2007), 2008, 23 : 557 - 561
  • [42] Resisting oxygen plasma damage in low-k hydrogen silsesquioxane films by hydrogen plasma treatment
    Singh, SK
    Kumbhar, AA
    Dusane, RO
    MATERIALS LETTERS, 2006, 60 (13-14) : 1579 - 1581
  • [43] Plasma processing of low-k dielectrics
    Baklanov, Mikhail R.
    de Marneffe, Jean-Francois
    Shamiryan, Denis
    Urbanowicz, Adam M.
    Shi, Hualiang
    Rakhimova, Tatyana V.
    Huang, Huai
    Ho, Paul S.
    JOURNAL OF APPLIED PHYSICS, 2013, 113 (04)
  • [44] Optical emission diagnostics of etching of low-k dielectrics in a two frequency inductively coupled plasma
    Miyauchi, M.
    Miyoshi, Y.
    Petrovic, Z. Lj.
    Makabe, T.
    SOLID-STATE ELECTRONICS, 2007, 51 (10) : 1418 - 1424
  • [45] Investigation of surface roughening of low-k films during etching using fluorocarbon plasma beams
    Yin, Yunpeng
    Rasgon, Stacy
    Sawin, Herbert H.
    JOURNAL OF VACUUM SCIENCE & TECHNOLOGY B, 2006, 24 (05): : 2360 - 2371
  • [46] Comparative study of SiOCH low-k films with varied porosity interacting with etching and cleaning plasma
    Shamiryan, D
    Baklanov, MR
    Vanhaelemeersch, S
    Maex, K
    JOURNAL OF VACUUM SCIENCE & TECHNOLOGY B, 2002, 20 (05): : 1923 - 1928
  • [47] Effects of etch rate on plasma-induced damage to porous low-k films
    Iba, Yoshihisa
    Kirimura, Tomoyuki
    Sasaki, Makoto
    Kobayashi, Yasushi
    Nakata, Yoshihiro
    Nakaishi, Masafumi
    Japanese Journal of Applied Physics, 2008, 47 (8 PART 3): : 6923 - 6930
  • [48] Plasma damage and repair of porous low-k carbon-doped oxide films
    Yoo, Hui Jae
    Bielefeld, Jeffery D.
    Balakrishnan, Sridhar
    Boyanov, Boyan
    Clendenning, Scott B.
    Kloster, Grant M.
    Paluda, Patrick M.
    RamachandraRao, Vijayakumar S.
    Suri, Satyarth
    Younkin, Todd R.
    ADVANCED METALLIZATION CONFERENCE 2007 (AMC 2007), 2008, 23 : 705 - 709
  • [49] Toward Successful Integration of Porous Low-k Materials: Strategies Addressing Plasma Damage
    Lionti, K.
    Volksen, W.
    Magbitang, T.
    Darnon, M.
    Dubois, G.
    ECS JOURNAL OF SOLID STATE SCIENCE AND TECHNOLOGY, 2015, 4 (01) : N3071 - N3083
  • [50] Meeting ITRS Roadmap challenges with low-k dielectric etching
    Thomas, DJ
    Song, YP
    Powell, K
    SOLID STATE TECHNOLOGY, 2001, 44 (03) : 107 - +