共 50 条
- [31] STUDY ON THE TEST METHOD OF OXIDE SCALE ADHESION INSIDE SUPERHEATER/REHEATER TUBES BASED ON IMAGE RECOGNITION JOINT EPRI - 123HIMAT INTERNATIONAL CONFERENCE ON ADVANCES IN HIGH-TEMPERATURE MATERIALS, 2019, 2019, : 685 - 693
- [32] Root Cause Analysis of Failure in Superheater Tubes in a Power Plant Metallography, Microstructure, and Analysis, 2019, 8 : 275 - 280
- [34] Failure causes of cracking and bending of boiler superheater tube in power plant MULTISCALING ASSOCIATED WITH STRUCTURAL AND MATERIAL INTEGRITY UNDER ELEVATED TEMPERATURE, 2006, : 373 - 378
- [35] Failure Analysis Of Steel Superheater Tube Fractured In A Boiler Of A Power Plant FRACTURE AND STRENGTH OF SOLIDS VII, PTS 1 AND 2, 2011, 462-463 : 467 - 471