Effects of elevated temperatures on cold-formed stainless steel double shear bolted connections

被引:0
|
作者
Cai, Yancheng [1 ]
Young, Ben [1 ]
机构
[1] Hong Kong Polytech Univ, Dept Civil & Environm Engn, Hong Kong, Peoples R China
关键词
D O I
10.1201/9781003348450-168
中图分类号
TU [建筑科学];
学科分类号
0813 ;
摘要
A total of 35 cold-formed stainless steel double shear bolted connection specimens were tested using transient state test method. The specimens of bolted connections were fabricated by three different grades of stainless steel, namely, EN 1.4301 (AISI 304), EN 1.4571 (AISI 316Ti having small amount of titanium) and EN 1.4162 (AISI S32101). The connection tests were conducted at three different load levels of 0.25, 0.50 and 0.75 of the failure load at room temperature. The stainless steel grade EN 1.4571 generally performed better than the other two stainless steel grades as higher values of critical temperatures were obtained. Two failure modes, namely the bearing and net section tension failures, were observed in the transient state tests.
引用
收藏
页码:357 / 358
页数:2
相关论文
共 50 条
  • [22] An Experimental Study on Structural Behaviours of Single Shear Cold-formed Stainless Steel Bolted Connections with Two Bolts
    Kim, TaeSoo
    Kim, MinSeung
    Shin, SungWoo
    ADVANCES IN FRACTURE AND DAMAGE MECHANICS IX, 2011, 452-453 : 617 - +
  • [23] The capacity of bolted cold-formed steel connections in bending
    Mojtabaei, S. M.
    Becque, J.
    Hajirasouliha, I
    STABILITY AND DUCTILITY OF STEEL STRUCTURES 2019, 2019, : 830 - 838
  • [24] Countersunk bolted moment connections in cold-formed steel
    Becque, J.
    Hajirasouliha, I
    INSIGHTS AND INNOVATIONS IN STRUCTURAL ENGINEERING, MECHANICS AND COMPUTATION, 2016, : 1074 - 1079
  • [25] Design of cold-formed stainless steel tubular joints at elevated temperatures
    Feng, Ran
    Young, Ben
    ENGINEERING STRUCTURES, 2012, 35 : 188 - 202
  • [26] Performance of cold-formed stainless steel tubular columns at elevated temperatures
    To, Ernest Chiu-Yin
    Young, Ben
    ENGINEERING STRUCTURES, 2008, 30 (07) : 2012 - 2021
  • [27] Shear Strength of a Cold-Formed Steel Sheet in Bolted Connections Using Oversized Holes
    Yu, Cheng
    Xu, Ke
    JOURNAL OF STRUCTURAL ENGINEERING-ASCE, 2013, 139 (05): : 860 - 864
  • [28] Failure modes of bolted cold-formed steel connections under static shear loading
    Ip, KH
    Chung, KF
    ADVANCES IN STEEL STRUCTURES, VOLS 1 AND 2, 1999, : 269 - 276
  • [29] Finite Element Analysis on Structural Behaviours of Single Shear Cold-formed Stainless Steel Bolted Connections with Two Bolts
    Lee, YongTaeg
    Kim, TaeSoo
    Lim, JinSeong
    Kim, SeungHun
    ADVANCES IN FRACTURE AND DAMAGE MECHANICS IX, 2011, 452-453 : 613 - 616
  • [30] Bearing strength of cold-formed steel bolted connections with a gap
    Yu, Cheng
    Panyanouvong, Mark Xouphab
    THIN-WALLED STRUCTURES, 2013, 67 : 110 - 115