Investigation of microstructure and microtexture development and its correlation with mechanical and formability behavior of dissimilar friction stir welded AA6061 and AA5754 sheets

被引:1
|
作者
Datta, Rahul [1 ]
Bhargava, Marrapu [1 ]
机构
[1] Natl Inst Technol Warangal, Dept Mech Engn, Warangal 506004, India
来源
关键词
Al alloys; Friction stir welding; Formability; Microstructures; Microtextures; ALUMINUM-ALLOY; WELDING PARAMETERS; TENSILE PROPERTIES; TEXTURE EVOLUTION; GRAIN-STRUCTURE; AL-ALLOY; DEFORMATION; JOINTS; VIBRATION; AA7075;
D O I
10.1016/j.mtcomm.2024.110556
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The major attention of the automotive, aerospace, and marine industries currently is towards light-weight structural parts, and this can be achieved by the use of the tailor-welded blanks (TWBs). Using Al alloys as a member of the TWBs lessens the structural weight further, but conventional fusion welding of these alloys is often associated with defects such as porosity, manifestation of segregation and under-fill formation. Friction stir welding (FSW) is a feasible approach not only for producing welds with minimal defects but also for their enhanced formability, which finds extensive applications across industries. Due to its capability of completely negating the rolling directional properties of the as-received sheet, FSW increases the uniformity in the strain distribution during the course of deformation. In the present study, the objective was to perform FSW for dissimilar materials (with advancing side AA6061 and retreating side AA5754 sheets) with a similar thickness of 1.5 mm and to investigate the formability behavior of the TWBs. The effect of different FSW process parameters like rotational speed (950 rpm, 1100 rpm, 1250 rpm, and 1400 rpm) and traverse speed (50 mm/min, 75 mm/min, and 100 mm/min) which were selected based on visual inspection and macrostructure studies of the welds, was investigated on the formability and mechanical behavior of welded AA6061 and AA5754 sheets. Tensile tests were performed for base materials along with the specimens welded at different process parameters according to ASTM E8 standard to evaluate the mechanical properties. Micro-hardness tests were performed at several locations of the cross-section in the transverse direction to the weld in either side. The assessment of formability was executed by deforming the as-received and welded specimens in uniaxial strain paths, plane strain paths, and biaxial strain paths using Limit Dome Height (LDH) tests. Tensile test evaluation of 1250 rpm-50 mm/min, 1250 rpm-75 mm/min, 1400 rpm-50 mm/min, and 1400 rpm-75 mm/min parameter combinations exhibited cracks away from the weld center towards the advancing side (AA6061 side) of the specimens, indicating good quality of the welds, which was in agreement with the stir zone macrostructures. The micro-hardness distribution plots also showed a drop in the hardness in the TMAZ of the advancing side, making it the weakest region of the weld. It has been observed from the LDH test that the formability of all the FSWed specimens was intermediate to the formability of AA5754 (superior formability) and AA6061 (inferior formability), irrespective of the strain paths that might be correlated to their corresponding strain hardening exponents. In the case of uniaxial and plane strain paths in the welded specimens, the failure was towards the advancing side, which was in agreement with the tensile properties, but in the case of biaxial stretching, it was failing at the weld center due to their corresponding microstructural characteristics. An abnormal behavior was witnessed in the equibiaxial stretching, i.e., the minor strain attained for all the welded specimens was significantly less. Comprehensive studies on microstructure and microtexture were performed on the un-deformed and deformed specimens to investigate the peculiar behavior, and it was inferred that the initial local misorientations play a pivotal role in determining the grain orientation spread (GOS) post-deformation. It was further observed that the average GOS values were analogous across all the deformed welded samples in their respective strain paths. It's noteworthy that the presence of the Cube texture component in the biaxial strain path significantly mitigated the impact of the Goss texture, resulting in the peculiar behavior i.e. a notable decrease in the minor strain observed in the deformed welded specimens in the biaxial strain path.
引用
收藏
页数:29
相关论文
共 50 条
  • [41] Microstructure and anisotropic mechanical behavior of friction stir welded AA2024 alloy sheets
    Zhang, Zhihan
    Li, Wenya
    Li, Jinglong
    Chao, Y. J.
    Vairis, A.
    MATERIALS CHARACTERIZATION, 2015, 107 : 112 - 118
  • [42] Mechanical behavior of AA5083/AA6061 friction stir welds using modal analysis
    Cavus, Emre Can
    Kocar, Oguz
    MATERIALS TESTING, 2023, 65 (06) : 961 - 971
  • [43] Optimization of process parameters of friction stir welded joints of dissimilar aluminum alloys AA3003 and AA6061 by RSM
    Nait Salah A.
    Mehdi H.
    Mehmood A.
    Wahab Hashmi A.
    Malla C.
    Kumar R.
    Materials Today: Proceedings, 2022, 56 : 1675 - 1683
  • [44] Effect of Overlapping Friction Stir Processing on Microstructure, Mechanical Properties and Corrosion Behavior of AA6061 Alloy
    Satyanarayana, Marukurti V. N. V.
    Adepu, Kumar
    Chauhan, Karan
    METALS AND MATERIALS INTERNATIONAL, 2021, 27 (09) : 3563 - 3573
  • [45] INFLUENCE OF POST-WELDING HEAT TREATMENT ON MECHANICAL AND MICROSTRUCTURAL BEHAVIOR OF FRICTION STIR WELDED AA7075-T651 AND AA6061 DISSIMILAR JOINTS
    Yuvaraj, K. P.
    Varthanan, P. Ashoka
    Boopathiraja, K. P.
    HIGH TEMPERATURE MATERIAL PROCESSES, 2018, 22 (01): : 17 - 34
  • [46] Shear texture development and microstructural analysis of friction stir welded AA5754 sheets during forming at different strain paths
    Datta, Rahul
    Bhargava, Marrapu
    MATERIALS TODAY COMMUNICATIONS, 2024, 38
  • [47] Investigation of Mechanical and Metallurgical Properties of Friction Stir Corner Welded Dissimilar Thickness AA5086-AA6061 Aluminium Alloys
    Krishnan, Manigandan
    Subramaniam, Senthil Kumar
    MATERIALS RESEARCH-IBERO-AMERICAN JOURNAL OF MATERIALS, 2018, 21 (04):
  • [48] Microstructure and tensile properties of friction stir welded dissimilar AA6061-AA5086 aluminium alloy joints
    Ilangovan, M.
    Boopathy, S. Rajendra
    Balasubramanian, V.
    TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2015, 25 (04) : 1080 - 1090
  • [49] Effect of Overlapping Friction Stir Processing on Microstructure, Mechanical Properties and Corrosion Behavior of AA6061 Alloy
    Marukurti V. N. V. Satyanarayana
    Kumar Adepu
    Karan Chauhan
    Metals and Materials International, 2021, 27 : 3563 - 3573
  • [50] Friction stir welding parameters optimization for tailored welded blank sheets of AA1100 with AA6061 dissimilar alloy using response surface methodology
    Mallieswaran, K.
    Padmanabhan, R.
    Balasubramanian, V
    ADVANCES IN MATERIALS AND PROCESSING TECHNOLOGIES, 2018, 4 (01) : 142 - 157