Improving creep-aging behavior and mechanical properties of AA7150 alloy via pre-aging

被引:4
|
作者
Zeng, Quanqing [1 ]
Feng, Sule [4 ]
Chen, Fei [1 ]
Wang, Dongyao [2 ]
Zhan, Lihua [1 ,2 ]
Yang, Youliang [1 ]
Tang, Lei [2 ,3 ]
Liu, Changzhi [5 ]
Yan, Dongyang [5 ]
机构
[1] Cent South Univ, Res Inst Light Alloy, Changsha 410083, Hunan, Peoples R China
[2] Cent South Univ, Coll Mech & Elect Engn, Changsha 410083, Hunan, Peoples R China
[3] Cent South Univ, Sch Mat Sci & Engn, Changsha 410083, Hunan, Peoples R China
[4] Shanghai Spaceflight Precis Machinery Inst, Shanghai, Peoples R China
[5] Beijing Inst Astronaut Syst Engn, Beijing 100076, Peoples R China
基金
中国国家自然科学基金;
关键词
AA7150; alloy; Pre; -aging; Creep; -ageing; Strength; Creep strain; 7075; ALUMINUM-ALLOY; DYNAMIC PRECIPITATION; AL; SPRINGBACK; MICROSTRUCTURES; OPTIMIZATION; SEGREGATION; TEMPERATURE; EVOLUTION; STRENGTH;
D O I
10.1016/j.msea.2024.146130
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Improving creep ageing behavior and mechanical properties of Al-Zn-Mg-Cu alloys via different pre-aging temperature, using the creep ageing test, room-temperature tensile test and transmission electron microscopy observation. A pre-aging temperature of 120 degrees C markedly improved the mechanical properties of the samples, including a tensile strength of 605.2 MPa, yield strength of 583.4 MPa, and elongation of 13.8 %. Pre-aging generated a "peak age region" during creep ageing, advantageous for extending the ageing time and enhancing creep strain without compromising strength. Detailed microstructure and mechanical performance characterizations were employed to discuss and unveil the strengthening mechanisms. The results additionally illustrated that pre-aging effectively reduces creep strain, as compared to the T4 sample, by minimizing vacancy concentration. Furthermore, pre-aging can manipulate lattice distortion and creep strain by facilitating atom diffusion, and a larger lattice with a pre-aging temperature of 100 degrees C results in higher creep strain. Moreover, elevating the pre-aging temperature (120 degrees C) reduces vacancy concentration, thereby inhibiting the phase transformation from eta ' to eta precipitates. This led to the attainment of a desirable microstructure consisting of eta ' precipitate with high density and dispersed distribution, significantly enhancing the strength of the alloy. Hence, a new method is provided for the manufacture of large-scale panel component with excellent mechanical properties.
引用
收藏
页数:15
相关论文
共 50 条
  • [41] Effects of natural aging after pre-aging on clustering and bake-hardening behavior in an Al-Mg-Si alloy
    Aruga, Yasuhiro
    Kozuka, Masaya
    Takaki, Yasuo
    Sato, Tatsuo
    SCRIPTA MATERIALIA, 2016, 116 : 82 - 86
  • [42] Effect of pre-aging treatment on hot compression behavior of AZ31 magnesium alloy
    Shang, L.
    Yue, S.
    Essadiqi, E.
    Javaid, A.
    Verma, R.
    MAGNESIUM TECHNOLOGY 2008, 2008, : 263 - +
  • [43] Effect of pre-aging on microstructure and properties of 2000 series aluminum alloy for automotive body sheets
    王孟君
    黄电源
    姜海涛
    任杰
    Transactions of Nonferrous Metals Society of China, 2007, (S1) : 262 - 265
  • [44] Effects of Pre-Stretching on Creep Behavior, Mechanical Property and Microstructure in Creep Aging of Al-Cu-Li Alloy
    Zhang, Jin
    Jiang, Zhen
    Xu, Fushun
    Chen, Mingan
    MATERIALS, 2019, 12 (03)
  • [45] Effect of pre-aging process on microstructure and properties of 7075-T8 aluminium alloy
    Zhang, Weijian
    Su, Ruiming
    Li, Guanglong
    Qu, Yingdong
    JOURNAL OF ALLOYS AND COMPOUNDS, 2023, 960
  • [46] Effect of pre-strain on creep aging behavior of 2524 aluminum alloy
    Xu, Yongqian
    Zhan, Lihua
    Li, Wenke
    JOURNAL OF ALLOYS AND COMPOUNDS, 2017, 691 : 564 - 571
  • [47] Anisotropy in creep-aging behavior of Al-Li alloy under different stress levels: experimental and constitutive modeling
    Peng, Nanhui
    Zhan, Lihua
    Xu, Yongqian
    Liu, Chunhui
    Ma, Bolin
    Chen, Kai
    Ren, Haobo
    JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2022, 20 : 3456 - 3470
  • [48] Preparation of nanoprecipitates and ultrafine grains for WE43 alloy to enhance mechanical properties by pre-aging treatment prior to extrusion
    Cheng, Tianqi
    Zeng, Ying
    Cui, Zhuang
    Fan, Lingling
    Li, Shupeng
    Miao, Junwei
    Xu, Shiwei
    Liu, Manping
    JOURNAL OF ALLOYS AND COMPOUNDS, 2025, 1013
  • [49] Effect of pre-aging treatment on microstructure and properties of an Al-Mg-Si-Cu alloy
    Ji, Yan-Li
    Guo, Fu-An
    Pan, Yan-Feng
    Zhong, Hao
    Cailiao Rechuli Xuebao/Transactions of Materials and Heat Treatment, 2010, 31 (02): : 85 - 89
  • [50] Effect of pre-aging on microstructure and properties of 2000 series aluminum alloy for automotive body sheets
    Meng-jun, Wang
    Dian-yuan, Huang
    Hai-tao, Jiang
    Jie, Ren
    TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2007, 17 : S262 - S265