Experimental Research on the Structural Performance of Shield Tunnel Segments Subjected to Different Fire Temperatures

被引:1
|
作者
Chen, Hongbin [1 ]
Jiang, Yujing [1 ]
Pan, Dongdong [2 ]
Sun, Huibin [3 ]
Zhang, Qian [4 ]
Yan, Peng [5 ,6 ]
机构
[1] Nagasaki Univ, Grad Sch Engn, Nagasaki 8528521, Japan
[2] Shandong Univ, Res Ctr Geotech & Struct Engn, Jinan 250061, Peoples R China
[3] Shandong Jianzhu Univ, Sch Transportat Engn, Jinan 250101, Peoples R China
[4] Shijiazhuang Tiedao Univ, Key Lab Struct Hlth Monitoring & Control, Shijiazhuang 050043, Peoples R China
[5] Shandong Univ Sci & Technol, State Key Lab Min Disaster Prevent & Control Cofou, Qingdao 266590, Peoples R China
[6] Shandong Univ Sci & Technol, Minist Sci & Technol, Qingdao 266590, Peoples R China
关键词
Shield tunnel segment; Different fire temperatures; Physical damage; Temperature distribution; Mechanical behavior; MAGNESIUM OXYSULFATE CEMENT; MECHANICAL-PROPERTIES; COMPOSITE BINDERS; WATER RESISTANCE; MICROSTRUCTURE; MGO-MGCL2-H2O; CARBONATION; STRENGTH; CONCRETE; FESO4;
D O I
10.1061/JMCEE7.MTENG-17685
中图分类号
TU [建筑科学];
学科分类号
0813 ;
摘要
In order to determine the damaging effect of different fire temperatures on a segment, experimental research was carried out on the structural performance of segments subjected to different fire temperatures. A temperature plateau occurred when the temperature reached 100 degrees C. There were two temperature layers across the 300 mm thickness of the segment due to heating on one side only, and the temperature gradient within 0-50 mm was much more significant than that within 50-300 mm. The concrete spalling and the cracking initiated on the fired surface of the segment were severe; the maximum depth of concrete spalling on the fired surface of the segment at different fire temperatures was 600 degrees C: 15 mm; 800 degrees C: 45 mm; and 1,000 degrees C: 67 mm; further, the main reinforcement was exposed or even softened. Cracking was also initiated on the unfired surface, and even penetrating cracks developed on the side surface. The damage at both ends of the segment was more severe than that in the center. The fire temperatures were 600 degrees C, 800 degrees C, and 1,000 degrees C, the maximum midspan deflections were 5.27, 7.83, and 11.79 mm, the maximum midspan axial forces were 65.58, 208.41, and 333.63 kN, and the maximum reinforcement stresses were 22.49, 35.08, and 52.63 MPa, respectively. The mechanical parameters of the segment increased during the firing process and recovered during the cooling process, which is equivalent to a loading and unloading cycle for the segment. This study advances the understanding of the structural performance of shield tunnel segments subjected to different fire temperatures.
引用
收藏
页数:11
相关论文
共 50 条
  • [21] Experimental investigation on fire damage to staggered segmental lining of shield tunnel
    Chen, Hongbin
    Liu, Teng
    You, Xinhua
    Yuan, Dajun
    Ping, Yang
    Zhang, Qinglin
    TUNNELLING AND UNDERGROUND SPACE TECHNOLOGY, 2023, 141
  • [22] Experimental Study on Fire Resistant of Shield Tunnel Segment in Civil Engineering
    Guo, Xinjun
    Xu, Zhisheng
    Zhang, Yan
    ADVANCED RESEARCH ON CIVIL ENGINEERING AND MATERIAL ENGINEERING, 2012, 568 : 7 - 12
  • [23] Research on corrosion deterioration and failure process of shield tunnel segments under loads
    Liu, Sijin
    He, Chuan
    Feng, Kun
    An, Zheli
    Tumu Gongcheng Xuebao/China Civil Engineering Journal, 2018, 51 (06): : 120 - 128
  • [24] Research on the Deterioration Characteristics of Shield Tunnel Segments under the Action of Seawater Erosion
    Xu, Chong
    Guo, Jiaqi
    Xu, Yafeng
    Lin, Jinhai
    Xue, Dandan
    Zhao, Qiulin
    Journal of Railway Engineering Society, 2021, 38 (06) : 58 - 63
  • [25] Structural safety assessment of concrete tunnel shells subjected to fire loading
    Zeiml, Matthias
    Lackner, Roman
    Mang, Herbert A.
    Computational Modelling of Concrete Structures, 2006, : 821 - 831
  • [26] Experimental study on ultimate bearing capacity of shield tunnel segments under unloading conditions
    Zhang, K. P.
    Zhang, X. H.
    Zhang, Q.
    Pei, Z. C.
    Qi, L. Z.
    PROCEEDINGS OF THE ITA-AITES WORLD TUNNEL CONGRESS 2023, WTC 2023: Expanding Underground-Knowledge and Passion to Make a Positive Impact on the World, 2023, : 3343 - 3350
  • [27] Analysis and thinking on structural performance evolution of shield tunnel lining
    Zhu M.
    Chen X.-S.
    Wang X.-T.
    Gongcheng Lixue/Engineering Mechanics, 2022, 39 (03): : 33 - 50
  • [28] Experimental study on the tensile performance of circumferential joint in shield tunnel
    Wang, Qi
    Geng, Ping
    Guo, Xiangyu
    Zeng, Guanxiong
    Chen, Changjian
    He, Chuan
    TUNNELLING AND UNDERGROUND SPACE TECHNOLOGY, 2021, 112
  • [29] Experimental study on the performance of shield tunnel tail grout in ground
    Liang, Jiaxin
    Liu, Wei
    Yin, Xinsheng
    Li, Wentao
    Yang, Zhe
    Yang, Jichen
    UNDERGROUND SPACE, 2025, 20 : 277 - 292
  • [30] Structural fire performance of concrete and shotcrete tunnel liners
    Caner, A
    Zlatanic, S
    Munfah, N
    JOURNAL OF STRUCTURAL ENGINEERING-ASCE, 2005, 131 (12): : 1920 - 1925