IMPROVEMENT OF SIO2/SI INTERFACE BY LOW-TEMPERATURE ANNEALING IN WET ATMOSPHERE

被引:22
|
作者
SANO, N
SEKIYA, M
HARA, M
KOHNO, A
SAMESHIMA, T
机构
[1] Sony Corporation Research Center, Hodogaya-ku, Yokohama 240, 174, Fujitsuka-cho
[2] Faculty of Science, Kyushu University, Higashi-ku, Fukuoka 812, 6-10-1, Hakozaki
[3] Max-Planck-Institut für Festköperforschung, D-70569 Stuttgart
关键词
D O I
10.1063/1.113918
中图分类号
O59 [应用物理学];
学科分类号
摘要
A postannealing technique was developed in order to improve the quality of SiO2 films formed by a parallel-plate remote plasma chemical vapor deposition. The wave number of the antisymmetric stretching mode of Si-O-Si bonding in the SiO2 film increased from 1058 to 1069 cm-1 by an annealing in H2O vapor at 270°C. It was estimated that averaged bonding angle of Si-O-Si was widened from 137.8°to 141.0°. The annealing in the H2O vapor ambient at 270°C for 30 min efficiently reduced the interface trap density to 2.0×1010cm-2 eV-1 and the effective oxide charges density from 7×1011 to 5×109 cm-2 for a metal-oxide-semiconductor (MOS) diode using the SiO2 film.© 1995 American Institute of Physics.
引用
收藏
页码:2107 / 2109
页数:3
相关论文
共 50 条
  • [21] Low-temperature atomic hydrogen treatment of SiO2/Si structures
    Zhang, H
    Kumagai, A
    Xu, G
    Ishibashi, K
    JAPANESE JOURNAL OF APPLIED PHYSICS PART 1-REGULAR PAPERS BRIEF COMMUNICATIONS & REVIEW PAPERS, 2003, 42 (10): : 6252 - 6255
  • [22] Research on annealing temperature of SiO2 on Si substrate
    Lv, Hao
    Ding, Yaoming
    Liu, Aimei
    Tong, Jufang
    Yi, Xunong
    Li, Qianguang
    Chen, Chen
    Shi, Bangren
    ADVANCED MATERIALS AND PROCESSES, PTS 1-3, 2011, 311-313 : 1258 - +
  • [23] HIGH-TEMPERATURE DECOMPOSITION OF SIO2 AT THE SI/SIO2 INTERFACE
    RUBLOFF, GW
    TROMP, RM
    VANLOENEN, EJ
    BALK, P
    LEGOUES, FK
    JOURNAL OF VACUUM SCIENCE & TECHNOLOGY A-VACUUM SURFACES AND FILMS, 1986, 4 (03): : 1024 - 1025
  • [24] HIGH-TEMPERATURE SIO2 DECOMPOSITION AT THE SIO2/SI INTERFACE
    TROMP, R
    RUBLOFF, GW
    BALK, P
    LEGOUES, FK
    VANLOENEN, EJ
    PHYSICAL REVIEW LETTERS, 1985, 55 (21) : 2332 - 2335
  • [25] Effect of postoxidation annealing on Si/SiO2 interface roughness
    Chen, XD
    Gibson, JM
    JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1999, 146 (08) : 3032 - 3038
  • [26] Effect of low-temperature interphase charge transport at the Si/SiO2 interface on the photoresponse of silicon barrier structures
    N. I. Bochkareva
    S. A. Khorev
    Semiconductors, 2000, 34 : 1177 - 1182
  • [27] Effect of low-temperature interphase charge transport at the Si/SiO2 interface on the photoresponse of silicon barrier structures
    Bochkareva, NI
    Khorev, SA
    SEMICONDUCTORS, 2000, 34 (10) : 1177 - 1182
  • [28] Low-temperature treatment of Si/SiO2 structures in an RF hydrogen plasma
    Szekeres, A
    Alexandrova, S
    VACUUM, 1996, 47 (12) : 1483 - 1486
  • [29] LOW-TEMPERATURE ANNEALING OF AL-IMPLANTED SI-SIO2 STRUCTURES
    ABERG, AT
    PHYSICA STATUS SOLIDI A-APPLIED RESEARCH, 1977, 42 (02): : 639 - 645
  • [30] Low-Temperature Cathodoluminescence in Disordered SiO2
    Evans, Amberly
    Dennison, John Robert
    Wilson, Gregory
    Dekany, Justin
    IEEE TRANSACTIONS ON PLASMA SCIENCE, 2014, 42 (01) : 272 - 277