Delayed hydride cracking behavior of Zr-2.5Nb alloy pressure tubes for PHWR700

被引:13
|
作者
Sunil, S. [1 ]
Bind, A. K. [1 ]
Khandelwal, H. K. [1 ]
Singh, R. N. [1 ]
Chakravartty, J. K. [1 ]
机构
[1] Bhabha Atom Res Ctr, Mech Met Div, Bombay 400085, Maharashtra, India
关键词
Zr-2.5Nb alloy; PHWR700; Pressure tube; Delayed hydride cracking; STRESS INTENSITY FACTOR; ZIRCONIUM ALLOYS; HYDROGEN CONCENTRATION; PCT NB; FABRICATION; TEXTURE; MICROSTRUCTURE; TEMPERATURE; DEPENDENCE; REACTORS;
D O I
10.1016/j.jnucmat.2015.08.002
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
In order to attain improved in-reactor performance few prototypes pressure tubes of Zr-2.5Nb alloy were manufactured by employing forging to break the cast structure and to obtain more homogeneous microstructure. Both double forging and single forging were employed. The forged material was further processed by employing hot extrusion, cold pilgering and autoclaving. A detailed characterization in terms of mechanical properties and microstructure of the prototype tubes were carried for qualifying it for intended use as pressure tubes in PHWR700 reactors. In this work, Delayed Hydride Cracking (DHC) behavior of the forged Zr-2.5Nb pressure tube material characterized in terms of DHC velocity and threshold stress intensity factor associated with DHC (K-JH) was compared with that of conventionally manufactured material in the temperature range of 200-283 degrees C. Activation energy associated with the DHC in this alloy was found to be similar to 60 kymol for the forged materials. (C) 2015 Elsevier B.V. All rights reserved.
引用
收藏
页码:208 / 219
页数:12
相关论文
共 50 条
  • [41] Delayed hydride cracking velocity in Zr-2.5Nb: detection by acoustic emission and theoretical model testing
    J. I. Mieza
    G. Vigna
    E. Chomik
    G. Domizzi
    Journal of Materials Science, 2008, 43 : 4945 - 4952
  • [42] Delayed hydride cracking velocity of irradiated Zr-2.5Nb tubes after a 30-year operation in the Wolsong Unit 1
    Kim, YS
    Ahn, SB
    Im, KS
    Oh, WH
    PRICM 5: THE FIFTH PACIFIC RIM INTERNATIONAL CONFERENCE ON ADVANCED MATERIALS AND PROCESSING, PTS 1-5, 2005, 475-479 : 1409 - 1414
  • [43] Temperature dependence of the velocity of delayed hydride cracking in Zr-2.5% Nb Alloy
    Markelov V.A.
    Kotov P.V.
    Zheltkovskaya T.N.
    Inorganic Materials: Applied Research, 2010, 1 (03) : 217 - 224
  • [44] The transformation behaviour of the β-phase in Zr-2.5Nb pressure tubes
    Griffiths, M.
    Winegar, J. E.
    Buyers, A.
    JOURNAL OF NUCLEAR MATERIALS, 2008, 383 (1-2) : 28 - 33
  • [45] Threshold stress intensity factor for delayed hydride cracking in Zr-2.5%Nb pressure tube alloy
    Singh, R. N.
    Stahle, P.
    Chakravartty, J. K.
    Shmakov, A. A.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2009, 523 (1-2): : 112 - 117
  • [46] GETTERING OF HYDROGEN FROM ZR-2.5NB PRESSURE TUBES
    CANN, CD
    SEXTON, EE
    BAHURMUZ, AA
    WHITE, AJ
    BALNESS, HR
    LEDOUX, GA
    JOURNAL OF THE LESS-COMMON METALS, 1991, 172 : 1297 - 1305
  • [47] The development of Zr-2.5Nb pressure tubes for CANDU reactors
    Cheadle B.A.
    Journal of ASTM International, 2010, 7 (08):
  • [48] Manufacturing variability and deformation for Zr-2.5Nb pressure tubes
    Bickel, G. A.
    Griffiths, M.
    JOURNAL OF NUCLEAR MATERIALS, 2008, 383 (1-2) : 9 - 13
  • [49] Influence of metallurgical variables on delayed hydride cracking in Zr-Nb pressure tubes
    Cirimello, P
    Domizzi, G
    Haddad, R
    JOURNAL OF NUCLEAR MATERIALS, 2006, 350 (02) : 135 - 146
  • [50] Influence of metallurgical variables on delayed hydride cracking in Zr-Nb pressure tubes
    Domizzi, G.
    Haddad, R.
    JOURNAL OF NUCLEAR MATERIALS, 2008, 374 (1-2) : 331 - 333