Influence of particles in Cu-Al2O3 system on fracture mechanism

被引:2
|
作者
Besterci, M
Ivan, J
Kovac, L
机构
[1] Slovak Acad Sci, Inst Mat Res, Kosice 04353, Slovakia
[2] SAS, Inst Mat & Mech Machines, Bratislava 83008, Slovakia
关键词
fracture mechanism; in situ tensile test in SEM; Cu-Al2O3; dispersion strengthened system;
D O I
10.1016/S0921-5093(00)02030-X
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
The influence of Al2O3 particles on fracture of the Cu-Al2O3 system is analyzed by 'in situ tensile test in SEM'. It has been shown, that tensile strain in the extrusion direction produced first micro cavities on matrix-particle interfaces due to decohesion of particles from the matrix. The cavities grow and coalesce first in the direction of rows of particles with growing strain, and then in direction perpendicular to the rows, leading to final fracture. The strain at fracture is dependent on Al2O3 particle volume fraction. The fracture mechanism is not dependent on Al2O3 particle volume fraction in the tested range. Model explaining the fracture mechanism was introduced. (C) 2001 Elsevier Science B.V. All rights reserved.
引用
收藏
页码:667 / 670
页数:4
相关论文
共 50 条
  • [41] Structure and strength of rapidly quenched Cu-Al2O3 composites
    Il'insky, AI
    Terletsky, AS
    Zozulya, EW
    PROPERTIES AND PROCESSING OF VAPOR-DEPOSITED COATINGS, 1999, 555 : 279 - 281
  • [42] Structure and strength of rapidly quenched Cu-Al2O3 composites
    Department of Materials Science, Kharkov State Polytechnic University, Frunze Street 21, Kharkov, Ukraine
    Mater Res Soc Symp Proc, (279-281):
  • [43] Fabrication of Cu-Al2O3/ceramic particles by using brick particles as supports for highly-efficient selenium adsorption
    Wu, Jieyi
    Huang, Xueyun
    Chen, Hao
    Gou, Mei
    Zhang, Tao
    JOURNAL OF ENVIRONMENTAL CHEMICAL ENGINEERING, 2021, 9 (02):
  • [44] Process and progress of sintering behavior of Cu-Al2O3 composites
    Dash, K.
    Panda, S.
    Ray, B. C.
    EMERGING MATERIALS RESEARCH, 2013, 2 (01) : 32 - 38
  • [45] The oxidation behavior of an ODS copper alloy Cu-Al2O3
    Ogbuji, LU
    OXIDATION OF METALS, 2004, 62 (3-4): : 141 - 151
  • [46] THERMOCHEMICAL SYNTHESIS OF NANOSTRUCTURED Cu-Al2O3 COMPOSITE POWDER
    Seyedraoufi, Z. S.
    Saghafian, H.
    Shabestari, S. G.
    CHEMICAL INDUSTRY & CHEMICAL ENGINEERING QUARTERLY, 2014, 20 (03) : 339 - 344
  • [47] Nanostructured Cu-Al2O3 composite produced by thermochemical process
    Lee, DW
    Baek, JH
    Kim, BK
    Advances in Refractories for the Metallurgical Industries IV, 2004, : 757 - 765
  • [48] Microstructural parameters of Cu-Al2O3 dispersion strengthened materials
    Besterci, M.
    Velgosová, O.
    Leško, A.
    Kohátek, I.
    Materials Science Forum, 2003, 416-418 (01) : 35 - 40
  • [49] Research on Jet Electrodeposited Cu-Al2O3 Nanocomposition Coatings
    Chen, Jinsong
    Huang, Yinhui
    Qiao, Bin
    Yang, Jianming
    He, Yiqiang
    ADVANCES IN ENGINEERING DESIGN AND OPTIMIZATION, PTS 1 AND 2, 2011, 37-38 : 1041 - +
  • [50] Microstructural parameters of dispersion strengthened Cu-Al2O3 materials
    Besterci, Michal
    Kohutek, Ivan
    Velgosova, Oksana
    JOURNAL OF MATERIALS SCIENCE, 2008, 43 (03) : 900 - 905