Oxidation behavior of a Ni-Cr-Fe superalloy from 800 °C to 1100 °C in air: Formation and mechanism of multilayer oxide films

被引:0
|
作者
Zhao, Zhiwei [1 ,2 ]
Wang, Songlin [1 ]
Lu, Yanling [1 ,3 ]
Li, Jiuxiao [2 ]
Li, Xin [1 ,3 ]
机构
[1] Chinese Acad Sci, Shanghai Inst Appl Phys, Shanghai 201800, Peoples R China
[2] Shanghai Univ Engn Sci, Sch Mat Sci & Engn, Shanghai 201620, Peoples R China
[3] Univ Chinese Acad Sci, Beijing 100049, Peoples R China
基金
中国国家自然科学基金;
关键词
K4169; superalloy; Oxidation behavior; Oxide scales; Diffusion; Mechanisms; HIGH-TEMPERATURE OXIDATION; NICKEL-BASED SUPERALLOY; CYCLIC OXIDATION; MICROSTRUCTURE; ALLOY; KINETICS; GROWTH; SCALE; RANGE;
D O I
10.1016/j.jallcom.2025.179393
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
The oxidation behavior of a K4169 superalloy was investigated over a temperature range of 800 degrees C to 1100 degrees C in air for 100 hours. The formation of oxide film was analyzed using multiscale characterization techniques. The results show that the oxidation kinetics followed the parabolic law, with an oxidation activation energy of 234.59 f 3.72 kJ.mol-1. At 800 degrees C and 900 degrees C, a double oxide layer formed, comprising an outer layer of Cr2O3 with minor TiO2 and NiCr2O4 mixed oxides, and an inner layer of Al2O3. At temperatures above 1000 degrees C, the structure of the outer and inner layers remained unchanged, and a new intermediate layer appeared, primarily consisting of an Nb-rich layer and TiO2. The formation of the multilayer oxide structure was attributed to the competing mechanisms of external diffusion of alloying elements through the matrix and internal diffusion of oxygen. With prolonged oxidation, the continuous diffusion of Ti destroyed the continuous and protective Cr2O3 layer, while Al absorbed incoming oxygen, forming fibrous A12O3 that hindered further oxygen diffusion into the alloy matrix. The impact of oxidation time on oxide scale formation was similar to that of temperature, both leading to a thicker oxidation layer and the degradation of protective layers.
引用
收藏
页数:16
相关论文
共 50 条
  • [31] Isothermal Oxidation Behaviors of Packed Aluminide Coatings of Ni-Cr-W Superalloy at 1100°C
    Wang Jian
    Zhang Pingxiang
    Hu Rui
    Li Jinshan
    Ma Jian
    RARE METAL MATERIALS AND ENGINEERING, 2015, 44 (05) : 1169 - 1172
  • [32] Isothermal Oxidation Behavior Characteristics of a Second Generation Ni-base Single Crystal Superalloy in Air at 1000 and 1100°C
    Latief, Fahamsyah H.
    Kakehi, Koji
    Fu, Xintao
    Tashiro, Yuma
    INTERNATIONAL JOURNAL OF ELECTROCHEMICAL SCIENCE, 2012, 7 (09): : 8369 - 8383
  • [33] High-temperature oxidation behavior and mechanism of a new type of wrought Ni-Fe-Cr-Al superalloy up to 1300°C
    Huang, JF
    Fang, HS
    Fu, XR
    Huang, FX
    Wan, H
    Zhang, QF
    Deng, SP
    Zu, JS
    OXIDATION OF METALS, 2000, 53 (3-4): : 273 - 287
  • [34] High-temperature oxidation behavior and mechanism of a new type of wrought Ni-Fe-Cr-Al superalloy up to 1300 °C
    Huang, Jinfeng
    Fang, Hongsheng
    Fu, Xiaorong
    Huang, Fuxiang
    Wan, Hong
    Zhang, Qianfa
    Deng, Shiping
    Zu, Jishseng
    Oxidation of Metals, 2000, 53 (03): : 273 - 287
  • [35] The Formation Mechanism of a Multilayer-Structure Oxide Film during the Oxidation of FeCrAl in Air at 700 ?C
    Gao, Zichen
    Wang, Xinyu
    Zhou, Danna
    Wu, Qingsheng
    Li, Chunjing
    Song, Liangliang
    Liu, Shaojun
    METALS, 2023, 13 (02)
  • [36] Oxidation behavior of high Hf nickel-based superalloy in air at 900, 1000 and 1100°C
    Xiao, Jiu-han
    Xiong, Ying
    Wang, Li
    Jiang, Xiang-wei
    Wang, Dong
    Li, Kai-wen
    Dong, Jia-sheng
    Lou, Lang-hong
    INTERNATIONAL JOURNAL OF MINERALS METALLURGY AND MATERIALS, 2021, 28 (12) : 1957 - 1965
  • [37] Oxidation behavior of high Hf nickel-based superalloy in air at 900, 1000 and 1100°C
    Jiu-han Xiao
    Ying Xiong
    Li Wang
    Xiang-wei Jiang
    Dong Wang
    Kai-wen Li
    Jia-sheng Dong
    Lang-hong Lou
    International Journal of Minerals, Metallurgy and Materials, 2021, 28 : 1957 - 1965
  • [38] Oxidation behavior of the single-crystal Ni-base superalloy DD32 in air at 900, 1000, and 1100°C
    Huang, L.
    Sun, X. F.
    Guan, H. R.
    Hu, Z. Q.
    OXIDATION OF METALS, 2006, 65 (5-6): : 391 - 408
  • [39] Oxidation Behavior of the Single-Crystal Ni-base Superalloy DD32 in Air at 900, 1000, and 1100°C
    L. Huang
    X. F. Sun
    H. R. Guan
    Z. Q. Hu
    Oxidation of Metals, 2006, 65 : 391 - 408
  • [40] Oxidation behavior characteristics of an aluminized Ni-based single crystal superalloy CM186LC between 900 °C and 1100 °C in air
    Latief, Fahamsyah H.
    Kakehi, Koji
    Tashiro, Yuma
    JOURNAL OF INDUSTRIAL AND ENGINEERING CHEMISTRY, 2013, 19 (06) : 1926 - 1932