The critical current irreversibility of Bi(2223)/Ag tape and its modification

被引:0
|
作者
兰玉成
郭树权
肖业皋
叶斌
曾荣
周怡茹
机构
[1] National Laboratory for Superconductivity
[2] Institute of Physics
[3] Chinese Academy of Sciences
[4] Beijing
[5] China
[6] General Research Insitute for Non-ferrous Metal
[7] Beijing
关键词
D O I
暂无
中图分类号
O482 [固体性质];
学科分类号
摘要
<正> The critical currents of Bi(2223)/Ag tape at magnetic fields up to 2.5T have been measured at different field orientations. The IC values depend on the history of magnetic fields. This phenomenon can be explained in terms of irreversibility of the effective magnetic field caused by the induced persistent current and the screening persistent current. If the mean of the increasing and the decreasing applied field (Hap), defined as the effective field (Hcff), is linearly related to the applied field, i.e. Heff, using Heff instead of Hap, the modified IC(H) curves curves are obtainable.
引用
收藏
页码:108 / 112
页数:5
相关论文
共 50 条
  • [31] Critical current of a Bi-2223/Ag pancake coil
    Lahtinen, M
    Paasi, J
    Han, Z
    APPLIED SUPERCONDUCTIVITY 1995, VOLS. 1 AND 2: VOL 1: PLENARY TALKS AND HIGH CURRENT APPLICATIONS; VOL 2: SMALL SCALE APPLICATIONS, 1995, 148 : 715 - 718
  • [32] Anisotropy of critical current and glass-liquid transition flux density in Bi-2223/Ag tape
    Nakamura, T
    Yamamoto, T
    Tsuchiya, S
    Fujio, A
    Hoshino, T
    Muta, I
    Oh, SS
    Ha, HS
    SUPERCONDUCTOR SCIENCE & TECHNOLOGY, 2000, 13 (11): : 1521 - 1525
  • [33] Intragranular critical current density of superconductor grain in screen-printed Ag-Bi2223 tape
    Kawano, K
    Oota, A
    Fukuta, K
    Higuchi, T
    Fujimoto, H
    CRYOGENICS, 1999, 39 (10) : 853 - 858
  • [34] Distribution of local critical current along sample length and its relation to overall current in a long Bi2223/Ag superconducting composite tape
    Ochiai, S.
    Doko, D.
    Okuda, H.
    Oh, S. S.
    Ha, D. W.
    SUPERCONDUCTOR SCIENCE & TECHNOLOGY, 2006, 19 (11): : 1097 - 1103
  • [35] The influence of tape arrangements on the critical current of Bi-2223 superconducting current leads
    Qu, T.-M.
    Gu, C.
    Li, X.-F.
    Zhao, L.
    Li, P.
    Zhang, H.-J.
    Han, Z.
    IEEE TRANSACTIONS ON APPLIED SUPERCONDUCTIVITY, 2007, 17 (02) : 2232 - 2235
  • [36] Fatigue behavior and its influence on the critical current of externally reinforced Bi-2223 superconducting tape
    Shin, HS
    Dizon, JRC
    Kim, KH
    Oh, SS
    Ha, DW
    IEEE TRANSACTIONS ON APPLIED SUPERCONDUCTIVITY, 2005, 15 (02) : 3556 - 3559
  • [37] Influence of modification of annealing and sheath materials on critical current density of Bi-2223/Ag tapes
    Ha, DW
    Kim, SC
    Yang, JS
    Oh, SS
    Ha, HS
    IEEE TRANSACTIONS ON APPLIED SUPERCONDUCTIVITY, 2005, 15 (02) : 2478 - 2481
  • [38] Irreversibility Line and Flux Relaxation in Bi:2223/Ag Tape Prepared by CTFF Technique: H//c axis
    İ. Düzgün
    A. Öztürk
    S. Çelebi
    Journal of Superconductivity and Novel Magnetism, 2010, 23 : 1349 - 1354
  • [39] The influence of tensile strain to critical current of Bi2223 composite tape
    Mukai, Y.
    Shin, J. K.
    Ochiai, S.
    Okuda, H.
    Sugano, M.
    Osamura, K.
    PHYSICA C-SUPERCONDUCTIVITY AND ITS APPLICATIONS, 2008, 468 (15-20): : 1801 - 1804
  • [40] Research on effect of ferromagnetic material on the critical current of Bi-2223 tape
    Wu, Yi
    Rong, Mingzhe
    Li, Jian
    Wang, Xiaohua
    IEICE TRANSACTIONS ON ELECTRONICS, 2008, E91C (08): : 1222 - 1227