Effects of steam concentration and flow rate on the high temperature oxidation of PEO-coated zirconium alloy at 1000 °C and 1200 °C

被引:3
|
作者
Guan, Haohao [1 ,2 ]
Wang, Xingping [1 ,2 ]
Xu, Chi [1 ,2 ]
Liao, Yizhao [1 ,2 ]
Gao, Chuanli [1 ,2 ]
Du, Jiancheng [1 ,2 ]
Jin, Xiaoyue [2 ]
Xue, Wenbin [1 ,2 ]
Zhang, Jinlong [3 ]
机构
[1] Beijing Normal Univ, Coll Nucl Sci & Technol, Key Lab Beam Technol, Minist Educ, Beijing 100875, Peoples R China
[2] Beijing Acad Sci & Technol, Inst Radiat Technol, Beijing 100875, Peoples R China
[3] Shanghai Univ, Inst Mat, Shanghai 200072, Peoples R China
来源
基金
中国国家自然科学基金;
关键词
ZIRLO zirconium alloy; High-temperature steam oxidation; Plasma electrolytic oxidation; Steam flow rate; Steam concentration; ZIRCALOY-4; BEHAVIOR; OXIDE; ZR-1NB-1SN-0.1FE; ELECTROLYTE; ENVIRONMENT; RESISTANCE; MORPHOLOGY; MIXTURES; KINETICS;
D O I
10.1016/j.surfcoat.2022.128896
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
A compact oxide coating of 7 mu m thick on ZIRLO zirconium alloy was fabricated by plasma electrolytic oxidation (PEO) in phosphate electrolyte. The effects of steam concentration and flow rate on the steam oxidation behavior of PEO-coated ZIRLO alloy at 1000 degrees C and 1200 degrees C were evaluated by thermogravimetric analysis (TGA). The morphologies, compositions, phase constituents before and after the steam oxidation were characterized. It is found that the critical steam concentration without steam starvation for PEO-coated ZIRLO alloy at 50 ml/min flow rate is 35 % at 1000 degrees C. Meanwhile, the critical flow rate at 50 % steam concentration is 35 ml/min at 1000 degrees C and 150 ml/min at 1200 degrees C. A dimensionless number (P = 39) is suggested corresponding to the critical steam concentration and flow rate. It means that the minimum mass of steam injection is about 39 per unit mass gain of sample, in order to avoid the steam starvation for Zr alloys after 3600 s steam exposure. The steam oxide layers consist of monoclinic zirconia (M-ZrO2) and a little tetragonal zirconia (T-ZrO2) phase at different temperatures, steam concentrations and flow rates. The hydrogen has not diffused into the steam oxide layer and ZIRLO substrate due to the hindrance of ZrO2 coating to the hydrogen diffusion.
引用
收藏
页数:12
相关论文
共 50 条
  • [41] Oxidation behavior of Zr-2.5Nb alloy exposed to steam in the temperature range of 600-1200 °C
    Krishna, V. S. V. Anantha
    Nouduru, Sai Karthik
    Mandapaka, Kiran K.
    Ahmedabadi, Parag M.
    Abraham, Geogy J.
    Shukla, S.
    Roychowdhury, S.
    Kain, V.
    JOURNAL OF NUCLEAR MATERIALS, 2024, 592
  • [42] THE OXIDATION OF PURE ZIRCONIUM IN STEAM FROM 1000-DEGREES TO 1416-DEGREES-C
    PAWEL, RE
    CAMPBELL, JJ
    JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1981, 128 (09) : 1999 - 2005
  • [43] Evolution of the oxidation behaviors of highly oxidation-resistant (Ti0.8Nb0.2)C in 1000-1200 °C steam
    Yu, Dan
    Tan, Yongqiang
    RSC ADVANCES, 2022, 12 (32) : 20492 - 20498
  • [44] Effect of the 345 °C and 16.5 MPa autoclave corrosion on the oxidation behavior of Cr-coated zirconium claddings in the high-temperature steam
    Liu, Haiyong
    Feng, Yajie
    Yao, Yirong
    Li, Bingsheng
    Wang, Renda
    Shi, Xiaoguang
    Li, Peng
    Shu, Jie
    Huang, Feng
    Huang, Qing
    Ge, Fangfang
    CORROSION SCIENCE, 2021, 189
  • [45] Oxidation Behaviors of Zr-Sn-Nb Alloy in 1000∼1250 °C Steam
    Zhang Feng
    Zhang Chengyu
    Zhao Wanqian
    Zhang Yao
    Chen Le
    Li Mei
    Song Pengcheng
    RARE METAL MATERIALS AND ENGINEERING, 2021, 50 (10) : 3677 - 3683
  • [46] High-temperature steam oxidation of (Ti, Mo)C-forming FeCrAlY alloy
    Kim, Sungyu
    Lee, Chang-Hoon
    Jang, Jae Hoon
    Moon, Joonho
    Kim, Ji Hyun
    Bahn, Chi Bum
    JOURNAL OF NUCLEAR MATERIALS, 2023, 574
  • [47] Oxidation resistance of Mo/Cr bilayer coating on Zr alloy in a 1200 °C steam environment
    Wang, Zheng
    Zhang, Yingpeng
    Zhou, Shenghao
    Wang, Zhenyu
    Yao, Yirong
    Wang, Aiying
    Li, Ming
    Ke, Peiling
    CORROSION COMMUNICATIONS, 2024, 14 : 49 - 57
  • [48] HIGH TEMPERATURE STEAM CORROSION OF MICROARC OXIDATION COATINGS ON 6061 ALUMINUM ALLOY AT 300°C/3 MPa STEAM
    Qu, Yao
    Yang, Chaolin
    Jin, Xiaoyue
    Du, Jiancheng
    Xue, Wenbin
    SURFACE REVIEW AND LETTERS, 2021, 28 (01)
  • [49] High temperature oxidation behaviour of mullite coated C/C composites in air
    Fritze, H
    Lenk, A
    Witke, T
    Weber, S
    Scherrer, S
    Weiss, R
    Schultrich, B
    Borchardt, G
    HIGH TEMPERATURE CORROSION AND PROTECTION OF MATERIALS 4, PTS 1 AND 2, 1997, 251-2 : 909 - 915
  • [50] High temperature oxidation behavior of SiC-coated C/C composites
    Aoki, T
    Hatta, H
    Kogo, Y
    Fukuda, H
    Goto, Y
    Yarii, T
    JOURNAL OF THE JAPAN INSTITUTE OF METALS, 1998, 62 (04) : 404 - 412