Additively manufactured fine-grained Al-Fe-Cu-Sc-Zr alloy with resistance to brittleness under high temperature

被引:0
|
作者
Shi, Qianyu [1 ]
Chen, Jibing [1 ]
Chen, Junsheng [1 ]
Wang, Yueting [2 ,3 ]
Xia, Xizhen [2 ,3 ]
Li, Ruidi [2 ,3 ]
机构
[1] Wuhan Polytech Univ, Sch Mech Engn, Wuhan 430023, Hubei, Peoples R China
[2] Cent South Univ, Powder Met Res Inst, Changsha 410083, Hunan, Peoples R China
[3] Cent South Univ, State Key Lab Powder Met, Changsha 410083, Hunan, Peoples R China
基金
中国国家自然科学基金;
关键词
Additive manufacturing; Laser powder bed fusion; Aluminum alloy; Anti-brittleness; High temperature; MECHANICAL-PROPERTIES; MICROSTRUCTURAL EVOLUTION; DEFORMATION-BEHAVIOR; LASER; SOLIDIFICATION; DEPENDENCE;
D O I
10.1016/j.jmrt.2024.11.104
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Existing additively manufactured aluminum alloys exhibit a sharp decrease in yield strength at moderate temperatures (200 degrees C-400 degrees C), failing to meet the high-temperature resistance required in the complex service environments of aerospace applications. In this paper, an Al-2.5Fe-2Cu-0.6Sc-0.3Zr alloy material was designed and formed by laser powder bed fusion (L-PBF) technology. The optimal composition ratio was obtained by comparing the formed structures and properties, and then the phase composition, microstructure, precipitation distribution and mechanical properties were characterized and analyzed at high temperature. The result shows that the alloy's primary precipitate phases are Al6Fe (Al23CuFe4) and L12-Al3(Sc, Zr) at nano scale. Adding Zr and Sc, the thermal stability of Al6Fe is enhanced, delaying its transformation to the 0-Al13Fe4 phase and refining the particle size. The Al23CuFe4 phase, stabilized thermodynamically by substituting of Cu for Al atoms in the orthorhombic structure (oC28), also contributes to the stabilization of the Al6Fe phase. Moreover, This aluminum alloy obtained a yield strength of 449 MPa at room temperature and a yield strength of 142 MPa at 300 degrees C. In addition, it also shows excellent brittleness resistance under high temperature, which is better than most L-PBF aluminum alloys reported so far. These findings offer valuable insights for the future development of aluminumbased alloys with heat-resistant performance, and promising strategies for addressing particle coarsening under high temperature and intermediate-temperature brittleness.
引用
收藏
页码:7310 / 7324
页数:15
相关论文
共 50 条
  • [41] Liquid Phase Behavior during Elevated Temperature Deformation of the Fine-Grained 5083 Al Alloy
    Honghua Yan and Kaifeng Zhang School of Materials Science and Engineering
    Journal of Materials Science & Technology, 2009, 25 (05) : 673 - 676
  • [42] An additively manufactured heat-resistant Al-Ce-Sc-Zr alloy: Microstructure, mechanical properties and thermal stability
    Yang, Ziwei
    Chen, Chao
    Li, Dan
    Wu, Yiyou
    Geng, Zhaowen
    Konakov, Vladimir
    Zhou, Kechao
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2023, 872
  • [43] Effect of sintering temperature on fine-grained Cu-W composites with high copper
    Wang, Xiran
    Wei, Shizhong
    Xu, Liujie
    Fang, Fang
    Li, Jiwen
    Pan, Kunming
    Peng, Bo
    MATERIALS CHARACTERIZATION, 2019, 153 : 121 - 127
  • [44] Novel Fabrication of Bulk Fine-Grained Al-Cu-Mg Alloy with Superior Mechanical Properties
    Zheng, Ruixiao
    Ma, Chaoli
    ADVANCED ENGINEERING MATERIALS, 2016, 18 (06) : 1027 - 1035
  • [45] Enhancement of high-temperature deformation in fine-grained silicon carbide with Al doping
    Tokiyama, Takuya
    Shinoda, Yutaka
    Akatsu, Takashi
    Wakai, Fumihiro
    MATERIALS SCIENCE AND ENGINEERING B-ADVANCED FUNCTIONAL SOLID-STATE MATERIALS, 2008, 148 (1-3): : 261 - 264
  • [46] Microstructure, metallurgical defects and hardness of Al–Cu–Mg–Li–Zr alloy additively manufactured by selective laser melting
    Xu, Rong
    Li, Ruidi
    Yuan, Tiechui
    Niu, Pengda
    Wang, Minbo
    Lin, Zehuan
    Journal of Alloys and Compounds, 2021, 835
  • [47] Creep deformation and cavitation in an additively manufactured Al-8.6Cu-0.4Mn-0.9Zr (wt%) alloy
    Rakhmonov, Jovid U.
    Michi, Richard
    Bahl, Sumit
    Rahman, Obaidullah
    Frederick, Curtis
    Ziabari, Amir Koushyar
    Dunand, David C.
    Dehoff, Ryan
    Plotkowski, Alex
    Shyam, Amit
    ADDITIVE MANUFACTURING, 2024, 84
  • [48] High temperature tensile behavior of ultra-fine grained Al-3.3Mg-0.2Sc-0.2Zr alloy by equal channel angular pressing
    Geng, HB
    Kang, SB
    Min, BK
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2004, 373 (1-2): : 229 - 238
  • [49] Microstructural evolution and strengthening mechanisms in a heat-treated additively manufactured Al-Cu-Mn-Zr alloy
    Michi, Richard A.
    Sisco, Kevin
    Bahl, Sumit
    Allard, Lawrence F.
    Wagner, Karla B.
    Poplawsky, Jonathan D.
    Leonard, Donovan N.
    Dehoff, Ryan R.
    Plotkowski, Alex
    Shyam, Amit
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2022, 840
  • [50] Improving the processability and grain structures of additively manufactured Al-Fe-Cu-xZr alloy: Experiment and high-fidelity simulation
    Xu, Jing-Yu
    Yuan, Wei-Hao
    Zhang, Cheng
    Pan, Jie
    Yin, Shuo
    Chen, Hui
    Liu, Lin
    ADDITIVE MANUFACTURING, 2024, 84