Additively manufactured fine-grained Al-Fe-Cu-Sc-Zr alloy with resistance to brittleness under high temperature

被引:0
|
作者
Shi, Qianyu [1 ]
Chen, Jibing [1 ]
Chen, Junsheng [1 ]
Wang, Yueting [2 ,3 ]
Xia, Xizhen [2 ,3 ]
Li, Ruidi [2 ,3 ]
机构
[1] Wuhan Polytech Univ, Sch Mech Engn, Wuhan 430023, Hubei, Peoples R China
[2] Cent South Univ, Powder Met Res Inst, Changsha 410083, Hunan, Peoples R China
[3] Cent South Univ, State Key Lab Powder Met, Changsha 410083, Hunan, Peoples R China
基金
中国国家自然科学基金;
关键词
Additive manufacturing; Laser powder bed fusion; Aluminum alloy; Anti-brittleness; High temperature; MECHANICAL-PROPERTIES; MICROSTRUCTURAL EVOLUTION; DEFORMATION-BEHAVIOR; LASER; SOLIDIFICATION; DEPENDENCE;
D O I
10.1016/j.jmrt.2024.11.104
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Existing additively manufactured aluminum alloys exhibit a sharp decrease in yield strength at moderate temperatures (200 degrees C-400 degrees C), failing to meet the high-temperature resistance required in the complex service environments of aerospace applications. In this paper, an Al-2.5Fe-2Cu-0.6Sc-0.3Zr alloy material was designed and formed by laser powder bed fusion (L-PBF) technology. The optimal composition ratio was obtained by comparing the formed structures and properties, and then the phase composition, microstructure, precipitation distribution and mechanical properties were characterized and analyzed at high temperature. The result shows that the alloy's primary precipitate phases are Al6Fe (Al23CuFe4) and L12-Al3(Sc, Zr) at nano scale. Adding Zr and Sc, the thermal stability of Al6Fe is enhanced, delaying its transformation to the 0-Al13Fe4 phase and refining the particle size. The Al23CuFe4 phase, stabilized thermodynamically by substituting of Cu for Al atoms in the orthorhombic structure (oC28), also contributes to the stabilization of the Al6Fe phase. Moreover, This aluminum alloy obtained a yield strength of 449 MPa at room temperature and a yield strength of 142 MPa at 300 degrees C. In addition, it also shows excellent brittleness resistance under high temperature, which is better than most L-PBF aluminum alloys reported so far. These findings offer valuable insights for the future development of aluminumbased alloys with heat-resistant performance, and promising strategies for addressing particle coarsening under high temperature and intermediate-temperature brittleness.
引用
收藏
页码:7310 / 7324
页数:15
相关论文
共 50 条
  • [21] Age hardening and the potential for superplasticity in a fine-grained Al-Mg-Li-Zr alloy
    Furukawa, M
    Berbon, PB
    Horita, Z
    Nemoto, M
    Tsenev, NK
    Valiev, RZ
    Langdon, TG
    METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1998, 29 (01): : 169 - 177
  • [22] Fine-grained structure and superplasticity of Al-Cu-Mg-Fe-Ni alloys
    Kotov, A. D.
    Mikhaylovskaya, A. V.
    Golovin, I. S.
    Portnoy, V. K.
    SUPERPLASTICITY IN ADVANCED MATERIALS, 2013, 735 : 55 - +
  • [23] High strain rate superplasticity in a fine-grained PM 7475 Al alloy
    Kim, WJ
    Kim, JK
    METALS AND MATERIALS INTERNATIONAL, 1998, 4 (06) : 1133 - 1141
  • [24] Structural and kinetic aspects of continuous grain coarsening in a fine-grained Al-0.3Sc alloy
    Ferry, M.
    Burhan, N.
    ACTA MATERIALIA, 2007, 55 (10) : 3479 - 3491
  • [25] Continuous and discontinuous grain coarsening in a fine-grained particle-containing Al-Sc alloy
    Ferry, M
    Hamilton, NE
    Humphreys, FJ
    ACTA MATERIALIA, 2005, 53 (04) : 1097 - 1109
  • [26] Fine-grained aluminium crossover alloy for high-temperature sheet forming
    Samberger, Sebastian
    Weissensteiner, Irmgard
    Stemper, Lukas
    Kainz, Christina
    Uggowitzer, Peter J.
    Pogatscher, Stefan
    ACTA MATERIALIA, 2023, 253
  • [27] Plastic deformation of fine-grained Al-Cu-Fe-(B) icosahedral poly-quasicrystals at elevated temperature
    Wang Jian-Bo
    Ma Jia-Yan
    Lu Lu
    Xiong Dong-Xia
    Zhao Dong-Shan
    Wang Ren-Hui
    CHINESE PHYSICS LETTERS, 2007, 24 (08) : 2331 - 2334
  • [28] Plastic deformation of fine-grained Al-Cu-Fe-(B) icosahedral poly-quasicrystals at elevated temperature
    Department of Physics, Wuhan University, Ministry of Education, Wuhan 430072, China
    不详
    Chin. Phys. Lett., 2007, 8 (2331-2334):
  • [29] Improved work hardening capability and ductility of an additively manufactured and deformed Al-Mn-Mg-Sc-Zr alloy
    Schliephake, Daniel
    Lopes, Christophe
    Eggeler, Yolita M.
    Chen, Hans
    Freudenberger, Jens
    Bayoumy, Dina
    Huang, Aijun J.
    Kauffmann, Alexander
    JOURNAL OF ALLOYS AND COMPOUNDS, 2022, 924
  • [30] An additively manufactured Al-14.1Mg-0.47Si-0.31Sc-0.17Zr alloy with high specific strength, good thermal stability and excellent corrosion resistance
    Jiang Bi
    Zhenglong Lei
    Yanbin Chen
    Xi Chen
    Nannan Lu
    Ze Tian
    Xikun Qin
    JournalofMaterialsScience&Technology, 2021, 67 (08) : 23 - 35