Natural Aging Behaviour of the EN AW 6082 and Lead Free EN AW 6023 Aluminium Alloys

被引:0
|
作者
Fujda M. [1 ]
Matvija M. [1 ]
Glogovský M. [1 ]
Orišenko I. [1 ]
机构
[1] Faculty of Materials, Metallurgy and Recycling, Technical University of Kosice, Letna 9, Kosice
来源
Manufacturing Technology | 2017年 / 17卷 / 05期
关键词
AlMgSi alloy; Mechanical properties; Microstructure; Natural aging; Sn;
D O I
10.21062/ujep/x.2017/a/1213-2489/MT/17/5/701
中图分类号
学科分类号
摘要
The natural aging behaviour of EN AW 6082 aluminium alloy and lead-free EN AW 6023 aluminium alloy with good free cutting machinability was investigated using Vickers microhardness measurements, tensile test analysis, and a light microscopy characterisation. The different chemical composition of the analysed alloys did not affect the alloys microhardness after quenching, but the solid solution grain sizes of the quenched alloys differed greatly. The microhardness and tensile strength of EN AW 6082 increased with aging time right after alloy quenching. On the contrary, microhardness and tensile strength of lead-free EN AW 6023 increased markedly until after 500 hours of natural aging. The natural aging of the 6023 alloy could be suppressed by the formation of Sn-vacancy pairs after alloy quenching that impede the strengthening clusters formation. Finer grains of solid solution that were found in the 6023 alloy microstructure resulted in higher tensile strength and lower ductility of the 6023 alloy compared to the 6082 alloy, even though the microhardness of the naturally aged 6023 alloy state was lower. © 2017 Copyright © 2017. Published by Manufacturing Technology. All rights reserved. All Rights Reserved.
引用
收藏
页码:19 / 20
页数:1
相关论文
共 50 条
  • [21] Experimental Analysis of the Behaviour of Aluminium Alloy EN 6082AW T6 at High Temperature
    Toric, Neno
    Brnic, Josip
    Boko, Ivica
    Brcic, Marino
    Burgess, Ian W.
    Uzelac, Ivana
    METALS, 2017, 7 (04):
  • [22] EFFECT OF AGING PARAMETERS OF EN AW-7021 ALUMINIUM ALLOYS ON STRESS CORROSION CRACKING
    Boczkal, S.
    Wegrzyn, M.
    Szymanski, W.
    Bem, J.
    Wala, K.
    Plonka, B.
    Lesniak, D.
    Nowak, M.
    ARCHIVES OF METALLURGY AND MATERIALS, 2024, 69 (03) : 1061 - 1069
  • [23] Enhanced Mechanical Properties of Aluminium Alloy EN AW 6082 Recycled without Remelting
    Krolo, Jure
    Lela, Branimir
    Ljumovic, Petar
    Bagavac, Petra
    TEHNICKI VJESNIK-TECHNICAL GAZETTE, 2019, 26 (05): : 1253 - 1259
  • [24] The Influence of the Casting Speed in Horizontal Continuous Casting of Aluminium Alloy EN AW 6082
    Obali, Akin
    Dilek, Kerem Ahmet
    Akdi, Seracettin
    Urk, Deniz Kavrar
    Gokelma, Mertol
    LIGHT METALS 2021, 50TH EDITION, 2021, : 900 - 906
  • [25] Controlled grain size distribution and refinement of an EN AW-6082 aluminium alloy
    Lampke, Thomas
    Dietrich, Dagmar
    Nickel, Daniela
    Bergmann, Markus
    Zachaeus, Rene
    Neugebauer, Reimund
    INTERNATIONAL JOURNAL OF MATERIALS RESEARCH, 2011, 102 (08) : 977 - 981
  • [26] Effect of natural aging on mechanical response of the artificially aged EN AW 6063 aluminium alloy
    Fujda M.
    Matvija M.
    Glogovský M.
    Materials Science Forum, 2019, 952 : 74 - 81
  • [27] Continuous Time-Temperature-Precipitation-Diagrams of the Aluminium Alloys EN AW-7020 and EN AW-7050 Discussion
    Krug, P.
    Prietzel, K. -O.
    von Hehl, A.
    von Bargen, R.
    HTM-JOURNAL OF HEAT TREATMENT AND MATERIALS, 2007, 62 (06): : 293 - 293
  • [28] Deterioration of Property of Aluminum Alloys (EN AW-1050A, EN AW-5754 and EN AW-6060) by Absorbed Hydrogen
    Wlodarczyk, Pawel P.
    Wlodarczyk, Barbara
    APPLIED SCIENCES-BASEL, 2022, 12 (03):
  • [29] Study of Corrosion, Structural, and Mechanical Properties of EN AW-6082 and EN AW-7075 Welded Joints
    Wojdat, Tomasz
    Kustron, Pawel
    Jaskiewicz, Karol
    Pabian, Jaroslaw
    MATERIALS, 2021, 14 (16)
  • [30] Dependency of mechanical properties on artificial aging conditions for EN AW 6082 aluminum alloy
    Gortan, Mehmet Okan
    Yuksel, Berkay
    METALLURGICAL RESEARCH & TECHNOLOGY, 2023, 120 (02)