Reduction and oxidation kinetics of nickel-based oxygen-carriers for chemical-looping combustion and chemical-looping reforming

被引:0
|
作者
机构
[1] Dueso, Cristina
[2] Ortiz, María
[3] Abad, Alberto
[4] García-Labiano, Francisco
[5] De Diego, Luis F.
[6] Gayán, Pilar
[7] Adánez, Juan
来源
Adánez, J. (jadanez@icb.csic.es) | 1600年 / Elsevier B.V.卷 / 188期
关键词
The kinetics of reduction with CH4; H2 and CO and oxidation with O2 of two NiO-based oxygen-carriers for chemical-looping combustion (CLC) and chemical-looping reforming (CLR) prepared by impregnation; NiO18-αAl and NiO21-γAl; have been determined in this work. In both solids; nickel was present as NiO and NiAl2O4 in the oxidized state and the NiO/NiAl2O4 ratio in the particles was a function of the solid conversion reached in the previous reduction process. Both nickel compounds were active for oxygen transfer although with very different reactivities. Therefore; kinetic parameters for NiO and NiAl2O4 reduction were determined for each oxygen carrier and each reacting gas. The reaction rate of NiO reduction was the same in NiO18-αAl and NiO21-γAl particles. A model which assumed a linear relationship between time and conversion was used to describe NiO reduction. Nevertheless; differences in reactivity were observed during NiAl2O4 reduction depending on the type of support; α-Al2O3; or; γ-Al2O3; probably due to a different crystalline structure of the alumina. The changing grain size model for spherical grain geometry was used to obtain the kinetic parameters of the NiAl2O4 reduction working with both NiO-based oxygen-carriers. Chemical reaction control was assumed for NiO18-αAl whereas diffusion through the product layer was also considered when NiO21-γAl was used as oxygen-carrier. The oxidation reaction was very fast with both materials although small differences were observed again between NiO18-αAl and NiO21-γAl oxygen carriers; probably owing to the presence of a higher amount of NiAl2O4 in the solid supported on γ-Al2O3. The combined model for consecutive reduction of NiO and NiAl2O4 in the oxygen-carrier particles with the kinetic parameters obtained in this work predicted adequately the experimental results with both materials. These kinetic data could be used for the design of CLC and CLR systems. © 2012 Elsevier B.V;
D O I
暂无
中图分类号
学科分类号
摘要
Journal article (JA)
引用
收藏
相关论文
共 50 条
  • [1] Reduction and oxidation kinetics of nickel-based oxygen-carriers for chemical-looping combustion and chemical-looping reforming
    Dueso, Cristina
    Ortiz, Maria
    Abad, Alberto
    Garcia-Labiano, Francisco
    de Diego, Luis F.
    Gayan, Pilar
    Adanez, Juan
    CHEMICAL ENGINEERING JOURNAL, 2012, 188 : 142 - 154
  • [2] DETERMINATION OF REACTIVITY AND THERMODYNAMIC ANALYSIS OF NICKEL-BASED OXYGEN CARRIERS FOR CHEMICAL-LOOPING COMBUSTION
    Figueredo, Adolfo L.
    Carvalho, Fabiola C.
    Nascimento, Jose C.
    Ruiz, Juan A. C.
    Chiavone-Filho, Osvaldo
    Pereira, Camila G.
    BRAZILIAN JOURNAL OF CHEMICAL ENGINEERING, 2019, 36 (03) : 1155 - 1164
  • [3] Selection of oxygen carriers for chemical-looping combustion
    Adánez, J
    de Diego, LF
    García-Labiano, F
    Gayán, P
    Abad, A
    Palacios, JM
    ENERGY & FUELS, 2004, 18 (02) : 371 - 377
  • [4] Manganese ores as oxygen carriers for chemical-looping combustion (CLC) and chemical-looping with oxygen uncoupling (CLOU)
    Sundqvist, Sebastian
    Khalilian, Nazli
    Leion, Henrik
    Mattisson, Tobias
    Lyngfelt, Anders
    JOURNAL OF ENVIRONMENTAL CHEMICAL ENGINEERING, 2017, 5 (03): : 2552 - 2563
  • [5] Chemical-looping combustion and chemical-looping reforming in a circulating fluidized-bed reactor using Ni-based oxygen carriers
    Ryden, Magnus
    Lyngfelt, Anders
    Mattisson, Tobias
    ENERGY & FUELS, 2008, 22 (04) : 2585 - 2597
  • [7] Innovative Oxygen Carriers Uplifting Chemical-looping Combustion
    Mattisson, Tobias
    Adanez, Juan
    Mayer, Karl
    Snijkers, Frans
    Williams, Gareth
    Wesker, Evert
    Bertsch, Otmar
    Lyngfelt, Anders
    12TH INTERNATIONAL CONFERENCE ON GREENHOUSE GAS CONTROL TECHNOLOGIES, GHGT-12, 2014, 63 : 113 - 130
  • [8] Reduction kinetics of iron-based oxygen carriers using methane for chemical-looping combustion
    Luo, Ming
    Wang, Shuzhong
    Wang, Longfei
    Lv, Mingming
    JOURNAL OF POWER SOURCES, 2014, 270 : 434 - 440
  • [9] Modeling of chemical-looping combustion process of methane with nickel-based oxygen carrier
    Kaige Zhang
    Jin Liang
    Huili Liu
    Guirong Bao
    Hua Wang
    Experimental and Computational Multiphase Flow, 2024, 6 : 180 - 194
  • [10] Continuous regime of chemical-looping combustion (CLC) and chemical-looping with oxygen uncoupling (CLOU) reactivity of CuO oxygen carriers
    Zhou, Zhiquan
    Han, Lu
    Nordness, Oscar
    Bollas, George M.
    APPLIED CATALYSIS B-ENVIRONMENTAL, 2015, 166 : 132 - 144