The tests for determining fracture data which are described in literature often deal with the methods of linear-elastic fracture mechanics (LEFM). The critical stress intensity factor K//I//C can only be determined with unusually large material thicknesses and, in addition to that, is strongly dependent on temperature and time. Therefore, great problems are involved in transferring the LEFM-data to thin-wall moldings. In recent years, the Institut fuer Kunststoffverarbeitung (IKV) have determined material characteristics in special tensile impact tests. These data - the minimum fracture strain and the minimum volume-specific work to fracture - represent real minima, which are not exceeded even in cases of fastest loading and lowest temperatures.
引用
收藏
页码:110 / 114
相关论文
共 50 条
  • [41] Comparative study on the wear behavior of long and short glass fiber reinforced plastics
    Srinivasan, V.
    Karthikeyan, R.
    Ganesan, G.
    Asaithambi, B.
    METALS AND MATERIALS INTERNATIONAL, 2010, 16 (02) : 205 - 212
  • [42] Fatigue life prediction of injection moulded short glass fiber reinforced plastics
    Kanters, Marc J. W.
    Douven, Lucien F. A.
    Savoyat, Pierre
    FATIGUE DESIGN 2019, INTERNATIONAL CONFERENCE ON FATIGUE DESIGN, 8TH EDITION, 2019, 19 : 698 - 710
  • [43] THE STRENGTH OF THE FIBER POLYMER INTERFACE IN SHORT GLASS FIBER-REINFORCED POLYPROPYLENE
    MITTAL, RK
    GUPTA, VB
    JOURNAL OF MATERIALS SCIENCE, 1982, 17 (11) : 3179 - 3188
  • [44] Glass fiber-reinforced plastics in scrubbers
    Lux, R
    CORROSIVE DAMAGE IN POWER PLANTS, 1997, 1333 : 55 - 67
  • [45] WETTING AND ADHESION IN GLASS FIBER REINFORCED PLASTICS
    JARVIS, NL
    ZISMAN, WA
    BULLETIN DE LA SOCIETE CHIMIQUE DE FRANCE, 1970, : 3202 - &
  • [46] MOISTURE VS GLASS FIBER REINFORCED PLASTICS
    KING, HA
    MATERIALS PROTECTION, 1967, 6 (09): : 20 - &
  • [47] Creep tests of glass fiber reinforced plastics
    Li, L. H.
    Chen, L.
    Wang, Z.
    GEOSYNTHETICS IN CIVIL AND ENVIRONMENTAL ENGINEERING, 2008, : 128 - +
  • [48] AUTOMOTIVE GLASS-FIBER REINFORCED PLASTICS
    ORTEGA, AJ
    SPE JOURNAL, 1969, 25 (08): : 76 - &
  • [49] Calculation method of the flexural tensile strength of the glass fiber-reinforced polymer stirrup based on the database
    Bai H.
    Xue W.
    Jiang J.
    Harbin Gongcheng Daxue Xuebao/Journal of Harbin Engineering University, 45 (02): : 223 - 229
  • [50] INSTANTANEOUS EFFECT OF INTERNAL MOISTURE CONDITIONS ON STRENGTH OF GLASS-FIBER-REINFORCED PLASTICS
    ISHAI, O
    ARNON, U
    JOURNAL OF TESTING AND EVALUATION, 1978, 6 (06) : 364 - 368