Effect of Ce and solidification cooling rate on the microstructure and mechanical properties of AA2017 aluminum alloy

被引:2
|
作者
Rojas-Arias, N. [1 ,2 ,3 ]
Silva, Argos Soares [1 ,2 ]
Sousa, Sarah Maria de Albuquerque [1 ]
Gouveia, Guilherme Lisboa de [1 ]
Amancio-Filho, S. T. [3 ]
Coury, F. G. [1 ,2 ,4 ]
Spinelli, Jose Eduardo [1 ,2 ]
Gargarella, P. [1 ,2 ,4 ]
机构
[1] Univ Fed Sao Carlos, Grad Program Mat Sci & Engn, BR-13565905 Sao Carlos, SP, Brazil
[2] Univ Fed Sao Carlos, Dept Mat Engn, BR-13565905 Sao Carlos, SP, Brazil
[3] Graz Univ Technol, Graz Univ Technol, Inst Mat Sci Joining & Forming, BMK Endowed Professorship Aviat, Kopernikusgasse 24-1, A-8010 Graz, Austria
[4] Univ Fed Sao Carlos, Ctr Characterizat & Dev Mat CCDM, BR-13565905 Sao Carlos, SP, Brazil
基金
巴西圣保罗研究基金会; 瑞典研究理事会;
关键词
AA2017; Cerium; Directional solidification; Microstructure; Microhardness; Compressive strength; RARE-EARTH CE; DIRECTIONAL SOLIDIFICATION; EQUIAXED TRANSITION; CERIUM; COLUMNAR; DIFFUSION; TI;
D O I
10.1016/j.jallcom.2024.174848
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
Controlling dendritic growth and grain size in new Ce-containing Al-based alloys becomes crucial due to new envisioned applications and Ce rising demand in casting processes. In the present work Ce effect on the 2xxx Al series microstructures at various industrial-scale solidification cooling rates was investigated. The directional solidification technique is crucial in this endeavor since can generate several solidified samples related to several cooling rates. The AA2017 alloy and a modified version containing 3 wt % of Ce were both produced under directional solidification and various microstructure aspects were characterized. The mechanical behavior was analyzed by microhardness and compression tests. The Ce addition reduced primary and secondary dendritic spacing without impacting grain size. Cells were only observed to form on the Ce-containing alloy at cooling rates of approximately 19 degrees C/s; while dendritic configurations dominated all other conditions. While round pockets composed of Al+Al2Cu+Mg2Si ternary eutectic formed the interdendritic zones in the AA2017 alloy, the AA2017-Ce alloy microstructure was mainly constituted by elongated AlCeSi + Al8CeCu4 interdendritic phases. Finally, the addition of Ce favored an increase in the microhardness and compressive strength values of the AA2017 alloy, which is attributed to the refinement of the solidification structure, as well as the formation of a greater fraction of secondary reinforcement phases.
引用
收藏
页数:14
相关论文
共 50 条
  • [31] Effect of cooling rate on the microstructure and mechanical properties of ZK60 alloy
    Lin, Jinbao
    Wang, Qudong
    Peng, Liming
    Zhou, Yang
    Ding, Wenjiang
    2006 BIMW: 2006 BEIJING INTERNATIONAL MATERIALS WEEK, PTS 1-4: MAGNESIUM, 2007, 546-549 : 319 - +
  • [32] Effect of Cooling Rate During Solidification of Aluminum-Chromium Alloy
    Muthusamy, G.
    Wagstaff, S.
    Allanore, A.
    LIGHT METALS 2020, 2020, : 204 - 209
  • [33] Effect of cooling speed and ultrasonic vibration on solidification structure and mechanical properties of 7085 aluminum alloy
    Li An-qing
    Zhang Li-hua
    Jiang Ri-peng
    Li Xiao-qian
    Zhang Yun
    CAILIAO GONGCHENG-JOURNAL OF MATERIALS ENGINEERING, 2021, 49 (08): : 63 - 71
  • [34] Effect of Cooling Conditions on the Solidification Microstructure and Mechanical Properties of Al–18Si Alloy
    Ze Zhu
    Han Zhou
    Ya Liu
    Changjun Wu
    Jianhua Wang
    Transactions of the Indian Institute of Metals, 2023, 76 : 2827 - 2833
  • [35] Effect of Cooling Conditions on the Solidification Microstructure and Mechanical Properties of Al-18Si Alloy
    Zhu, Ze
    Zhou, Han
    Liu, Ya
    Wu, Changjun
    Wang, Jianhua
    TRANSACTIONS OF THE INDIAN INSTITUTE OF METALS, 2023, 76 (10) : 2827 - 2833
  • [36] Effect of cooling rates on solidification, microstructure and mechanical properties in tungsten
    Li, Sixu
    Cui, Shiyong
    Chen, Haotian
    Li, Jia
    Huang, Hongtao
    Luo, Hao
    CRYSTENGCOMM, 2019, 21 (26): : 3930 - 3938
  • [37] Effect of Ce on solidification and mechanical properties of A360 alloy
    Voncina, Maja
    Kores, Stanislav
    Mrvar, Primoz
    Medved, Jozef
    JOURNAL OF ALLOYS AND COMPOUNDS, 2011, 509 (27) : 7349 - 7355
  • [38] Investigation of The Effect of Mechanical Vibration Applied During Solidification on The Microstructure and Properties of Aluminum 356 Alloy
    Ozgu, Taha Sureyya
    Calin, Recep
    Tanis, Naci Arda
    ARCHIVES OF FOUNDRY ENGINEERING, 2024, 24 (01) : 26 - 31
  • [39] The effect of cooling rate of solidification on microstructure and alloy element segregation of as cast alloy 718
    Jingchen, Z
    Ping, Y
    SUPERALLOYS 718, 625, 706 AND VARIOUS DERIVATIVES, 2001, : 133 - 140
  • [40] Interplay Between Cooling Rate, Microstructure, and Mechanical Properties of an Al-Ce-Ni-Mn Alloy
    Kozakevich, Jordan
    Stroh, Joshua
    Mallouhi, Victor
    Sediako, Dimitry
    Weiss, David
    LIGHT METALS 2022, 2022, : 83 - 91