Microstructure and properties of a HIP manufactured SiC p reinforced high alloyed Al - Zn - Mg - Cu - Zr - Ti aluminum matrix composite

被引:4
|
作者
Yao, Hui [1 ]
Xu, Xiaojing [1 ]
Luo, Yuntian [1 ]
Han, Tian [1 ]
Zhou, Qingshan [1 ]
机构
[1] Jiangsu Univ, Inst Adv Mfg & Modern Equipment Technol, Zhenjiang, Peoples R China
来源
JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T | 2024年 / 30卷
关键词
Aluminum matrix composites; SiC particles; Microstructure; Mechanical properties; Corrosion properties; MECHANICAL-PROPERTIES; STRENGTHENING MECHANISMS; CORROSION BEHAVIOR; LOCALIZED CORROSION; TENSILE PROPERTIES; HEAT-TREATMENT; DEFORMATION; RESISTANCE; SUSCEPTIBILITY; PARTICLES;
D O I
10.1016/j.jmrt.2024.04.190
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
In this study, a hot isostatic pressing (HIP) manufactured SiC particles (SiC p ) reinforced high alloyed Al - Zn - Mg - Cu - Zr - Ti aluminum matrix composite was fabricated through ball-milling, HIP, homogenization, hot extrusion, solution treatment, and aging treatment. The results showed the presence of an interfacial reaction layer, MgAl 2 O 4 , around the SiC p , which enhanced the bonding between the particles and the matrix. The aging treatment resulted in the formation of different aging precipitates, which were featured by GP zone for T4, GP zone + eta ' (metastable MgZn 2 ) + eta (stable MgZn 2 ) for T6 and GP zone + eta ' (metastable MgZn 2 ) for T6I4. The composite samples of T4, T6, and T6I4 exhibited different mechanical properties. Specifically, the elastic modulus was measured as 102.9, 103.4, and 102.3 GPa, the yield strength was 685.3, 598.1, and 619.7 MPa, the ultimate tensile strength was 713.6, 618.9, and 633.3 MPa, and the elongation was 2.2%, 1.8%, and 2.8%, respectively. Furthermore, the corrosion behavior of the composite was evaluated through electrochemical, intergranular corrosion, and exfoliation corrosion. The corrosion current density was found to be 3.17 x 10 -7 , 4.97 x 10 -7 , and 3.67 x 10 -7 A cm -2 , the corrosion potential was measured as -0.70, -0.81, and -0.56 V, and the maximum intergranular corrosion depth was 139.9, 167.8, and 106.2 mu m for T4, T6, and T6I4, respectively. The severity of exfoliation corrosion varied, with T4 showing severe pitting, T6 exhibiting moderate pitting, and T6I4 displaying slight pitting. The strengthening mechanism and load transfer strengthening of the composites were discussed in detail based on theoretical calculations, and the anti-corrosion mechanisms were also analyzed.
引用
收藏
页码:4856 / 4867
页数:12
相关论文
共 50 条
  • [21] Effect of ECAP consolidation temperature on the microstructure and mechanical properties of Al-Cu-Ti metallic glass reinforced aluminum matrix composite
    Rezaei, M. R.
    Shabestari, S. G.
    Razavi, S. H.
    JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY, 2017, 33 (09) : 1031 - 1038
  • [22] Effect of Mg addition on the microstructure and mechanical properties of SiC nanowires reinforced 6061Al matrix composite
    Yang, Wenshu
    Chen, Guoqin
    Qiao, Jing
    Zhang, Qiang
    Dong, Ronghua
    Wu, Gaohui
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2017, 689 : 189 - 194
  • [23] Microstructure of Mg-Zn Matrix Composite Reinforced with Nano-SiC Prepared by Thixomolding
    Rogal, Lukasz
    Bobrowski, Piotr
    Stan-Glowinska, Katarzyna
    Szlezynger, Maciej
    Litynska-Dobrzynska, Lidia
    MATERIALS TRANSACTIONS, 2019, 60 (05) : 704 - 707
  • [24] Effect of Heat Treatment on the Microstructure and Mechanical Properties of a Composite Made of Al-Si-Cu-Mg Aluminum Alloy Reinforced with SiC Particles
    Li, Xin
    Yan, Hong
    Wang, Zhi-Wei
    Li, Ning
    Liu, Jian-Long
    Nie, Qiao
    METALS, 2019, 9 (11)
  • [25] Effect of Zr, Ti and Cr additions on microstructure and properties of super-high strength Al-Zn-Mg-Cu alloys
    Fang H.
    Chao H.
    Zhang Z.
    Chen K.
    Fang, Huachan (fanghc@csu.edu.cn), 1600, Central South University of Technology (47): : 420 - 429
  • [26] Effect of Zn/Mg and Cu/Mg on microstructure and properties of Al-xZn-3.0Mg-yCu-0.2Zr rolled aluminum alloy
    Xu, Xiaojing
    Zhu, Chenyu
    Wang, Hao
    Jia, Weijie
    Du, Donghui
    Cai, Chengbin
    Wang, Tianlun
    MATERIALS RESEARCH EXPRESS, 2019, 6 (01)
  • [27] Effect of Zn/Mg Ratio on Microstructure and Properties of Cold Extruded Al-xZn-2.4Mg-0.84Cu-0.2Zr-0.25Ti Aluminum Alloy
    Li, Chen
    Xu, Xiaojing
    Chen, Hanhui
    Tabie, Vitus
    Cai, Jie
    Liu, Yangguang
    Liu, Zheng
    Peng, Ching-Tun
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2020, 29 (09) : 5787 - 5795
  • [28] Effect of Zn/Mg Ratio on Microstructure and Properties of Cold Extruded Al-xZn-2.4Mg-0.84Cu-0.2Zr-0.25Ti Aluminum Alloy
    Chen Li
    Xiaojing Xu
    Hanhui Chen
    Vitus Tabie
    Jie Cai
    Yangguang Liu
    Zheng Liu
    Ching-Tun Peng
    Journal of Materials Engineering and Performance, 2020, 29 : 5787 - 5795
  • [29] Effect of combined addition of Zr, Ti and Y on microstructure and tensile properties of an Al-Zn-Mg-Cu alloy
    Li, Jiaheng
    Zhang, Yingbo
    Li, Mojia
    Hu, Yunfeng
    Zeng, Qi
    Zhang, Pu
    MATERIALS & DESIGN, 2022, 223
  • [30] Influence of Zr on the microstructure and mechanical properties of an Al-Zn-Mg-Cu alloy
    Yang, Shoujie
    Xie, Youhua
    Dai, Shenglong
    Yan, Minggao
    2006 BIMW: 2006 BEIJING INTERNATIONAL MATERIALS WEEK, PTS 1-4: MAGNESIUM, 2007, 546-549 : 1069 - +