Effect of Solution Parameters on Microstructure and Magnetic Properties of Sm2Co17 Magnet

被引:0
|
作者
Jia, Shulin [1 ]
Shi, Huigang [1 ]
Xiang, Junyou [2 ]
机构
[1] School of Physics Science and Technology, Lanzhou University, Gansu, Lanzhou,730000, China
[2] Division of the Permanent magnet materials, Hangzhou Kede Magnetic Components Co., Ltd, Hangzhou,310000, China
关键词
Cobalt alloys - Magnetic after effect - Magnetic domains - Permanent magnets - Powder metallurgy - Samarium alloys - Samarium compounds;
D O I
10.11785/S1000-4343.20250108
中图分类号
学科分类号
摘要
Sm2Co17 magnet samples with different solution temperature and solution time were prepared by powder metallurgy method. The effects of solution temperature and solution time on the microstructure and macroscopic magnetic properties of magnet were studied. The results show that the 2:17H phase and 1:7H phase are mutually transformed under different solution temperature and time. With the solution temperature increases and the solution time prolongates, the grain size of the magnet increases gradually. At the same solution temperature, the width of the magnetic domains treated with 9 h solution is smaller than that of the magnets treated with 6 h solution, and the uniformity of the domains is obviously improved. The magnetic energy of the magnet sample after 9 h solution treatment is(BH)max=32.11 MGOe, Hcj=26.56 kOe, Br=11.45 kGs, Sq=73.1 %. © 2025 Editorial Office of Chinese Rare Earths. All rights reserved.
引用
收藏
页码:87 / 95
相关论文
共 50 条
  • [22] Robust ferromagnetism in the compressed permanent magnet Sm2Co17
    Jeffries, J. R.
    Veiga, L. S. I.
    Fabbris, G.
    Haskel, D.
    Huang, P.
    Butch, N. P.
    McCall, S. K.
    Holliday, K.
    Jenei, Z.
    Xiao, Y.
    Chow, P.
    PHYSICAL REVIEW B, 2014, 90 (10):
  • [23] Coercive Sm2Co17 powder for the bonded magnet application
    Liu, W.L.
    Liang, Y.L.
    Scott, D.W.
    Ma, B.M.
    Bounds, C.O.
    IEEE Transactions on Magnetics, 1995, 31 (6 pt 2): : 3686 - 3688
  • [24] COERCIVE SM2CO17 POWDER FOR THE BONDED MAGNET APPLICATION
    LIU, WL
    LIANG, YL
    SCOTT, DW
    MA, BM
    BOUNDS, CO
    IEEE TRANSACTIONS ON MAGNETICS, 1995, 31 (06) : 3686 - 3688
  • [25] Preparation and magnetic properties of amorphous and nanocrystalline Sm2Co17 alloys
    Lu, Nianduan
    Song, Xiaoyan
    Liu, Xuemei
    Zhang, Jiuxing
    INTERMETALLICS, 2010, 18 (06) : 1180 - 1184
  • [26] Structural transformations and magnetic properties of alloys of type Sm2Co17
    Rastegaev, VS
    Gudim, ZY
    Kutepov, AV
    RUSSIAN METALLURGY, 1998, (02): : 115 - 118
  • [27] Influence of Ti substitution on the structure and magnetic properties of Sm2Co17
    Wang, WQ
    Yan, Y
    Jin, HM
    PHYSICA B-CONDENSED MATTER, 2003, 328 (3-4) : 372 - 376
  • [28] Microstructure of Sm2Co17 magnets and its influence on coercivity
    李丽娅
    易健宏
    黄伯云
    彭元东
    杜娟
    Transactions of Nonferrous Metals Society of China, 2004, (04) : 790 - 793
  • [29] Sm2Co17 Microstructure Changes During Disproportionation in Hydrogen
    Bulyk, I. I.
    Burkhovetskyi, V. V.
    Tarenkov, V. Yu.
    Lyutyy, P. Ya.
    METALLOFIZIKA I NOVEISHIE TEKHNOLOGII, 2013, 35 (10): : 1437 - 1449
  • [30] Microstructure of Sm2Co17 magnets and its influence on coercivity
    Li, LY
    Yi, JH
    Huang, BY
    Peng, YD
    Du, J
    TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2004, 14 (04) : 790 - 793