Newly developed electrochemical evaluation method of temper embrittlement of Cr-Mo-V steel and 2.25 Cr-1 Mo steel

被引:0
|
作者
Watanabe, Yutaka
Shoji, Tetsuo
机构
关键词
Electrochemistry - Steel - Heat Resisting - Steel Heat Treatment;
D O I
暂无
中图分类号
学科分类号
摘要
A nondestructive electrochemical method is developed for detection and evaluation of temper embrittlement of Cr-Mo-V Steel and 2.25 Cr-1 Mo steel. In this method, temper embrittlement can be detected and evaluated by the second peak of current density 'IP2' which appears in the anodic polarization curves measured in a calcium nitrate solution. In contrast to nonembrittled materials (couplings and de-embrittling heat-treated materials) which exhibited the dull and low second peak, the sharp and high second peak current appeared in the anodic polarization curves measured on embrittled materials. This increase in IP2 is caused by selective dissolution of embrittled (impurity-enriched) grain boundaries and that increase in IP2 has a good correlation with the shifts in FATT. Temper embrittlement can be nondestructively evaluated by IP2 measurements with high accuracy.
引用
收藏
页码:1233 / 1239
相关论文
共 50 条
  • [41] Tempering embrittlement of 2.25Cr-1Mo steel for, a long term of service
    Hua, L
    Xu, H
    Wang, ZW
    Wang, ZD
    ENVIRONMENT EFFECTS ON FRACTURE AND DAMAGE, 2004, : 105 - 109
  • [42] INFLUENCE OF MICROSTRUCTURE ON HYDROGEN EMBRITTLEMENT BEHAVIOR OF 2.25CR-1MO STEEL
    VALENTINI, R
    SOLINA, A
    MATERIALS SCIENCE AND TECHNOLOGY, 1994, 10 (10) : 908 - 914
  • [43] EFFECT OF HEAT-TREATMENT ON TEMPER EMBRITTLEMENT SUSCEPTIBILITY OF CR-MO-V STEELS
    VISWANATHAN, R
    SHAW, BJ
    SCRIPTA METALLURGICA, 1974, 8 (11): : 1255 - 1260
  • [44] SUBMERGED-ARC STRIP OVERLAY WELDING OF 2.25 CR-1 MO STEEL
    CHANDEL, RS
    HOARE, R
    CIM BULLETIN, 1983, 76 (854): : 60 - 60
  • [45] Studies on hydrogen permeability of 2.25% Cr-1% Mo ferritic steel: correlation with microstructure
    Parvathavarthini, N
    Saroja, S
    Dayal, RK
    Khatak, HS
    JOURNAL OF NUCLEAR MATERIALS, 2001, 288 (2-3) : 187 - 196
  • [46] SUBSTRUCTURE AND STRENGTHENING MECHANISMS IN 2.25 CR-1 MO STEEL AT ELEVATED-TEMPERATURES
    JONES, WB
    VANDEAVYLE, JA
    METALLURGICAL TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1980, 11 (08): : 1275 - 1286
  • [47] EFFECT OF THERMAL CYCLING ON THE ALLOY 800 2.25 CR-1 MO STEEL JOINT
    BHADURI, AK
    VENKADESAN, S
    ZEITSCHRIFT FUR METALLKUNDE, 1991, 82 (02): : 135 - 138
  • [48] CRITICAL LITERATURE REVIEW OF EMBRITTLEMENT IN 2 1/4 CR-1 MO STEEL
    EMMER, LG
    CLAUSER, CD
    LOW, JR
    WELDING RESEARCH COUNCIL BULLETIN, 1973, (183): : 1 - 25
  • [49] EFFECT OF OXIDATION ON HOLD TIME FATIGUE BEHAVIOR OF 2.25 CR-1 MO STEEL
    TERANISHI, H
    MCEVILY, AJ
    METALLURGICAL TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1979, 10 (11): : 1806 - 1808
  • [50] Misorientation development in grains of tensile strained and crept 2.25%Cr-1%Mo steel
    Fukuoka, C
    Morishima, K
    Yoshizawa, H
    Mino, K
    SCRIPTA MATERIALIA, 2002, 46 (01) : 61 - 66