Effect of Solution Parameters on Microstructure and Magnetic Properties of Sm2Co17 Magnet

被引:0
|
作者
Jia, Shulin [1 ]
Shi, Huigang [1 ]
Xiang, Junyou [2 ]
机构
[1] School of Physics Science and Technology, Lanzhou University, Gansu, Lanzhou,730000, China
[2] Division of the Permanent magnet materials, Hangzhou Kede Magnetic Components Co., Ltd, Hangzhou,310000, China
关键词
Cobalt alloys - Magnetic after effect - Magnetic domains - Permanent magnets - Powder metallurgy - Samarium alloys - Samarium compounds;
D O I
10.11785/S1000-4343.20250108
中图分类号
学科分类号
摘要
Sm2Co17 magnet samples with different solution temperature and solution time were prepared by powder metallurgy method. The effects of solution temperature and solution time on the microstructure and macroscopic magnetic properties of magnet were studied. The results show that the 2:17H phase and 1:7H phase are mutually transformed under different solution temperature and time. With the solution temperature increases and the solution time prolongates, the grain size of the magnet increases gradually. At the same solution temperature, the width of the magnetic domains treated with 9 h solution is smaller than that of the magnets treated with 6 h solution, and the uniformity of the domains is obviously improved. The magnetic energy of the magnet sample after 9 h solution treatment is(BH)max=32.11 MGOe, Hcj=26.56 kOe, Br=11.45 kGs, Sq=73.1 %. © 2025 Editorial Office of Chinese Rare Earths. All rights reserved.
引用
收藏
页码:87 / 95
相关论文
共 50 条
  • [1] Interface microstructure and magnetic properties of α-Sm2Co17/β-Sm2Co17 dual phase nanowire magnetic composite
    Cui, Chunxiang
    Yang, Wei
    Ding, Jinhua
    Cui, Sen
    INTERMETALLICS, 2019, 111
  • [2] The effect of microstructure on magnetic properties of TLP bonded Sm2Co17 hard magnets
    Mostaan, Hossein
    Rafiei, Mandi
    Oraei, Mohammad Mandi
    Baharzadeh, Ehsan
    APPLIED PHYSICS A-MATERIALS SCIENCE & PROCESSING, 2020, 126 (06):
  • [3] Effect of Cr underlayer on microstructure and magnetic properties of Sm2Co17 thin films
    Chen, SK
    Wu, GY
    Tsai, JL
    Chin, TS
    IEEE TRANSACTIONS ON MAGNETICS, 2001, 37 (04) : 2593 - 2595
  • [4] The effect of microstructure on magnetic properties of TLP bonded Sm2Co17 hard magnets
    Hossein Mostaan
    Mahdi Rafiei
    Mohammad Mahdi Oraei
    Ehsan Baharzadeh
    Applied Physics A, 2020, 126
  • [5] Preparation, Magnetic Properties and Microstructure of MnBi/Sm2Co17 Composite Magnetic Powder
    Shan Jiefeng
    Yu Nengjun
    Zhang Suyin
    Jin Xiangyang
    Wu Qiong
    Zhang Pengyue
    Ge Hongliang
    RARE METAL MATERIALS AND ENGINEERING, 2021, 50 (04) : 1448 - 1454
  • [6] EFFECT OF SUBSTITUTION OF NICKEL ON MAGNETIC-PROPERTIES OF SM2CO17
    MERCHES, M
    SANKAR, SG
    WALLACE, WE
    JOURNAL OF APPLIED PHYSICS, 1978, 49 (03) : 2055 - 2057
  • [7] Metallographic microstructure and magnetic properties of Sm2Co17 rare earth permanent magnet material by a strip casting technique
    Shen, Anguo
    Wang, Jingdong
    Zhang, Ming
    Tan, Fuming
    Li, Bian
    Xu, Liang
    Yuan, Tao
    Xiyou Jinshu Cailiao Yu Gongcheng/Rare Metal Materials and Engineering, 2013, 42 (04): : 865 - 867
  • [8] Metallographic Microstructure and Magnetic Properties of Sm2Co17 Rare Earth Permanent Magnet Material by a Strip Casting Technique
    Shen Anguo
    Wang Jingdong
    Zhang Ming
    Tan Fuming
    Li Bian
    Xu Liang
    Yuan Tao
    RARE METAL MATERIALS AND ENGINEERING, 2013, 42 (04) : 865 - 867
  • [9] Effects of oxygen and carbon on the magnetic properties and microstructure Of Sm2Co17 permanent magnets
    Tian Jianjun
    Zhang Shengen
    Qu Xuanhui
    RARE METALS, 2007, 26 (04) : 299 - 304
  • [10] Investigation on microstructure and magnetic properties of Sm2Co17 magnets aged at high temperature
    Feng, Haibo
    Chen, Hongsheng
    Guo, Zhaohui
    Pan, Wei
    Zhu, Minggang
    Li, Wei
    JOURNAL OF APPLIED PHYSICS, 2011, 109 (07)