Formation of Inclusion in Ti–Al Killed Low C–Mn Steel

被引:0
|
作者
Cheng-wei YANG [1 ]
Xin-hua WANG [2 ]
Tie OU [3 ]
Jiang-hua QI [1 ]
Wan-jun ZHU [1 ]
Jun-fu CHEN [1 ]
Li-ping LIN [1 ]
机构
[1] Research and Development Center,Wuhan Iron and Steel (Group) Corp.
[2] School of Metallurgical and Ecological Engineering, University of Science and Technology Beijing
[3] Research and Development Center,Wuhan Iron and Steel (Group) Corp., Wuhan 430080, Hubei, China
关键词
Ti-killed steel; oxide metallurgy; inclusion;
D O I
暂无
中图分类号
TG142.71 [不锈钢、耐酸钢];
学科分类号
080502 ;
摘要
The formation of inclusion in Ti–Al complex deoxidized C–Mn steel was investigated. When Al content in steel is very low([Al]=0.0005%), for 0.003%<[Ti]<0.007%, the inclusion is the Al2O3–SiO2–MnO–TiOx composite inclusion; for [Ti]≥0.009%, the inclusion is TiOx in the steel. When [Ti]=0.005%, [Al]<0.001%, the inclusion is the Al2O3–SiO2–MnO–TiOx composite inclusion; while [Al]>0.006%, inclusions would be pure Al2O3. The experimental results agree with the thermodynamics conclusions.
引用
收藏
页码:87 / 90
页数:4
相关论文
共 50 条
  • [11] Thermodynamics of Complex Sulfide Inclusion Formation in Ca-Treated Al-Killed Structural Steel
    Yin-tao Guo
    Sheng-ping He
    Gu-jun Chen
    Qian Wang
    Metallurgical and Materials Transactions B, 2016, 47 : 2549 - 2557
  • [12] Thermodynamics of Complex Sulfide Inclusion Formation in Ca-Treated Al-Killed Structural Steel
    Guo, Yin-tao
    He, Sheng-ping
    Chen, Gu-jun
    Wang, Qian
    METALLURGICAL AND MATERIALS TRANSACTIONS B-PROCESS METALLURGY AND MATERIALS PROCESSING SCIENCE, 2016, 47 (04): : 2549 - 2557
  • [13] Inclusion Population Evolution in Ti-alloyed Al-killed Steel during Secondary Steelmaking Process
    Zinngrebe, Enno
    Van Hoek, Corrie
    Visser, Henk
    Westendorp, Albert
    Jung, In-Ho
    ISIJ INTERNATIONAL, 2012, 52 (01) : 52 - 61
  • [14] EFFECTS OF MN CONTENT AND COILING CONDITION OF HOT STRIP ON THE RECRYSTALLIZATION TEXTURE OF LOW C AL-KILLED STEEL SHEETS
    MIZUI, N
    TETSU TO HAGANE-JOURNAL OF THE IRON AND STEEL INSTITUTE OF JAPAN, 1985, 71 : 1358 - 1358
  • [15] Inclusion Characteristics and Acicular Ferrite Formation in the Simulated Heat-Affected Zone of Ti-Zr-Killed Low-Carbon Steel
    Liu, Fangce
    Bi, Yue
    Wang, Chao
    Kang, Jian
    He, Tong
    Liu, Yandong
    Yuan, Guo
    METALS AND MATERIALS INTERNATIONAL, 2023, 29 (03) : 715 - 729
  • [16] Inclusion Characteristics and Acicular Ferrite Formation in the Simulated Heat-Affected Zone of Ti-Zr-Killed Low-Carbon Steel
    Fangce Liu
    Yue Bi
    Chao Wang
    Jian Kang
    Tong He
    Yandong Liu
    Guo Yuan
    Metals and Materials International, 2023, 29 : 715 - 729
  • [17] Nucleation Behavior Analysis of Intragranular Acicular Ferrite in a Ti-killed C-Mn Steel
    Feng Chai
    Hang Su
    Cai-fu Yang
    Dong-mei Xue
    Journal of Iron and Steel Research International, 2014, 21 : 369 - 374
  • [18] Nucleation Behavior Analysis of Intragranular Acicular Ferrite in a Ti-killed C-Mn Steel
    Feng CHAI
    Hang SU
    Cai-fu YANG
    Dong-mei XUE
    Journal of Iron and Steel Research(International), 2014, 21 (03) : 369 - 374
  • [19] Nucleation Behavior Analysis of Intragranular Acicular Ferrite in a Ti-killed C-Mn Steel
    Chai, Feng
    Su, Hang
    Yang, Cai-fu
    Xue, Dong-mei
    JOURNAL OF IRON AND STEEL RESEARCH INTERNATIONAL, 2014, 21 (03) : 369 - 374
  • [20] Inclusion Evolution after Calcium Addition in Low Carbon Al-Killed Steel with Ultra Low Sulfur Content
    Yang, Guangwei
    Wang, Xinhua
    ISIJ INTERNATIONAL, 2015, 55 (01) : 126 - 133