A study on the flow behavior and bubble evolution of circular oscillating laser welding of SUS301L-HT stainless steel

被引:6
|
作者
Zhao, Xu [1 ,2 ]
Chen, Jintao [2 ]
Lei, Zheng [2 ]
Zhang, Weihua [1 ]
Chen, Hui [2 ]
机构
[1] Southwest Jiaotong Univ, State Key Lab Tract Power, Chengdu 610031, Peoples R China
[2] Southwest Jiaotong Univ, Sch Mat Sci & Engn, Chengdu 610031, Peoples R China
关键词
Oscillating laser beam welding; Flow behavior; Formation of bubbles; Suppression mechanism; Flow mode transition; NUMERICAL-SIMULATION; KEYHOLE; DYNAMICS; POROSITY; BEAM; MICROSTRUCTURE; PREDICTION;
D O I
10.1016/j.ijheatmasstransfer.2022.123726
中图分类号
O414.1 [热力学];
学科分类号
摘要
The flow characteristics, bubble formation and inhibition mechanisms of circular oscillating laser beam welding (OLBW) at distinct stages were elucidated in present work. The formation processes of bubbles mainly included the following manners. First, one or more of vortex P2, the recoil pressure flow P3, the migration flows FMF and BMF impinged the keyhole wall. The necking generated, gradually destabilized, and finally collapsed. Second, the self-instability of needle-like keyhole bottom (NKB) with large curva-ture induced the bubble formation. Third, complex melt flow broke the abnormal deformation of the keyhole or the bubble wall to form a new bubble. The bubble suppression mechanisms were summa-rized to three categories. First, the recoil pressure on the inner wall of bubble was at a low level, and the volume of bubble continually decreased until it collapsed. Second, high recoil pressure penetrated the metal liquid bridge between keyhole and bubble. Third, when recoil pressure was greater than the resultant force between surface tension and melt dynamic pressure, the bubble constantly fluctuated and gradually merged with the moving keyhole. As the frequency increased from 10 Hz to 200 Hz, poros-ity showed an exponential decrease from 7.16% to 0.35% in circular oscillation mode. A unified porosity prediction curve based on the Reynolds number was built with a coefficient of determination of 0.989. When fluid changed from laminar to turbulent flow, the critical Reynolds number was set as 10 0 0, the predicted porosity was 0.912%, and the critical frequencies in circular and infinite oscillation modes were 143 Hz or 115 Hz, respectively, which were consistent with experiment results.(c) 2022 Elsevier Ltd. All rights reserved.
引用
收藏
页数:23
相关论文
共 50 条
  • [41] Laser butt welding of thin stainless steel 316L sheets in asymmetric configurations: A numerical study
    Ebrahimi, Amin
    Hermans, Marcel J. M.
    JOURNAL OF ADVANCED JOINING PROCESSES, 2023, 8
  • [42] Study of the viscoplastic deformation behavior of SUS316L stainless steel and effects of dynamic aging, cyclic loading and temperature
    Kaneko, K
    Oyamada, T
    Shimizu, D
    PROGRESS IN EXPERIMENTAL AND COMPUTATIONAL MECHANICS IN ENGINEERING, 2003, 243-2 : 439 - 444
  • [43] Effect of flow rate on corrosion behavior of 316L stainless steel welding seam in liquid lead bismuth eutectic
    Luo M.
    Lei Y.
    Chen G.
    Xiao L.
    Hanjie Xuebao/Transactions of the China Welding Institution, 2019, 40 (03): : 65 - 70
  • [44] A study of the behavior and effects of nitrogen take-up from protective gas shielding in laser welding of stainless steel
    Wu, S. K.
    Zheng, K.
    Zou, J. L.
    Jiang, F.
    Han, X. H.
    JOURNAL OF MANUFACTURING PROCESSES, 2018, 34 : 477 - 485
  • [45] Study on droplet transfer and weld quality in laser-MIG hybrid welding of 316L stainless steel
    Gao, Zhongmei
    Jiang, Ping
    Wang, Chunming
    Shao, Xinyu
    Pang, Shengyong
    Zhou, Qi
    Li, Xiongbin
    Wang, Yilin
    INTERNATIONAL JOURNAL OF ADVANCED MANUFACTURING TECHNOLOGY, 2017, 88 (1-4): : 483 - 493
  • [46] Study on droplet transfer and weld quality in laser-MIG hybrid welding of 316L stainless steel
    Zhongmei Gao
    Ping Jiang
    Chunming Wang
    Xinyu Shao
    Shengyong Pang
    Qi Zhou
    Xiongbin Li
    Yilin Wang
    The International Journal of Advanced Manufacturing Technology, 2017, 88 : 483 - 493
  • [47] Experimental study on the whole-life heterogeneous ratchetting and ratchetting-fatigue interaction of SUS301L stainless steel butt-welded joint
    Luo, Huiliang
    Kang, Guozheng
    Kan, Qianhua
    Ma, Chuanping
    FATIGUE & FRACTURE OF ENGINEERING MATERIALS & STRUCTURES, 2020, 43 (01) : 36 - 50
  • [48] SUBSTRUCTURE EVOLUTION AND FLOW BEHAVIOR OF AISI 316L STAINLESS-STEEL POLYCRYSTALS AT ROOM-TEMPERATURE
    JANECEK, M
    TANGRI, K
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 1991, 138 (02): : 237 - 245
  • [49] Numerical simulation of molten pool flow behavior and keyhole evolution behavior in dual-laser beam oscillating bilateral synchronous welding of T-joints
    Xia, Peiyun
    Wang, Chunming
    Mi, Gaoyang
    Zhang, Mingyang
    Xiong, Lingda
    Zhang, Xiong
    Zhai, Chuncheng
    Feng, Xiaosong
    Hu, Yiyang
    INTERNATIONAL JOURNAL OF HEAT AND MASS TRANSFER, 2023, 209
  • [50] Flow behavior and microstructural evolution during hot deformation of AISI Type 316 L(N) austenitic stainless steel
    Samantaray, Dipti
    Mandal, Sumantra
    Phaniraj, C.
    Bhaduri, A. K.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2011, 528 (29-30): : 8565 - 8572