A COMPOSITE-MATERIAL WITH A MATRIX OF HIGH-CHROMIUM CAST-IRON

被引:0
|
作者
PONOMARENKO, VP
STOIKO, VP
SHVARTSER, AY
机构
关键词
D O I
10.1007/BF00708342
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
引用
收藏
页码:819 / 821
页数:3
相关论文
共 50 条
  • [21] High-chromium cast iron sintered of sprayed powders
    G. A. Baglyuk
    Yu. F. Ternovoi
    V. N. Terekhov
    Powder Metallurgy and Metal Ceramics, 2007, 46 : 194 - 196
  • [22] INCREASING THE QUALITY OF ROLLING ROLLS OF HIGH-CHROMIUM CAST-IRON BY HIGH-TEMPERATURE HEAT-TREATMENT
    SKOBLO, TS
    VISHNYAKOVA, EN
    MOZHAROVA, NM
    DUBROV, VA
    BONDIN, RD
    METAL SCIENCE AND HEAT TREATMENT, 1990, 32 (9-10) : 734 - 736
  • [23] High-chromium white cast iron in slurry pumps
    Collins, Allan N.
    Chromium review, 1988, (09): : 5 - 8
  • [24] Wear Resistance of High-Chromium Cast Iron.
    Matsui, A.
    Hara, M.
    Aufbereitungs-Technik/Mineral Processing, 1975, 16 (08): : 418 - 424
  • [25] High-chromium white cast iron in slurry pumps
    Collins, Allan, 1600, (163):
  • [26] Abrasion Wear Behavior of High-chromium Cast Iron
    Pokusova, M.
    Brusilova, A.
    Soos, L'.
    Berta, I.
    ARCHIVES OF FOUNDRY ENGINEERING, 2016, 16 (02) : 69 - 74
  • [27] MECHANISM OF SURFACE-LAYER HARDENING IN IMPACT-ABRASIVE WEAR OF HIGH-CHROMIUM CAST-IRON
    KOMAROV, OS
    IVASHKIN, VV
    URBANOVICH, NI
    METAL SCIENCE AND HEAT TREATMENT, 1990, 32 (3-4) : 278 - 280
  • [28] High-chromium cast iron sintered of sprayed powders
    Baglyuk, G. A.
    Ternovoi, Yu. F.
    Terekhov, V. N.
    POWDER METALLURGY AND METAL CERAMICS, 2007, 46 (3-4) : 194 - 196
  • [29] WEAR INDUCED MARTENSITE IN HIGH CHROMIUM CAST-IRON
    SINATORA, A
    POHL, M
    WALDHERR, EU
    SCRIPTA METALLURGICA ET MATERIALIA, 1995, 32 (06): : 857 - 861
  • [30] JET SLURRY CORROSIVE WEAR OF HIGH-CHROMIUM CAST-IRON AND HIGH-CARBON STEEL GRINDING BALL ALLOYS
    PITT, CH
    CHANG, YM
    CORROSION, 1986, 42 (06) : 312 - 317