Activation Energy of thermal Degradation of Tetrafluoroethylene-Propylene Elastomer

被引:0
|
作者
Ito, Masayuki [1 ]
Nozaki, Masahide [1 ]
Kosaka, Tomomi [1 ]
机构
[1] Tokyo Gakugei Univ, 4-1-4 Nukuikitamachi, Koganei, Tokyo 1848501, Japan
来源
KGK-KAUTSCHUK GUMMI KUNSTSTOFFE | 2022年 / 75卷 / 06期
关键词
Polyoxymethylene ISO 11358-2; ISO; 11358-3; Tetrafluoroethylene-propylene Elastomer; thermal Degradation; Activation Energy; Thermogravimetry;
D O I
暂无
中图分类号
TQ [化学工业];
学科分类号
0817 ;
摘要
The effect of the pre-aging at 250 degrees C before the measurement of thermogravimetry of tetrafluoroethylene-propylene elastomer was studied. The longer the pre-aging time, the more the linearity of the analyzed line with reference to ISO 11358-2 was improved. The activation energy of the sample aged 240 h was from 159 kJ/mol to 164 Id/mol, which was depending on the weight retained. The value obtained with reference to ISO 11358-3 was from 149 kJ/mol to 159 kJ/mol.