Microstructure and properties of a HIP manufactured SiC p reinforced high alloyed Al - Zn - Mg - Cu - Zr - Ti aluminum matrix composite

被引:4
|
作者
Yao, Hui [1 ]
Xu, Xiaojing [1 ]
Luo, Yuntian [1 ]
Han, Tian [1 ]
Zhou, Qingshan [1 ]
机构
[1] Jiangsu Univ, Inst Adv Mfg & Modern Equipment Technol, Zhenjiang, Peoples R China
来源
JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T | 2024年 / 30卷
关键词
Aluminum matrix composites; SiC particles; Microstructure; Mechanical properties; Corrosion properties; MECHANICAL-PROPERTIES; STRENGTHENING MECHANISMS; CORROSION BEHAVIOR; LOCALIZED CORROSION; TENSILE PROPERTIES; HEAT-TREATMENT; DEFORMATION; RESISTANCE; SUSCEPTIBILITY; PARTICLES;
D O I
10.1016/j.jmrt.2024.04.190
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
In this study, a hot isostatic pressing (HIP) manufactured SiC particles (SiC p ) reinforced high alloyed Al - Zn - Mg - Cu - Zr - Ti aluminum matrix composite was fabricated through ball-milling, HIP, homogenization, hot extrusion, solution treatment, and aging treatment. The results showed the presence of an interfacial reaction layer, MgAl 2 O 4 , around the SiC p , which enhanced the bonding between the particles and the matrix. The aging treatment resulted in the formation of different aging precipitates, which were featured by GP zone for T4, GP zone + eta ' (metastable MgZn 2 ) + eta (stable MgZn 2 ) for T6 and GP zone + eta ' (metastable MgZn 2 ) for T6I4. The composite samples of T4, T6, and T6I4 exhibited different mechanical properties. Specifically, the elastic modulus was measured as 102.9, 103.4, and 102.3 GPa, the yield strength was 685.3, 598.1, and 619.7 MPa, the ultimate tensile strength was 713.6, 618.9, and 633.3 MPa, and the elongation was 2.2%, 1.8%, and 2.8%, respectively. Furthermore, the corrosion behavior of the composite was evaluated through electrochemical, intergranular corrosion, and exfoliation corrosion. The corrosion current density was found to be 3.17 x 10 -7 , 4.97 x 10 -7 , and 3.67 x 10 -7 A cm -2 , the corrosion potential was measured as -0.70, -0.81, and -0.56 V, and the maximum intergranular corrosion depth was 139.9, 167.8, and 106.2 mu m for T4, T6, and T6I4, respectively. The severity of exfoliation corrosion varied, with T4 showing severe pitting, T6 exhibiting moderate pitting, and T6I4 displaying slight pitting. The strengthening mechanism and load transfer strengthening of the composites were discussed in detail based on theoretical calculations, and the anti-corrosion mechanisms were also analyzed.
引用
收藏
页码:4856 / 4867
页数:12
相关论文
共 50 条
  • [41] Microstructure and corrosion properties of aluminum matrix composite reinforced with al-based amorphous
    Liu, Peng
    Li, Shi-Kai
    Zhang, Yuan-Bin
    Liu, Yan
    Cailiao Gongcheng/Journal of Materials Engineering, 2015, 43 (03): : 67 - 71
  • [42] Microstructure and Tensile Properties of SiC Reinforced Aluminum Matrix Composite Prepared by Selective Laser Melting
    Zou Tianchun
    Zhu He
    Chen Minying
    Mei Siyuan
    Yang Xudong
    CHINESE JOURNAL OF LASERS-ZHONGGUO JIGUANG, 2021, 48 (10):
  • [43] Effect of Sc content on microstructure and properties of Al-Zn-Mg-Cu-Zr alloy
    Sun, Yuqiao
    Luo, Yuhong
    Pan, Qinglin
    Liu, Bing
    Long, Liang
    Wang, Weiyi
    Ye, Ji
    Huang, Zhiqi
    Xiang, Shengqian
    MATERIALS TODAY COMMUNICATIONS, 2021, 26
  • [44] THE EFFECT OF RRA ON THE MICROSTRUCTURE AND PROPERTIES OF A NOVEL Al-Zn-Mg-Cu-Zr ALLOY
    Li, Xiwu
    Xiong, Baiqing
    Zhang, Yongan
    Zhu, Baohong
    Liu, Hongwei
    Li, Zhihui
    INTERNATIONAL JOURNAL OF MODERN PHYSICS B, 2009, 23 (6-7): : 900 - 905
  • [45] Effect of Sc content on microstructure and properties of Al-Zn-Mg-Cu-Zr alloy
    Sun, Yuqiao
    Luo, Yuhong
    Pan, Qinglin
    Liu, Bing
    Long, Liang
    Wang, Weiyi
    Ye, Ji
    Huang, Zhiqi
    Xiang, Shengqian
    Materials Today Communications, 2021, 26
  • [46] The effects of Zr and Ti on the microstructure and tensile properties of Al-Cu-Mg aluminium alloy
    Nassirirad, A.
    Emamy, M.
    Pourbahari, B.
    CANADIAN METALLURGICAL QUARTERLY, 2018, 57 (04) : 470 - 480
  • [47] Microstructure Evolution of High-Alloyed Al-Zn-Mg-Cu-Zr Alloy Containing Trace Amount of Sc During Homogenization
    Wang, Yu
    Li, Zhihui
    Xiong, Baiqing
    Wen, Kai
    Huang, Shuhui
    Li, Xiwu
    Zhang, Yongan
    METALS AND MATERIALS INTERNATIONAL, 2019, 25 (03) : 697 - 704
  • [48] Effects of Sc, Zr and Ti on the microstructure and properties of Al alloys with high Mg content
    Xu Wang
    Guoqin Chen
    Bing Li
    Lianmei Wu
    Daming Jiang
    Rare Metals, 2010, 29 : 66 - 71
  • [49] Effects of Sc, Zr and Ti on the microstructure and properties of Al alloys with high Mg content
    Wang Xu
    Chen Guoqin
    Li Bing
    Wu Lianmei
    Jiang Daming
    RARE METALS, 2010, 29 (01) : 66 - 71
  • [50] Microstructure, mechanical properties and wear behavior of Mg matrix composites reinforced with Ti and nano SiC particles
    Ahmadian, Hossein
    Zhou, Tianfeng
    Alansari, A.
    Kumar, A. Senthil
    Fathy, A.
    Elmahdy, M.
    Yu, Qian
    Weijia, Guo
    JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2024, 31 : 4088 - 4103