Changes in Gloss Alteration, Surface Roughness, and Color of Direct Dental Restorative Materials after Professional Dental Prophylaxis

被引:3
|
作者
Miyashita-Kobayashi, Aya [1 ,2 ]
Haruyama, Akiko [3 ]
Nakamura, Keigo [2 ]
Wu, Chia-Ying [1 ,2 ]
Kuroiwa, Akihiro [4 ]
Yoshinari, Nobuo [1 ,2 ]
Kameyama, Atsushi [1 ,2 ]
机构
[1] Matsumoto Dent Univ, Grad Sch Oral Med, Dept Oral Hlth Promot, Shiojiri, Nagano 3990781, Japan
[2] Matsumoto Dent Univ, Sch Dent, Dept Operat Dent Endodontol & Periodontol, Shiojiri, Nagano 3990781, Japan
[3] Tokyo Dent Coll, Dept Operat Dent Cariol & Pulp Biol, Tokyo 1010061, Japan
[4] Matsumoto Dent Univ, Sch Dent, Dept Dent Mat Sci, Shiojiri, Nagano 3990781, Japan
关键词
resin-based composite; glass-ionomer cement; surface gloss; surface roughness; color change; 3D measuring laser microscopy; RESIN COMPOSITE; ORAL-HEALTH; BACTERIAL ADHESION; BIOFILM FORMATION; FLUORIDE RELEASE; SECONDARY CARIES; GLASS-IONOMER; CARE; STABILITY; INHIBITION;
D O I
10.3390/jfb15010008
中图分类号
R318 [生物医学工程];
学科分类号
0831 ;
摘要
In the context of optimizing dental care for patients who are elderly, the purpose of this in vitro study was to evaluate the surface gloss (with a micro-area gloss meter) of, surface roughness (with a compact surface roughness measuring instrument) of, and color change (with a dental colorimeter) in two commercially available injectable resin-based composites (Estelite Universal Flow (EUF) and Beautifil Flow Plus F00 (BFP)) as well as two glass-ionomer cements (GC Fuji II LC CAPSULE (FLC) and GC Fuji IX GP EXTRA CAPSULE (FGP)), before and after dental prophylaxis. After 24 h, the surfaces of each specimen were polished at 2500 rpm with a prophy brush (Mersage Brush, Shofu) and one-step prophylaxis paste (Prophy Paste Pro, Directa): under 100 or 300 gf load, and for 10 or 30 s, 4x cycles of cleaning. After mechanical cleaning, conditions were found for a significant reduction in the gloss level (EUF, BFP, or FLC; p < 0.05) and a significant increase in surface roughness (BFP; 300 gf load, 10 s x four cycles of cleaning). Overall, the longer time or higher prophylaxis load tended to decrease the surface gloss. However, the observed change in surface roughness varied between the restorative materials. There was no color change post-prophylaxis.
引用
收藏
页数:16
相关论文
共 50 条
  • [21] Surface roughness and hardness of some dental ceramics and restorative resins
    Karakaya, S
    Ünlü, N
    Öveçoglu, HS
    Özer, F
    EURO CERAMICS VIII, PTS 1-3, 2004, 264-268 : 2095 - 2098
  • [22] Effects of Dental Bleaching Agents on the Surface Roughness of Dental Restoration Materials
    Popescu, Alexandru Dan
    Tuculina, Mihaela Jana
    Diaconu, Oana Andreea
    Gheorghita, Lelia Mihaela
    Nicolicescu, Claudiu
    Cumpata, Cristian Niky
    Petcu, Cristiana
    Abdul-Razzak, Jaqueline
    Rica, Ana Maria
    Voinea-Georgescu, Ruxandra
    MEDICINA-LITHUANIA, 2023, 59 (06):
  • [23] Effect of dental restorative materials surface roughness on the in vitro biofilm formation of Streptococcus mutans biofilm
    Contreras-Guerrero, Paulina
    Ortiz-Magdaleno, Marine
    Salvador Urcuyo-Alvarado, Manuel
    Antonio Cepeda-Bravo, Juan
    Leyva-del Rio, Diana
    Elias Perez-Lopez, Jose
    Fernando Romo-Ramirez, Gabriel
    Octavio Sanchez-Vargas, Luis
    AMERICAN JOURNAL OF DENTISTRY, 2020, 33 (02): : 59 - 63
  • [24] Enhancing Esthetics in Direct Dental Resin Composite: Investigating Surface Roughness and Color Stability
    Hajdu, Adrian Ioan
    Dumitrescu, Ramona
    Balean, Octavia
    Lalescu, Dacian Virgil
    Buzatu, Berivan Laura Rebeca
    Bolchis, Vanessa
    Floare, Lucian
    Utu, Diana
    Jumanca, Daniela
    Galuscan, Atena
    JOURNAL OF FUNCTIONAL BIOMATERIALS, 2024, 15 (08)
  • [25] Surface roughness changes of two composite resin restorative materials after thermocycling
    Imtiaz, Taanya
    Ganesh, S. Balaji
    Jayalakshmi, S.
    JOURNAL OF ADVANCED PHARMACEUTICAL TECHNOLOGY & RESEARCH, 2022, 13 : S466 - S469
  • [26] Surface roughness changes of two composite resin restorative materials after thermocycling
    Imtiaz, Taanya
    Ganesh, S. Balaji
    Jayalakshmi, S.
    JOURNAL OF ADVANCED PHARMACEUTICAL TECHNOLOGY & RESEARCH, 2022, 13 (06) : 466 - 469
  • [27] Color stability and surface roughness of polished anterior restorative materials
    Yildiz, Esma
    Sirin Karaarslan, Emine
    Simsek, Mine
    Ozsevik, Abdul Semih
    Usumez, Aslihan
    DENTAL MATERIALS JOURNAL, 2015, 34 (05) : 629 - 639
  • [28] Studies on the Abrasive Wear Behaviour of the Direct Restorative Dental Materials
    Luca, Odette
    Vitalariu, Anca
    Cioloca, Catalina Holban
    Tatarciuc, Monica
    Popa, Diana Diaconu
    MATERIALE PLASTICE, 2019, 56 (03) : 625 - 628
  • [29] Translucency of esthetic dental restorative CAD/CAM materials and composite resins with respect to thickness and surface roughness
    Awad, Daniel
    Stawarczyk, Bogna
    Liebermann, Anja
    Ilie, Nicoleta
    JOURNAL OF PROSTHETIC DENTISTRY, 2015, 113 (06): : 534 - 540
  • [30] Effect of antacid gastric syrups on surface properties of dental restorative materials: an in vitro analysis of roughness and microhardness
    Ocal, Fikri
    Dayi, Burak
    BMC ORAL HEALTH, 2025, 25 (01):