A study on the flow behavior and bubble evolution of circular oscillating laser welding of SUS301L-HT stainless steel

被引:6
|
作者
Zhao, Xu [1 ,2 ]
Chen, Jintao [2 ]
Lei, Zheng [2 ]
Zhang, Weihua [1 ]
Chen, Hui [2 ]
机构
[1] Southwest Jiaotong Univ, State Key Lab Tract Power, Chengdu 610031, Peoples R China
[2] Southwest Jiaotong Univ, Sch Mat Sci & Engn, Chengdu 610031, Peoples R China
关键词
Oscillating laser beam welding; Flow behavior; Formation of bubbles; Suppression mechanism; Flow mode transition; NUMERICAL-SIMULATION; KEYHOLE; DYNAMICS; POROSITY; BEAM; MICROSTRUCTURE; PREDICTION;
D O I
10.1016/j.ijheatmasstransfer.2022.123726
中图分类号
O414.1 [热力学];
学科分类号
摘要
The flow characteristics, bubble formation and inhibition mechanisms of circular oscillating laser beam welding (OLBW) at distinct stages were elucidated in present work. The formation processes of bubbles mainly included the following manners. First, one or more of vortex P2, the recoil pressure flow P3, the migration flows FMF and BMF impinged the keyhole wall. The necking generated, gradually destabilized, and finally collapsed. Second, the self-instability of needle-like keyhole bottom (NKB) with large curva-ture induced the bubble formation. Third, complex melt flow broke the abnormal deformation of the keyhole or the bubble wall to form a new bubble. The bubble suppression mechanisms were summa-rized to three categories. First, the recoil pressure on the inner wall of bubble was at a low level, and the volume of bubble continually decreased until it collapsed. Second, high recoil pressure penetrated the metal liquid bridge between keyhole and bubble. Third, when recoil pressure was greater than the resultant force between surface tension and melt dynamic pressure, the bubble constantly fluctuated and gradually merged with the moving keyhole. As the frequency increased from 10 Hz to 200 Hz, poros-ity showed an exponential decrease from 7.16% to 0.35% in circular oscillation mode. A unified porosity prediction curve based on the Reynolds number was built with a coefficient of determination of 0.989. When fluid changed from laminar to turbulent flow, the critical Reynolds number was set as 10 0 0, the predicted porosity was 0.912%, and the critical frequencies in circular and infinite oscillation modes were 143 Hz or 115 Hz, respectively, which were consistent with experiment results.(c) 2022 Elsevier Ltd. All rights reserved.
引用
收藏
页数:23
相关论文
共 50 条
  • [31] Analysis of surface tension driven flow and solidification behavior in laser linear welding of stainless steel
    Li, Zhiyong
    Yu, Gang
    He, Xiuli
    Li, Shaoxia
    Tian, Chongxin
    Dong, Binxin
    OPTICS AND LASER TECHNOLOGY, 2020, 123
  • [32] Experimental study on multiaxial ratchetting-fatigue interaction of SUS301L stainless steel tubular welded joint
    Luo, Huiliang
    Qu, Kaicheng
    Yu, Chao
    Kan, Qianhua
    Kang, Guozheng
    INTERNATIONAL JOURNAL OF FATIGUE, 2024, 186
  • [33] Microstructural evolution in the welding zone of laser shock peened 316L stainless steel tube
    Lu, J. Z.
    Zhang, W. Q.
    Jing, X.
    Wu, L. J.
    Luo, K. Y.
    JOURNAL OF LASER APPLICATIONS, 2017, 29 (01)
  • [34] Experimental investigation and optimization of co-axial ring plus core dual beam laser welding parameters for SUS301 stainless steel sheet
    Liu, Zuguo
    Chen, Huiyang
    Jin, Xiangzhong
    MATERIALS AND MANUFACTURING PROCESSES, 2023, 38 (05) : 554 - 569
  • [35] A study on effect of laser overlay welding parameters of stainless steel 301 LN: tensile test, microstructure analysis and microhardness evaluation
    Farhadipour, Payam
    Dehghan, Shayan
    Barka, Noureddine
    Iltaf, Asim
    Farhadipour, Pedram
    WELDING INTERNATIONAL, 2024, 38 (06) : 409 - 421
  • [36] Two pass laser welding of TC4 Titanium alloy to 301L stainless steel via pure V interlayer
    Zhang, Yan
    Zhou, Jianping
    Sun, DaQian
    Li, HongMei
    JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2020, 9 (02): : 1400 - 1404
  • [37] Corrosion Behavior of a Laser-MIG Hybrid Welding-Brazing Joint of 6061 Aluminum Alloy to SUS304 Stainless Steel
    Liu, Ruilin
    Liu, Yunqi
    Lei, Zheng
    Tang, Hui
    He, Shaoxiong
    Li, Yuanxing
    Zhu, Zongtao
    CORROSION, 2021, 77 (12) : 1311 - 1320
  • [38] Research on Molten Pool Flow and Weld Formation of 304L Stainless Steel by Scanning Laser Overlap Welding
    Hui, Yang
    Fang, Li
    Hua Xueming
    Ke, Chen
    CHINESE JOURNAL OF LASERS-ZHONGGUO JIGUANG, 2022, 49 (22):
  • [39] Nd/YAG pulsed laser welding of TC4 titanium alloy to 301L stainless steel via pure copper interlayer
    Y Zhang
    D. Q Sun
    X. Y Gu
    Y. J Liu
    The International Journal of Advanced Manufacturing Technology, 2017, 90 : 953 - 961
  • [40] Nd/YAG pulsed laser welding of TC4 titanium alloy to 301L stainless steel via pure copper interlayer
    Zhang, Y.
    Sun, D. Q.
    Gu, X. Y.
    Liu, Y. J.
    INTERNATIONAL JOURNAL OF ADVANCED MANUFACTURING TECHNOLOGY, 2017, 90 (1-4): : 953 - 961