The Effect of Sintering Temperature on Mesoporous Structure of WO3 Doped Tio2 Powders

被引:3
|
作者
Petrovic, Srdan [1 ]
Rozic, Ljiljana [1 ]
Stojadinovic, Stevan [2 ]
Grbic, Bosko [1 ]
Vasilic, Rastko [2 ]
Vukovic, Zorica [1 ]
Radic, Nenad [1 ]
机构
[1] Univ Belgrade, IChTM Dept Catalysis & Chem Engn, Njegoseva 12, Belgrade, Serbia
[2] Univ Belgrade, Fac Phys, Studentski Trg 12-16, Belgrade 11000, Serbia
关键词
WOx-TiO2; powders; Sintering; Mesoporous structure; Photocatalytic; degradation; Azo dye; PLASMA ELECTROLYTIC OXIDATION; SOL-GEL SYNTHESIS; PHOTOCATALYTIC DEGRADATION; SURFACE-AREA; TIO2; NITROGEN; ANATASE; TITANIUM; FILMS;
D O I
10.2298/SOS1801123P
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
In this study, WO3 doped TiO2 powders were synthesized via sol-gel method combined with a hydrothermal process. The effect of sintering temperature on mesoporous structure and catalytic activities of these powders were investigated. The physical analysis via X-ray diffraction indicates that prepared samples are a mixture of anatase and rutile TiO2 phases. X-ray peak analysis is used to evaluate the crystallite size and lattice strain by the Williamson-Hall analysis. Considering all the reflections of the anatase phase the lattice strain ranging from c = 9.505 to c = 9.548 is calculated, suggesting that microstrain decreases when calcination temperature increases. N-2 adsorption-desorption analysis shows that the surface area and pore volume decrease with increasing temperature and that WOx-TiO2 powders primarily consist of mesopores. Sintering temperature induced a change in textural properties causing a systematic shift towards larger mesopores. Simultaneously, photoactivity in decolorization of methyl orange increases with increasing calcination temperature up to 700 degrees C, followed by significant decrease with its further increase.
引用
收藏
页码:123 / 132
页数:10
相关论文
共 50 条
  • [41] PREPARATION AND CHARACTERIZATION OF DOPED WO3 PHOTOCATALYST POWDERS
    ASHOKKUMAR, M
    MARUTHAMUTHU, P
    JOURNAL OF MATERIALS SCIENCE, 1989, 24 (06) : 2135 - 2139
  • [42] EPR study of nitrogen-doped mesoporous TiO2 powders
    Mei, P.
    Henderson, M.
    Kassiba, A.
    Gibaud, A.
    JOURNAL OF PHYSICS AND CHEMISTRY OF SOLIDS, 2010, 71 (01) : 1 - 6
  • [43] The research on the high quality TiO2, MoO3-doped WO3 electrochromic film
    Luo, Wei
    Fu, Xiang Kai
    Ma, Li Hua
    CHINESE CHEMICAL LETTERS, 2007, 18 (07) : 883 - 886
  • [45] Controllable synthesis of highly crystallized mesoporous TiO2/WO3 heterojunctions for acetone gas sensing
    Wang, Changyao
    Li, Yuhui
    Qiu, Pengpeng
    Duan, Linlin
    Bi, Wei
    Chen, Yan
    Guo, Dingyi
    Liu, Yupu
    Luo, Wei
    Deng, Yonghui
    CHINESE CHEMICAL LETTERS, 2020, 31 (05) : 1119 - 1123
  • [46] Synthesis of mesoporous WO3/TiO2 catalyst and its excellent catalytic performance for the oxidation of dibenzothiophene
    Qin, Yuejiao
    Xun, Suhang
    Zhan, Liangliang
    Lu, Qingqing
    He, Minqiang
    Jiang, Wei
    Li, Hongping
    Zhang, Ming
    Zhu, Wenshuai
    Li, Huaming
    NEW JOURNAL OF CHEMISTRY, 2017, 41 (02) : 569 - 578
  • [47] Effect of WO3 on the structure and properties of low sintering temperature and high strength vitrified bonds
    Han, J.
    He, F.
    Wang, L.L.
    Zhang, L.X.
    Ye, C.Q.
    Xie, J.L.
    Mei, S.X.
    Jin, M.F.
    Journal of Alloys and Compounds, 2016, 679 : 54 - 58
  • [48] Effect of WO3 on the structure and properties of low sintering temperature and high strength vitrified bonds
    Han, J.
    He, F.
    Wang, L. L.
    Zhang, L. X.
    Ye, C. Q.
    Xie, J. L.
    Mei, S. X.
    Jin, M. F.
    JOURNAL OF ALLOYS AND COMPOUNDS, 2016, 679 : 54 - 58
  • [49] Structure and Photocatalytic Properties of WO3/TiO2 Composite Film by Microarc Oxidation
    He Jian
    Cai Qizhou
    Xiao Feng
    Luo Qiang
    Wang Lijuan
    Zhu Di
    CHINESE JOURNAL OF CATALYSIS, 2009, 30 (11) : 1137 - 1142
  • [50] Sol–gel synthesis of mesoporous WO3–TiO2 composite thin films for photochromic devices
    Yahia Djaoued
    Subramanian Balaji
    Normand Beaudoin
    Journal of Sol-Gel Science and Technology, 2013, 65 : 374 - 383