Inhibited Cr(VI) formation in Cr2O3-containing refractory castable using reactive MgO as hydraulic binder

被引:14
|
作者
Guo, Liu [1 ]
Song, Shengqiang [2 ]
Mu, Yuandong [1 ]
Ye, Guotian [1 ]
Chen, Liugang [1 ]
机构
[1] Zhengzhou Univ, Sch Mat Sci & Engn, Henan Key Lab High Temp Funct Ceram, Zhengzhou 450001, Henan, Peoples R China
[2] Wuhan Univ Sci & Technol, State Key Lab Refractories & Met, Wuhan 430081, Peoples R China
基金
中国国家自然科学基金;
关键词
Cr(VI) inhibition; Reactive MgO; Refractory castable; Leaching; MICRO-SIZED MGCO3; HEXAVALENT CHROMIUM; MGAL2O4; SPINEL; HYDRATION; EVOLUTION; BEHAVIOR; LEACHABILITY; RESISTANCE; MECHANISM; CEMENTS;
D O I
10.1016/j.jeurceramsoc.2022.09.003
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Reactive MgO was used in the first time as alternative hydraulic binder of calcium aluminate cement (CAC) to prepare Cr2O3-bearing refractory castable. The formation of Cr(VI), and physical and mechanical properties of MgO-bonded refractory castables after heat-treating were investigated. Microstructural characterization and phase composition analyses on the heat-treated MgO-bonded refractory castable matrices resulted in a comprehensive understanding of the mechanism for the inhibition of Cr(VI), and of the strength development during firing. The results indicate that compared with CAC, Cr(VI) levels were 6.7-28.1 times lower using reactive MgO after firing at 700-1300 degrees C. The in situ Mg(Cr,Al)2O4 spinel formed from the preferential interactions among MgO and Cr2O3 and Al2O3 would be the main reason leading to the inhibited Cr(VI) formation and strength development during firing.
引用
收藏
页码:7656 / 7666
页数:11
相关论文
共 50 条
  • [31] Inhibition of Cr6+ by the formation of in-situ Cr3+ containing solid-solution in Al2O3-CaO-Cr2O3-SiO2 system
    Zhang, Wenke
    Song, Shengqiang
    Nath, Mithun
    Xue, Zhengliang
    Ma, Guojun
    Li, Yawei
    CERAMICS INTERNATIONAL, 2021, 47 (07) : 9578 - 9584
  • [32] INTERDIFFUSION STUDIES IN SYSTEM MGO-CR2O3
    GRESKOVICH, C
    STUBICAN, VS
    JOURNAL OF PHYSICS AND CHEMISTRY OF SOLIDS, 1969, 30 (04) : 909 - +
  • [33] EFFECT OF CR2O3 VAPORIZATION ON SINTERING OF MGO
    HENCH, LL
    RUSSELL, R
    TRANSACTIONS OF THE BRITISH CERAMIC SOCIETY, 1968, 67 (09): : 377 - &
  • [34] Dynamic corrosion of Al2O3-ZrO2-SiO2 and Cr2O3-containing refractories by molten frits. Part I: Macroscopic analysis
    Baudin, C.
    Criado, E.
    Bakali, J. J.
    Pena, P.
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2011, 31 (05) : 697 - 703
  • [35] The Effect of MgO-Al2O3 Spinel on Refractory Bricks Made from Al2O3-Cr2O3 Slag
    Zheng, Lijun
    Zhang, Guodong
    Qu, Dianli
    Liu, Feng
    MATERIALS PROCESSING TECHNOLOGY, PTS 1-4, 2011, 291-294 : 1795 - +
  • [36] Experimental Determination of CaO-CrO-Cr2O3-MgO-SiO2 and Thermodynamic Modeling of the CrO-Cr2O3-MgO-SiO2 System
    Arnout, Sander
    Guo, Muxing
    Jung, In-Ho
    Blanpain, Bart
    Wollants, Patrick
    JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 2009, 92 (08) : 1831 - 1839
  • [37] COHERENT PRECIPITATION IN SYSTEM MGO-AL2O3-CR2O3
    GRESKOVICH, C
    STUBICAN, VS
    JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1968, 51 (01) : 42 - +
  • [38] Solid solutions in the MgO-Al2O3-Cr2O3 system
    Turkin, A. I.
    Drebushchak, V. A.
    JOURNAL OF THERMAL ANALYSIS AND CALORIMETRY, 2009, 95 (01) : 81 - 86
  • [39] EFFECT OF YTTRIUM ON KINETICS OF NUCLEATION AND GROWTH OF CR2O3 AND AL2O3 LAYERS ON REFRACTORY ALLOYS CONTAINING FE, NI, CR AND AL
    PIVIN, JC
    ROQUESCARMES, C
    JOURNAL DE CHIMIE PHYSIQUE ET DE PHYSICO-CHIMIE BIOLOGIQUE, 1978, 75 (05) : 465 - 465
  • [40] Cr3+-Containing Carbonates and Cr2O3-Pbcn at Extreme Conditions
    Wang, Yu
    Bayarjargal, Lkhamsuren
    Bykov, Maxim
    Bykova, Elena
    Spahr, Dominik
    Glazyrin, Konstantin
    Milman, Victor
    Winkler, Bjoern
    INORGANIC CHEMISTRY, 2025, 64 (10) : 4996 - 5003