Rolling of Al-Cu bimetallic bars in modified elongating grooves

被引:0
|
作者
Mróz, Sebastian [1 ]
Szota, Piotr [1 ]
Wąsek, Seweryn [1 ]
Stefanik, Andrzej [1 ]
机构
[1] Częstochowa University of Technology, Institute of Metal Forming and Safety Enginering, Al. Armii Krajowej 19, Czestochowa,42-200, Poland
关键词
Explosive welding - Cladding (coating) - Copper alloys - Explosives - Aluminum alloys;
D O I
10.4028/www.scientific.net/SSP.220-221.875
中图分类号
学科分类号
摘要
In order to enhance the uniformity of cladding copper layer distribution over the bimetallic bar perimeter and length, the shape of the classical horizontal and vertical oval passes were modified. The rolling was carried out in the designed modified elongating grooves. The round Al-Cu bimetallic bars with an outer diameter of 22 mm and a copper layer share of 15 and 30%, after explosive cladding, were rolled on a D150 two-high shape mill. As a result of rolling in 4 passes, bars of a diameter of about 16.0 mm were obtained. By applying the modified grooves to the rolling of Al-Cu bimetallic bars, the stability of the rolling process was improved, whereby, finished bars with a uniform and tight cladding layer distribution over the core and small diameter dimensional deviations was obtained. © (2015) Trans Tech Publications, Switzerland.
引用
收藏
页码:875 / 880
相关论文
共 50 条
  • [41] Age hardening and creep resistance of cast Al-Cu alloy modified by praseodymium
    Bai, Zhihao
    Qiu, Feng
    Wu, Xiaoxue
    Liu, Yingying
    Jiang, Qichuan
    MATERIALS CHARACTERIZATION, 2013, 86 : 185 - 189
  • [42] Microstructural mechanism in adiabatic shear bands of Al-Cu alloy bars using electromagnetic impact upsetting
    Zhang Xu
    Cui Junjia
    Li Guangyao
    MATERIALS LETTERS, 2017, 194 : 62 - 65
  • [43] Microstructure and microtexture evolution of shear bands in Al-Cu single crystal during asymmetric rolling
    Guo, Xiaobin
    Deng, Yunlai
    Zhang, Yong
    Zhang, Jin
    Zhang, Xinming
    MATERIALS CHARACTERIZATION, 2017, 128 : 37 - 42
  • [44] Effects of Warm Rolling Deformation on the Microstructure and Ductility of Large 2219 Al-Cu Alloy Rings
    Guo, Wanfu
    Yi, Youping
    Huang, Shiquan
    He, Hailin
    Fang, Jie
    METALS AND MATERIALS INTERNATIONAL, 2020, 26 (01) : 56 - 68
  • [45] MICROSTRUCTURE, CORROSION AND WEAR BEHAVIOUR OF UFG-POWDER-METALLURGICAL Al-Cu ALLOYS, Al-Cu/Al2O3(p) AND Al-Cu/SiC(p) COMPOSITES
    Nickel, D.
    Alisch, G.
    Podlesak, H.
    Hockauf, M.
    Fritsche, G.
    Lampke, T.
    REVIEWS ON ADVANCED MATERIALS SCIENCE, 2010, 25 (03) : 261 - 269
  • [46] Decolorization of the azo dye reactive red X-3B by an Al-Cu bimetallic system
    National Engineering Research Center for Urban Pollution Control, Tongji University, Shanghai 200092, China
    Huanjing Kexue, 2008, 6 (1587-1592): : 1587 - 1592
  • [47] Assessment of atomic mobilities of Al and Cu in fcc Al-Cu alloys
    Liu, Dandan
    Zhang, Lijun
    Du, Yong
    Xu, Honghui
    Liu, Shuhong
    Liu, Libin
    CALPHAD-COMPUTER COUPLING OF PHASE DIAGRAMS AND THERMOCHEMISTRY, 2009, 33 (04): : 761 - 768
  • [48] Al-Cu approximants in the Al3Cu4 alloy
    Dong, C
    Zhang, QH
    Wang, DH
    Wang, YM
    EUROPEAN PHYSICAL JOURNAL B, 1998, 6 (01): : 25 - 32
  • [49] Precipitation of Al2Cu in blanket Al-Cu films
    Marcus, MA
    Bower, JE
    JOURNAL OF APPLIED PHYSICS, 1997, 82 (08) : 3821 - 3827
  • [50] Microplasma oxidation of Al-Cu alloys
    Moskovskij Inst Stali i Splavov, Moscow, Russia
    Zashchita Metallov, 1995, 31 (05): : 523 - 531