BRITTLE-FRACTURE OF COLD-WORKED STEEL WITH A FIBROUS STRUCTURE

被引:0
|
作者
BARAZ, VR [1 ]
RUNDKVIST, NA [1 ]
BELOV, AV [1 ]
SOKOLOV, AA [1 ]
NOVIKOV, SN [1 ]
机构
[1] IP BARDIN CENT FERROUS MET RES INST,MOSCOW,USSR
关键词
D O I
10.1007/BF00730922
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
The brittle fracture of cold drawn steel wire is related to its structural condition, which is characterized by intense loosening as the result of formation of stable microcracks. In this case failure by breaking away must be considered as a normal but alternative variation of brittle fracture. Lamination is an extreme case of brittle behavior of steel in torsion, which is aided not only by strong accumulation of microdiscontinuities and sharply expressed anisotropy but also the increasing influence of residual internal stresses. The tendency of high-strength wire toward lamination may be evaluated in torsion tests from the change in torsional moment and length of the specimens and also from the external appearance of the fracture. A treatment of the drawn wire promoting a reduction in residual microstresses makes it possible to decrease the tendency toward lamination. For example, a short temper under load promotes relaxation of these stresses. © 1990 Plenum Publishing Corporation.
引用
收藏
页码:196 / 200
页数:5
相关论文
共 50 条
  • [21] Hydrogen embrittlement interactions in cold-worked steel
    Huang, H.
    Shaw, W.J.D.
    Corrosion, 1995, 51 (01): : 30 - 36
  • [22] HARDENING AND TOUGHNESS OF COLD-WORKED STEEL WIRE
    BARANOV, AA
    ALIMOV, VI
    BEREZIN, AV
    YANSHIN, AV
    BILANCHUK, SN
    STEEL IN THE USSR, 1987, 17 (12): : 569 - 570
  • [23] TRANSFORMATIONS IN COLD-WORKED STEEL DURING HEATING
    TKACHENKO, FK
    MAYSTRUK, AY
    SERGEYKO, LG
    MELNICHE.AI
    RUSSIAN METALLURGY, 1973, (04): : 100 - 104
  • [24] RECRYSTALLIZATION OF COLD-WORKED STRUCTURAL-STEEL
    MARCHENKO, SS
    SYSOEVA, VS
    CHUMAK, GA
    METAL SCIENCE AND HEAT TREATMENT, 1974, 16 (9-10) : 732 - 735
  • [25] BRITTLE-FRACTURE OF STEEL WITH A HIGH PHOSPHORUS CONCENTRATION
    ENDRZHEEVSKII, BE
    MESHKOV, YY
    PAKHARENKO, GA
    METAL SCIENCE AND HEAT TREATMENT, 1994, 36 (11-12) : 577 - 581
  • [26] BRITTLE-FRACTURE OF STEEL ELECTROLYTICALLY SATURATED WITH HYDROGEN
    BIGGIERO, G
    BORRUTO, A
    MARAFINI, F
    SOVIET ATOMIC ENERGY, 1980, 49 (01): : 443 - 447
  • [27] FRACTOGRAPHIC STUDY OF RESISTANCE OF STEEL TO BRITTLE-FRACTURE
    KOVALEV, AI
    METAL SCIENCE AND HEAT TREATMENT, 1976, 18 (7-8) : 720 - 722
  • [28] BRITTLE-FRACTURE INITIATION IN PRESTRESSED STEEL SHEET
    CLAYTON, JQ
    METALS FORUM, 1983, 6 (01): : 34 - 42
  • [29] LOWER STRENGTH STEEL BRITTLE-FRACTURE ASSESSMENT
    MAGUED, MH
    KENNEDY, DJL
    JOURNAL OF THE STRUCTURAL DIVISION-ASCE, 1974, 100 (NST5): : 983 - 999
  • [30] PREVENTING BRITTLE-FRACTURE OF STEEL DURING GRINDING
    ISKHAKOV, SS
    RUSSIAN ENGINEERING JOURNAL-USSR, 1971, 51 (10): : 73 - &