Evaluation of Fracture Resistance of Occlusal Veneers Made of Different Types of Materials Depending on Their Thickness

被引:4
|
作者
Czechowski, Lukasz [1 ]
Dejak, Beata [1 ]
Konieczny, Bartlomiej [2 ]
Krasowski, Michal [2 ]
机构
[1] MU Lodz, Dept Prosthodont, PL-92213 Lodz, Poland
[2] Med Univ Lodz, Univ Lab Mat Res, PL-92213 Lodz, Poland
关键词
fracture resistance; occlusal veneers; dental ceramics; CAD/CAM COMPOSITE; ZIRCONIA; STRENGTH;
D O I
10.3390/ma16176006
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
Pathological tooth wear is an escalating social problem. Occlusal veneers can be an alternative to traditional prosthetic restorations such as crowns, inlays, and onlays. Background: The aim of this study is to assess the fracture resistance of occlusal veneers made of various materials depending on their thickness. Methods: In total, 120 occlusal veneers were examined. The restorations were made of four ceramics: leucite LC (IPS Empress Esthetic), hybrid HC (Vita Enamic), lithium disilicate LDC (IPS e.max Press), and zirconium oxide ZOC (Ceramill Zolid HT). A total of 30 veneers were made of each material, 10 for each of the three thicknesses: 1 mm, 1.5 mm, 2 mm. The restorations were cemented on identical abutments duplicated from the developed phantom tooth 35 (KaVo) with composite cement (All Bond Universal). The samples prepared in this way were subjected to a compressive strength test in a universal testing machine. Statistical analysis of the results was performed. Results: The average fracture resistance of occlusal veneers made of zirconium oxide ceramic was 1086-1640 N, of lithium disilicate ceramics 456-1044 N, of hybrid ceramics 449-576 N, and of leucite ceramics 257-499 N. Conclusions: Occlusal veneers made of ceramics, zirconium oxide and lithium disilicate, had the highest resistance to fractures. Restorations made of leucite ceramics turned out to be the least resistant to forces. The greater the thickness of the ceramic occlusal veneers, the greater their fracture resistance.
引用
收藏
页数:12
相关论文
共 50 条
  • [41] Ultra-thin occlusal veneers bonded to enamel and made of ceramic or hybrid materials exhibit load-bearing capacities not different from conventional restorations
    Ioannidis, Alexis
    Muhlemann, Sven
    Ozcan, Mutlu
    Husler, Jurg
    Hammerle, Christoph H. F.
    Benic, Goran I.
    JOURNAL OF THE MECHANICAL BEHAVIOR OF BIOMEDICAL MATERIALS, 2019, 90 : 433 - 440
  • [42] Evaluation of fracture strength for single crowns made of the different types of lithium disilicate glass–ceramics
    Chung-Ha Lim
    Yong-Seok Jang
    Min-Ho Lee
    Tae-Sung Bae
    Odontology, 2020, 108 : 231 - 239
  • [43] Influence of Ferrule Design and Occlusal Thickness on the Fracture Resistance and Failure Patterns of Zirconia Endocrowns
    Panda, Subhendu Kumar
    Patro, Tapan Kumar
    Dhal, Angurbala
    Garhnayak, Lokanath
    Kumar, Ullash
    Pattanaik, Nagen Ray
    JOURNAL OF PHARMACY AND BIOALLIED SCIENCES, 2024, 16 (SUPPL 4) : S3541 - S3543
  • [44] Resistance of CAD/CAM composite resin and ceramic occlusal veneers to fatigue and fracture in worn posterior teeth: A systematic review
    Maldonado, Karelys Del Cisne
    Espinoza, Juan Andres
    Astudillo, Daniela Andrea
    Delgado, Bolivar Andres
    Bravo, Wilson Daniel
    DENTAL AND MEDICAL PROBLEMS, 2024, 61 (03) : 417 - 426
  • [45] Influence of bonding surface and bonding methods on the fracture resistance and survival rate of full-coverage occlusal veneers made from lithium disilicate ceramic after cyclic loading
    Krummel, Anna
    Garling, Anne
    Sasse, Martin
    KernDepartment, Matthias
    DENTAL MATERIALS, 2019, 35 (10) : 1351 - 1359
  • [46] Evaluation of the fracture resistance of reattached incisal fragments using different materials and techniques
    Chazine, Michelle
    Sedda, Maurizio
    Ounsi, Hani F.
    Paragliola, Raffaele
    Ferrari, Marco
    Grandini, Simone
    DENTAL TRAUMATOLOGY, 2011, 27 (01) : 15 - 18
  • [47] Fracture resistance of CAD/CAM milled versus direct hand-made interim laminate veneers
    Abuhammoud, Salahaldeen
    Emtier, Banan
    Fu, Chin-Chuan
    Rojas-Rueda, Silvia
    Jurado, Carlos A.
    Afrashtehfar, Kelvin I.
    SAUDI DENTAL JOURNAL, 2024, 36 (06) : 920 - 925
  • [48] Evaluation of the mechanical properties of different materials for manufacturing occlusal splints
    Guimaraes, Danielly Mendonca
    Campaner, Marcio
    dos Santos, Rodrigo Wendel
    Pesqueira, Aldieris Alves
    de Medeiros, Rodrigo Antonio
    BRAZILIAN ORAL RESEARCH, 2023, 37
  • [49] Evaluation of fracture strength for single crowns made of the different types of lithium disilicate glass-ceramics
    Lim, Chung-Ha
    Jang, Yong-Seok
    Lee, Min-Ho
    Bae, Tae-Sung
    ODONTOLOGY, 2020, 108 (02) : 231 - 239
  • [50] Ceramic laminate veneers: effect of preparation design and ceramic thickness on fracture resistance and marginal quality in vitro
    Uwe Blunck
    Sabine Fischer
    Jan Hajtó
    Stefan Frei
    Roland Frankenberger
    Clinical Oral Investigations, 2020, 24 : 2745 - 2754