Effect of Solution Parameters on Microstructure and Magnetic Properties of Sm2Co17 Magnet

被引:0
|
作者
Jia, Shulin [1 ]
Shi, Huigang [1 ]
Xiang, Junyou [2 ]
机构
[1] School of Physics Science and Technology, Lanzhou University, Gansu, Lanzhou,730000, China
[2] Division of the Permanent magnet materials, Hangzhou Kede Magnetic Components Co., Ltd, Hangzhou,310000, China
关键词
Cobalt alloys - Magnetic after effect - Magnetic domains - Permanent magnets - Powder metallurgy - Samarium alloys - Samarium compounds;
D O I
10.11785/S1000-4343.20250108
中图分类号
学科分类号
摘要
Sm2Co17 magnet samples with different solution temperature and solution time were prepared by powder metallurgy method. The effects of solution temperature and solution time on the microstructure and macroscopic magnetic properties of magnet were studied. The results show that the 2:17H phase and 1:7H phase are mutually transformed under different solution temperature and time. With the solution temperature increases and the solution time prolongates, the grain size of the magnet increases gradually. At the same solution temperature, the width of the magnetic domains treated with 9 h solution is smaller than that of the magnets treated with 6 h solution, and the uniformity of the domains is obviously improved. The magnetic energy of the magnet sample after 9 h solution treatment is(BH)max=32.11 MGOe, Hcj=26.56 kOe, Br=11.45 kGs, Sq=73.1 %. © 2025 Editorial Office of Chinese Rare Earths. All rights reserved.
引用
收藏
页码:87 / 95
相关论文
共 50 条
  • [31] Magnetic properties and microstructure of Sm2Co17-based high temperature permanent magnet
    Yi, Jianhong
    Li, Liya
    Peng, Yuandong
    PROGRESS IN POWDER METALLURGY, PTS 1 AND 2, 2007, 534-536 : 1341 - +
  • [32] Studies on structural transformation and magnetic properties in Sm2Co17 type alloys
    Gopalan, R
    Muraleedharan, K
    Sastry, TSRK
    Singh, AK
    Joshi, V
    Rao, DVS
    Chandrasekaran, V
    JOURNAL OF MATERIALS SCIENCE, 2001, 36 (17) : 4117 - 4123
  • [33] Studies on structural transformation and magnetic properties in Sm2Co17 type alloys
    R. Gopalan
    K. Muraleedharan
    T. S. R. K. Sastry
    A. K. Singh
    V. Joshi
    D. V. Sridhara Rao
    V. Chandrasekaran
    Journal of Materials Science, 2001, 36 : 4117 - 4123
  • [34] Influence of Mn substitution on the structure and magnetic properties of Sm2Co17 compounds
    Sun, ZG
    Zhang, SY
    Zhang, HW
    Shen, BG
    JOURNAL OF PHYSICS-CONDENSED MATTER, 2001, 13 (09) : 2001 - 2008
  • [35] Atomic structure and the magnetic properties of Zr-doped Sm2Co17
    Ravel, B.
    Gallagher, K.
    PHYSICA SCRIPTA, 2005, T115 : 606 - 608
  • [36] Grain size dependent magnetic properties of nanocrystalline Sm2Co17/Cu
    Bessais, L
    Djéga-Mariadassou, C
    Zhang, J
    Lalanne, V
    Percheron-Guégan, A
    NANOPHASE AND NANOCOMPOSITE MATERIALS IV, 2002, 703 : 135 - 140
  • [37] Microstructure and Intrinsic Coercive Force of Sm2Co17 Type Permanent Magnet Alloys by Aging Treatment
    Lai Weiming
    Shen Anguo
    Cheng Lingli
    Bao Shengxiang
    Zhang Ming
    Xiang Hai-Rong
    RARE METAL MATERIALS AND ENGINEERING, 2013, 42 (05) : 971 - 974
  • [39] HYPERFINE INTERACTIONS OF SM AND CO IN SM2CO17
    POTENZIANI, E
    PAUL, DI
    TAUBER, A
    PHYSICAL REVIEW B, 1982, 25 (01): : 47 - 52
  • [40] Phase transformation in nanocrystalline Sm2Co17 permanent magnet material
    Song, Xiaoyan
    Lu, Nianduan
    Xu, Wenwu
    Zhang, Zhexu
    Zhang, Jiuxing
    JOURNAL OF APPLIED CRYSTALLOGRAPHY, 2009, 42 : 691 - 696