Inhibited Cr(VI) formation in Cr2O3-containing refractory castable using reactive MgO as hydraulic binder

被引:14
|
作者
Guo, Liu [1 ]
Song, Shengqiang [2 ]
Mu, Yuandong [1 ]
Ye, Guotian [1 ]
Chen, Liugang [1 ]
机构
[1] Zhengzhou Univ, Sch Mat Sci & Engn, Henan Key Lab High Temp Funct Ceram, Zhengzhou 450001, Henan, Peoples R China
[2] Wuhan Univ Sci & Technol, State Key Lab Refractories & Met, Wuhan 430081, Peoples R China
基金
中国国家自然科学基金;
关键词
Cr(VI) inhibition; Reactive MgO; Refractory castable; Leaching; MICRO-SIZED MGCO3; HEXAVALENT CHROMIUM; MGAL2O4; SPINEL; HYDRATION; EVOLUTION; BEHAVIOR; LEACHABILITY; RESISTANCE; MECHANISM; CEMENTS;
D O I
10.1016/j.jeurceramsoc.2022.09.003
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Reactive MgO was used in the first time as alternative hydraulic binder of calcium aluminate cement (CAC) to prepare Cr2O3-bearing refractory castable. The formation of Cr(VI), and physical and mechanical properties of MgO-bonded refractory castables after heat-treating were investigated. Microstructural characterization and phase composition analyses on the heat-treated MgO-bonded refractory castable matrices resulted in a comprehensive understanding of the mechanism for the inhibition of Cr(VI), and of the strength development during firing. The results indicate that compared with CAC, Cr(VI) levels were 6.7-28.1 times lower using reactive MgO after firing at 700-1300 degrees C. The in situ Mg(Cr,Al)2O4 spinel formed from the preferential interactions among MgO and Cr2O3 and Al2O3 would be the main reason leading to the inhibited Cr(VI) formation and strength development during firing.
引用
收藏
页码:7656 / 7666
页数:11
相关论文
共 50 条
  • [21] Formation and leachability of hexavalent chromium in the Al2O3-CaO-MgO-Cr2O3 system
    Wu, Yingjiang
    Song, Shengqiang
    Garbers-Craig, Andrie M.
    Xue, Zhengliang
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2018, 38 (06) : 2649 - 2661
  • [22] Binder Effect on Properties of Cr2O3-bearing Corundum-based Refractory Castables
    ZHANG Hongrui
    CHEN Liugang
    China's Refractories, 2023, 32 (03) : 36 - 41
  • [23] MECHANISMS OF FORMATION OF MGCR2O4 SPINEL FROM MGO AND CR2O3
    NAGATA, K
    NISHIWAKI, R
    MARUYAMA, T
    TETSU TO HAGANE-JOURNAL OF THE IRON AND STEEL INSTITUTE OF JAPAN, 1991, 77 (06): : 783 - 789
  • [24] PHASE EQUILIBRIA IN SYSTEMS NIO-CR2O3-O2 MGO-CR2O3-O2 AND CDO-CR2O3-O2 AT HIGH OXYGEN PRESSURES
    MULLER, O
    ROY, R
    WHITE, WB
    AMERICAN CERAMIC SOCIETY BULLETIN, 1967, 46 (04): : 367 - &
  • [25] PHASE EQUILIBRIA IN SYSTEMS NIO-CR2O3-O2 MGO-CR2O3-O2 AND CDO-CR2O3-O2 AT HIGH OXYGEN PRESSURES
    MULLER, O
    ROY, R
    WHITE, WB
    JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1968, 51 (12) : 693 - &
  • [26] Deterioration mechanism of Al2O3-MgO refractory castable in RH refining ladle
    Chen, Junfeng
    Zhang, Yu
    Liu, Guangping
    Wei, Guoping
    Zhao, Yi
    Yan, Wen
    Li, Nan
    OPEN CERAMICS, 2023, 16
  • [27] Dynamic corrosion of Al2O3-ZrO2-SiO2 and Cr2O3-containing refractories by molten frits. Part II: Microstructural study
    Pena, P.
    Criado, E.
    Bakali, J. J.
    Baudin, C.
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2011, 31 (05) : 705 - 714
  • [28] TEMPERATURE INTERACTIONS IN SYSTEM MGO-CR2O3
    KAKAZEI, MG
    MIKHEEV, VA
    SORIN, LO
    DOPOVIDI AKADEMII NAUK UKRAINSKOI RSR SERIYA A-FIZIKO-MATEMATICHNI TA TECHNICHNI NAUKI, 1974, (04): : 365 - 368
  • [29] MECHANISM OF INTERACTION BETWEEN MGO AND CR2O3
    BROSNAN, DA
    HULBERT, SF
    SMOAK, RH
    AMERICAN CERAMIC SOCIETY BULLETIN, 1968, 47 (04): : 426 - &
  • [30] VACUUM VAPORIZATION IN SYSTEM MGO-CR2O3
    SATA, T
    LEE, HL
    JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1978, 61 (7-8) : 326 - 329