THE RESISTANCE OF NICKEL AND IRON ALUMINIDES TO CAVITATION EROSION AND ABRASIVE WEAR

被引:68
|
作者
JOHNSON, M
MIKKOLA, DE
MARCH, PA
WRIGHT, RN
机构
[1] TENNESSEE VALLEY AUTHOR,ENGN LAB,NORRIS,TN 37828
[2] EG&G IDAHO INC,IDAHO NATL ENGN LAB,IDAHO FALLS,ID 83415
关键词
D O I
10.1016/0043-1648(90)90090-W
中图分类号
TH [机械、仪表工业];
学科分类号
0802 ;
摘要
The abrasive wear and cavitation erosion resistance of several alloys based on the intermetallic compounds Ni3Al and Fe3Al have been investigated. The erosion resistance of the nickel aluminides is relatively insensitive to alloying with iron or chromium and is comparable with or superior to that of many commercial erosion-resistant alloys; the abrasive wear resistance is found to be decreased by alloying, despite increased room temperature strength and refined grain size. Preliminary results for the iron aluminides indicate increased resistance to abrasive wear with increasing alloy content. It is suggested that the abrasive wear process causes temperature increases in the damage zone that are sufficient to cause the elevated temperature properties of the alloys to become dominant. Under these conditions, the wear resistance can be related to the tendency to disorder, either thermally or through plastic deformation.
引用
收藏
页码:279 / 289
页数:11
相关论文
共 50 条
  • [1] EROSION AND ABRASIVE WEAR-RESISTANCE OF POWDER-METALLURGY NICKEL ALUMINIDES
    MUSSATTO, MJ
    RUNDMAN, BK
    MIKKOLA, DE
    WRIGHT, RN
    JOURNAL OF METALS, 1987, 39 (10): : A65 - A65
  • [2] Abrasive Wear Resistance of Powder Composites at Abrasive Erosion and Abrasive Impact Wear
    Kulu, Priit
    Veinthal, Renno
    Kaeerdi, Helmo
    Tarbe, Riho
    MATERIALS SCIENCE-MEDZIAGOTYRA, 2008, 14 (04): : 328 - 332
  • [3] Sliding wear resistance of iron aluminides
    Sharma, G
    Sundararaman, M
    Prabhu, N
    Goswami, GL
    BULLETIN OF MATERIALS SCIENCE, 2003, 26 (03) : 311 - 314
  • [4] Sliding wear resistance of iron aluminides
    Garima Sharma
    M. Sundararaman
    N. Prabhu
    G. L. Goswami
    Bulletin of Materials Science, 2003, 26 : 311 - 314
  • [5] RESISTANCE TO WEAR AND CAVITATION EROSION OF BEARING ALLOYS
    OKADA, T
    IWAI, Y
    HOSOKAWA, Y
    WEAR, 1986, 110 (3-4) : 331 - 343
  • [6] ABRASIVE WEAR AND CAVITATION
    KOZYREV, SP
    SHALNEV, KK
    DOKLADY AKADEMII NAUK SSSR, 1962, 143 (01): : 60 - &
  • [7] CAVITATION EROSION AND ABRASIVE WEAR OF NI3AL ALLOYS
    JOHNSON, ML
    MIKKOLA, DE
    WRIGHT, RN
    INTERMETALLICS, 1995, 3 (05) : 389 - 396
  • [8] Wear resistance and mechanisms of composite hardfacings at abrasive impact erosion wear
    Surzhenkov, A.
    Viljus, M.
    Simson, T.
    Tarbe, R.
    Saarna, M.
    Casesnoves, F.
    6TH INTERNATIONAL CONFERENCE ON FRACTURE FATIGUE AND WEAR (FFW), 2017, 843
  • [9] EROSION BEHAVIOR OF NICKEL ALUMINIDES
    LUI, A
    SAHOO, M
    MORIN, G
    SIKKA, VK
    CIM BULLETIN, 1988, 81 (914): : 80 - 80
  • [10] Research on cavitation erosion and wear resistance performance of coatings
    Qiu, Ning
    Wang, Leqin
    Wu, Suhuan
    Likhachev, Dmitriy S.
    ENGINEERING FAILURE ANALYSIS, 2015, 55 : 208 - 223