Investigation of microstructure and microtexture development and its correlation with mechanical and formability behavior of dissimilar friction stir welded AA6061 and AA5754 sheets

被引:1
|
作者
Datta, Rahul [1 ]
Bhargava, Marrapu [1 ]
机构
[1] Natl Inst Technol Warangal, Dept Mech Engn, Warangal 506004, India
来源
关键词
Al alloys; Friction stir welding; Formability; Microstructures; Microtextures; ALUMINUM-ALLOY; WELDING PARAMETERS; TENSILE PROPERTIES; TEXTURE EVOLUTION; GRAIN-STRUCTURE; AL-ALLOY; DEFORMATION; JOINTS; VIBRATION; AA7075;
D O I
10.1016/j.mtcomm.2024.110556
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The major attention of the automotive, aerospace, and marine industries currently is towards light-weight structural parts, and this can be achieved by the use of the tailor-welded blanks (TWBs). Using Al alloys as a member of the TWBs lessens the structural weight further, but conventional fusion welding of these alloys is often associated with defects such as porosity, manifestation of segregation and under-fill formation. Friction stir welding (FSW) is a feasible approach not only for producing welds with minimal defects but also for their enhanced formability, which finds extensive applications across industries. Due to its capability of completely negating the rolling directional properties of the as-received sheet, FSW increases the uniformity in the strain distribution during the course of deformation. In the present study, the objective was to perform FSW for dissimilar materials (with advancing side AA6061 and retreating side AA5754 sheets) with a similar thickness of 1.5 mm and to investigate the formability behavior of the TWBs. The effect of different FSW process parameters like rotational speed (950 rpm, 1100 rpm, 1250 rpm, and 1400 rpm) and traverse speed (50 mm/min, 75 mm/min, and 100 mm/min) which were selected based on visual inspection and macrostructure studies of the welds, was investigated on the formability and mechanical behavior of welded AA6061 and AA5754 sheets. Tensile tests were performed for base materials along with the specimens welded at different process parameters according to ASTM E8 standard to evaluate the mechanical properties. Micro-hardness tests were performed at several locations of the cross-section in the transverse direction to the weld in either side. The assessment of formability was executed by deforming the as-received and welded specimens in uniaxial strain paths, plane strain paths, and biaxial strain paths using Limit Dome Height (LDH) tests. Tensile test evaluation of 1250 rpm-50 mm/min, 1250 rpm-75 mm/min, 1400 rpm-50 mm/min, and 1400 rpm-75 mm/min parameter combinations exhibited cracks away from the weld center towards the advancing side (AA6061 side) of the specimens, indicating good quality of the welds, which was in agreement with the stir zone macrostructures. The micro-hardness distribution plots also showed a drop in the hardness in the TMAZ of the advancing side, making it the weakest region of the weld. It has been observed from the LDH test that the formability of all the FSWed specimens was intermediate to the formability of AA5754 (superior formability) and AA6061 (inferior formability), irrespective of the strain paths that might be correlated to their corresponding strain hardening exponents. In the case of uniaxial and plane strain paths in the welded specimens, the failure was towards the advancing side, which was in agreement with the tensile properties, but in the case of biaxial stretching, it was failing at the weld center due to their corresponding microstructural characteristics. An abnormal behavior was witnessed in the equibiaxial stretching, i.e., the minor strain attained for all the welded specimens was significantly less. Comprehensive studies on microstructure and microtexture were performed on the un-deformed and deformed specimens to investigate the peculiar behavior, and it was inferred that the initial local misorientations play a pivotal role in determining the grain orientation spread (GOS) post-deformation. It was further observed that the average GOS values were analogous across all the deformed welded samples in their respective strain paths. It's noteworthy that the presence of the Cube texture component in the biaxial strain path significantly mitigated the impact of the Goss texture, resulting in the peculiar behavior i.e. a notable decrease in the minor strain observed in the deformed welded specimens in the biaxial strain path.
引用
收藏
页数:29
相关论文
共 50 条
  • [21] Effect of Friction Stir Processing on Microstructure and Mechanical Properties of TIG Welded Joint of AA6061 and AA7075
    Husain Mehdi
    R. S. Mishra
    Metallography, Microstructure, and Analysis, 2020, 9 : 403 - 418
  • [22] A parametric study of friction stir welded AA6061/SiC AMC and its effect on microstructure and mechanical properties
    Kumar, Devender
    Ottarackal, Denny J.
    Acharya, Uttam
    Medhi, Tanmoy
    Roy, Barnik Saha
    Saha, Subhash Chandra
    MATERIALS TODAY-PROCEEDINGS, 2021, 46 : 9378 - 9386
  • [23] A COMPARISON OF MICROSTRUCTURE AND MECHANICAL PROPERTIES OF TIG AND MIG WELDED DISSIMILAR AA7075 / AA6061 ALUMINIUM ALLOYS SUBJECTED TO FRICTION STIR PROCESSING
    Rana, Rajeev
    Karunakar, D. B.
    Karmakar, Anish
    PROCEEDINGS OF ASME 2023 18TH INTERNATIONAL MANUFACTURING SCIENCE AND ENGINEERING CONFERENCE, MSEC2023, VOL 2, 2023,
  • [24] Improvement of microstructure and corrosion properties of friction stir welded AA5754 by adding Zn interlayer
    Ali Shamsipur
    Amir Anvari
    Ahmad Keyvani
    International Journal of Minerals, Metallurgy, and Materials, 2018, 25 : 967 - 973
  • [25] Effect of SiC nanoparticles on the microstructure and texture of friction stir welded AA2024/AA6061
    Moradi, Mohammad Mahdi
    Aval, Hamed Jamshidi
    Jamaati, Roohollah
    Amirkhanlou, Sajjad
    Ji, Shouxun
    MATERIALS CHARACTERIZATION, 2019, 152 : 169 - 179
  • [26] Submerged Dissimilar Friction Stir Welding of AA6061 and AA7075 Aluminum Alloys: Microstructure Characterization and Mechanical Property
    Heidarzadeh, Akbar
    Javidani, Mousa
    Mofarrehi, Mohammadreza
    Farzaneh, Amir
    Chen, X-Grant
    METALS, 2021, 11 (10)
  • [27] Effects of rotational speed on microstructure and mechanical properties of dissimilar AA6061 and AA7075 friction stir welding joints
    Zhang, Jian
    Fan, Wen
    Zhu, Hai
    Wang, Wenlong
    Zeng, Tao
    JOURNAL OF MECHANICAL SCIENCE AND TECHNOLOGY, 2025, 39 (01) : 181 - 192
  • [28] Improvement of microstructure and corrosion properties of friction stir welded AA5754 by adding Zn interlayer
    Ali Shamsipur
    Amir Anvari
    Ahmad Keyvani
    International Journal of Minerals Metallurgy and Materials, 2018, 25 (08) : 967 - 973
  • [29] Improvement of microstructure and corrosion properties of friction stir welded AA5754 by adding Zn interlayer
    Shamsipur, Ali
    Anvari, Amir
    Keyvani, Ahmad
    INTERNATIONAL JOURNAL OF MINERALS METALLURGY AND MATERIALS, 2018, 25 (08) : 967 - 973
  • [30] Effect of Tool Travel Rate on Microstructure Evolution and Mechanical Properties of Dissimilar Friction Stir Welded Joints of AA7075 and AA6061 Aluminium Alloys
    Rana, Rajeev
    Karmakar, Anish
    Karunakar, D. B.
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2024, 33 (20) : 10835 - 10852