Improving creep-aging behavior and mechanical properties of AA7150 alloy via pre-aging

被引:4
|
作者
Zeng, Quanqing [1 ]
Feng, Sule [4 ]
Chen, Fei [1 ]
Wang, Dongyao [2 ]
Zhan, Lihua [1 ,2 ]
Yang, Youliang [1 ]
Tang, Lei [2 ,3 ]
Liu, Changzhi [5 ]
Yan, Dongyang [5 ]
机构
[1] Cent South Univ, Res Inst Light Alloy, Changsha 410083, Hunan, Peoples R China
[2] Cent South Univ, Coll Mech & Elect Engn, Changsha 410083, Hunan, Peoples R China
[3] Cent South Univ, Sch Mat Sci & Engn, Changsha 410083, Hunan, Peoples R China
[4] Shanghai Spaceflight Precis Machinery Inst, Shanghai, Peoples R China
[5] Beijing Inst Astronaut Syst Engn, Beijing 100076, Peoples R China
基金
中国国家自然科学基金;
关键词
AA7150; alloy; Pre; -aging; Creep; -ageing; Strength; Creep strain; 7075; ALUMINUM-ALLOY; DYNAMIC PRECIPITATION; AL; SPRINGBACK; MICROSTRUCTURES; OPTIMIZATION; SEGREGATION; TEMPERATURE; EVOLUTION; STRENGTH;
D O I
10.1016/j.msea.2024.146130
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Improving creep ageing behavior and mechanical properties of Al-Zn-Mg-Cu alloys via different pre-aging temperature, using the creep ageing test, room-temperature tensile test and transmission electron microscopy observation. A pre-aging temperature of 120 degrees C markedly improved the mechanical properties of the samples, including a tensile strength of 605.2 MPa, yield strength of 583.4 MPa, and elongation of 13.8 %. Pre-aging generated a "peak age region" during creep ageing, advantageous for extending the ageing time and enhancing creep strain without compromising strength. Detailed microstructure and mechanical performance characterizations were employed to discuss and unveil the strengthening mechanisms. The results additionally illustrated that pre-aging effectively reduces creep strain, as compared to the T4 sample, by minimizing vacancy concentration. Furthermore, pre-aging can manipulate lattice distortion and creep strain by facilitating atom diffusion, and a larger lattice with a pre-aging temperature of 100 degrees C results in higher creep strain. Moreover, elevating the pre-aging temperature (120 degrees C) reduces vacancy concentration, thereby inhibiting the phase transformation from eta ' to eta precipitates. This led to the attainment of a desirable microstructure consisting of eta ' precipitate with high density and dispersed distribution, significantly enhancing the strength of the alloy. Hence, a new method is provided for the manufacture of large-scale panel component with excellent mechanical properties.
引用
收藏
页数:15
相关论文
共 50 条
  • [31] Pre-aging time dependence of microstructure and mechanical properties in nanostructured Al-2wt%Cu alloy
    Bahram Azad
    Ehsan Borhani
    Metals and Materials International, 2016, 22 : 243 - 251
  • [32] Effect of pre-aging temperature on the behavior in the early stage of aging at high temperature for Al-Mg-Si alloy
    Saga, M
    Sasaki, Y
    Kikuchi, M
    Yan, Z
    Matsuo, M
    ALUMINIUM ALLOYS: THEIR PHYSICAL AND MECHANICAL PROPERTIES, PTS 1-3, 1996, 217 : 821 - 826
  • [33] Effect of Cryorolling After Pre-aging on Tensile Properties and Microstructures of AA7075 Plates
    Yafei Wang
    Haitao Gao
    Jianrui Xing
    Zeng Tan
    Charlie Kong
    Hailiang Yu
    JOM, 2023, 75 : 4832 - 4844
  • [34] Effect of pre-aging on properties of 2000 series aluminum alloy for automotive body sheets
    School of Materials Science and Engineering, Central South University, Changsha 410083, China
    不详
    Zhongnan Daxue Xuebao (Ziran Kexue Ban), 2008, 4 (755-759):
  • [35] Effect of varied initial dislocation densities on the anisotropic behavior of creep-aging in Al-Cu-Li alloy
    Hui, Shengmeng
    Zhan, Lihua
    Xu, Yongqian
    Ma, Bolin
    Zhou, Chang
    Xie, Min
    Feng, Jingpeng
    Feng, Tong
    JOURNAL OF MATERIALS SCIENCE, 2024, 59 (27) : 12661 - 12676
  • [36] Influence of Extrusion Temperature on the Aging Behavior and Mechanical Properties of an AA6060 Aluminum Alloy
    Berndt, Nadja
    Frint, Philipp
    Wagner, Martin F. -X
    METALS, 2018, 8 (01):
  • [37] Combined Effects of Pre-deformation and Pre-aging on the Mechanical Properties of Al-Cu-Mg Alloy with Sc and Zr Addition
    Yuhang Guo
    Naiqin Zhao
    Chunsheng Shi
    Chunnian He
    Jiajun Li
    Enzuo Liu
    Journal of Wuhan University of Technology-Mater. Sci. Ed., 2018, 33 : 680 - 687
  • [38] Combined Effects of Pre-deformation and Pre-aging on the Mechanical Properties of Al-Cu-Mg Alloy with Sc and Zr Addition
    Guo Yuhang
    Zhao Naiqin
    Shi Chunsheng
    He Chunnian
    Li Jiajun
    Liu Enzuo
    JOURNAL OF WUHAN UNIVERSITY OF TECHNOLOGY-MATERIALS SCIENCE EDITION, 2018, 33 (03): : 680 - 687
  • [39] Effects of pre-aging and minor Sc addition on the microstructure and mechanical properties of friction stir processed 7055 Al alloy
    Liu, C. Y.
    Zhang, B.
    Ma, Z. Y.
    Teng, G. B.
    Wei, L. L.
    Zhou, W. B.
    Zhang, X. Y.
    VACUUM, 2018, 149 : 106 - 113
  • [40] Effects of the Pre-Aging Period on the Formation Behavior of Nanoclusters in an Al-Mg-Cu Alloy
    Mihara, Mami
    Kobayashi, Equo
    Sato, Tatsuo
    MATERIALS TRANSACTIONS, 2015, 56 (04) : 500 - 506