Effects of steam concentration and flow rate on the high temperature oxidation of PEO-coated zirconium alloy at 1000 °C and 1200 °C

被引:3
|
作者
Guan, Haohao [1 ,2 ]
Wang, Xingping [1 ,2 ]
Xu, Chi [1 ,2 ]
Liao, Yizhao [1 ,2 ]
Gao, Chuanli [1 ,2 ]
Du, Jiancheng [1 ,2 ]
Jin, Xiaoyue [2 ]
Xue, Wenbin [1 ,2 ]
Zhang, Jinlong [3 ]
机构
[1] Beijing Normal Univ, Coll Nucl Sci & Technol, Key Lab Beam Technol, Minist Educ, Beijing 100875, Peoples R China
[2] Beijing Acad Sci & Technol, Inst Radiat Technol, Beijing 100875, Peoples R China
[3] Shanghai Univ, Inst Mat, Shanghai 200072, Peoples R China
来源
基金
中国国家自然科学基金;
关键词
ZIRLO zirconium alloy; High-temperature steam oxidation; Plasma electrolytic oxidation; Steam flow rate; Steam concentration; ZIRCALOY-4; BEHAVIOR; OXIDE; ZR-1NB-1SN-0.1FE; ELECTROLYTE; ENVIRONMENT; RESISTANCE; MORPHOLOGY; MIXTURES; KINETICS;
D O I
10.1016/j.surfcoat.2022.128896
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
A compact oxide coating of 7 mu m thick on ZIRLO zirconium alloy was fabricated by plasma electrolytic oxidation (PEO) in phosphate electrolyte. The effects of steam concentration and flow rate on the steam oxidation behavior of PEO-coated ZIRLO alloy at 1000 degrees C and 1200 degrees C were evaluated by thermogravimetric analysis (TGA). The morphologies, compositions, phase constituents before and after the steam oxidation were characterized. It is found that the critical steam concentration without steam starvation for PEO-coated ZIRLO alloy at 50 ml/min flow rate is 35 % at 1000 degrees C. Meanwhile, the critical flow rate at 50 % steam concentration is 35 ml/min at 1000 degrees C and 150 ml/min at 1200 degrees C. A dimensionless number (P = 39) is suggested corresponding to the critical steam concentration and flow rate. It means that the minimum mass of steam injection is about 39 per unit mass gain of sample, in order to avoid the steam starvation for Zr alloys after 3600 s steam exposure. The steam oxide layers consist of monoclinic zirconia (M-ZrO2) and a little tetragonal zirconia (T-ZrO2) phase at different temperatures, steam concentrations and flow rates. The hydrogen has not diffused into the steam oxide layer and ZIRLO substrate due to the hindrance of ZrO2 coating to the hydrogen diffusion.
引用
收藏
页数:12
相关论文
共 50 条
  • [21] Microstructural characteristics and different effects of 800-1200° preformed oxides on high-temperature steam oxidation of a zirconium alloy cladding
    Lee, Cheol Min
    Jeong, Hu Yeong
    Yoon, Aram
    Mok, Yong-Kyoon
    Sohn, Dong-Seong
    JOURNAL OF ALLOYS AND COMPOUNDS, 2018, 753 : 119 - 129
  • [22] HIGH TEMPERATURE OXIDATION OF POLYCRYSTALLINE DIAMOND COATED ZIRCONIUM ALLOY
    Skarohlid, Jan
    Skoda, Radek
    Kratochvilova, Irena
    PROCEEDINGS OF THE 24TH INTERNATIONAL CONFERENCE ON NUCLEAR ENGINEERING, 2016, VOL 5, 2016,
  • [23] Microstructural evolution of intermetallic phase precipitates in Cr-coated Zirconium alloy cladding in high-temperature steam oxidation up to 1400 °C
    Mohamad, Afiqa
    Nemoto, Yoshiyuki
    Furumoto, Kenichiro
    Okada, Yuji
    Sato, Daiki
    CORROSION SCIENCE, 2023, 224
  • [24] Reflood oxidation performances of Cr-coated Zr-Sn-Nb alloy cladding tubes at 1000 °C∼1200 °C
    Xiao, Weiwei
    Liu, Shihong
    Huang, Jinghao
    Zou, Shuliang
    JOURNAL OF NUCLEAR MATERIALS, 2024, 597
  • [25] High-temperature oxidation behavior of Ti2AlNb alloy with PEO/hBN composite coating at 1000 °C
    Wang, Shuaixing
    Liu, Xin
    Yin, Xiaole
    Zhang, Bangyan
    Du, Nan
    SURFACE & COATINGS TECHNOLOGY, 2020, 404
  • [26] High-temperature oxidation behavior of Inconel 693 alloy at 900 °C-1200 °C
    Liu, Tianyu
    Zhao, Qingbin
    Li, Yingju
    Meng, Xiangda
    Feng, Xiaohui
    Qu, Xiaorui
    Zheng, Ce
    Huang, Qiuyan
    Xu, Wenguo
    Yang, Yuansheng
    MATERIALS CHARACTERIZATION, 2023, 204
  • [27] High-temperature steam oxidation experiment of molten zirconium alloy
    Wang, Haoli
    Luo, Simin
    Zhao, Xinhai
    Zhang, Yapei
    Lan, Yicong
    Wu, Xiaocheng
    Wang, Dong
    Tian, Wenxi
    Qiu, Suizheng
    Su, G. H.
    CORROSION SCIENCE, 2024, 231
  • [28] Oxidation of Advanced Zirconium Cladding Alloys in Steam at Temperatures in the Range of 600–1200 °C
    Martin Steinbrück
    Nóra Vér
    Mirco Große
    Oxidation of Metals, 2011, 76 : 215 - 232
  • [29] High temperature oxidation of Zr-1Nb alloy with plasma electrolytic oxidation coating in 900-1200 °C steam environment
    Wang, Xingping
    Wei, Kejian
    Guan, Haohao
    Xu, Chi
    Xue, Wenbin
    Zhang, Yanwei
    Wang, Rongshan
    SURFACE & COATINGS TECHNOLOGY, 2021, 407
  • [30] Fiber texture-dependent oxidation behaviour of Cr-coated zirconium alloy in high temperature steam
    Wang, Yao
    Wang, Luhua
    Shang, Lunlin
    Bai, Guanghai
    Li, Jinshan
    Xue, Fei
    Gong, Weijia
    CORROSION SCIENCE, 2022, 205